Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 40.6 - 222 °C | 105 - 432 °F | Average value: 95.5 °C Grade Count:109 |
Overview of materials for Polycarbonate/PET Polyester Blend This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/PET Polyester Blend". Each property range of values reported is minimum and maximum values.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 40.6 - 106 °C | 105 - 223 °F | Average value: 59.7 °C Grade Count:56 |
Overview of materials for Polypropylene with 20% Calcium Carbonate (CaCO3) Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Calcium Carbonate (CaCO3) Filler". Each property range of values reported is mini.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 40.6 °C | 105 °F | ASTM D648 |
Spartech PP7220 Calcium Carbonate Filled High Impact Copolymer Provides the highest level of impact of all copolymers and are useful in applications where improved processing and stiffness are required versus unfilled copolymer materials.Information provided by.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 40.7 °C | 105 °F | |
Teknor Apex TELCAR® 1000-92 Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 40.7 °C | 105 °F | |
Teknor Apex TELCAR® 1000-92UV Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 40.6 °C | 105 °F | Unannealed; ASTM D648 |
Teknor Apex Telcar® TL-1000-92 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Automotive Spec.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 40.6 °C | 105 °F | Unannealed; ASTM D648 |
Teknor Apex Telcar® TL-1000-92-UV Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Automotive Spec.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 40.6 °C | 105 °F | ASTM D648 |
Clariant Renol BR7008 Polycarbonate/Polyester Alloy Data provided by Clariant Masterbatches |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 40.5 °C | 105 °F | ASTM D648 |
ExxonMobil HD 6706.17 Injection Molding Resin Product Description: HD 6706 is a narrow molecular weight hexane copolymer designed for good processability and excellent balance of ESR, Toughness and Stiffness properties. This resin is ideally su.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 40.5 °C | 105 °F | ASTM D648 |
ExxonMobil HD 6706.62 Injection Molding Resin Product Description: HD 6706 is a narrow molecular weight hexane copolymer designed for good processability and excellent balance of ESR, Toughness and Stiffness properties. This resin is ideally su.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 40.6 - 155 °C | 105 - 311 °F | Average value: 68.4 °C Grade Count:152 |
Overview of materials for Polypropylene, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Flame Retardant". Each property range of values reported is minimum and maximum values of.. |