Processing Properties | Metric | English | Comments |
---|---|---|---|
Die Temperature | 180 - 210 °C | 356 - 410 °F | |
Solvay Specialty Polymers Cogegum® GFR/350 Polyolefin, Unspecified
(Unverified Data**) Cogegum® XLPO-HFFR - Crosslinkable Halogen Free Fire Retardant compound Silane grafted compound moisture curable by addition of a catalyst masterbatch (Sioplas® method). It consists of a polyolefi.. |
|||
Die Temperature | 190 - 210 °C | 374 - 410 °F | Average value: 199 °C Grade Count:7 |
Overview of materials for Acetal Copolymer, 20% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% ar.. |
|||
Die Temperature | 190 - 210 °C | 374 - 410 °F | Extrusion |
Kraiburg TPE THERMOLAST® K TC3TPZ Thermoplastic Elastomer, General Purpose, Technical Performance The GP/AP Series is recommended for technical applications with excellent adhesion to PP. The compounds are available in natural and black colors. Typical applications:Function and design elements H.. |
|||
Die Temperature | 190 - 210 °C | 374 - 410 °F | Extrusion |
Kraiburg TPE THERMOLAST® K TC5FRZ Thermoplastic Elastomer, Flame retardant The FR Series is recommended for applications requiring high flame retardance. The compounds are halogen free and available in natural and black colors. Typical applications: Cable holders Seals for.. |
|||
Die Temperature | 190 - 210 °C | 374 - 410 °F | Extrusion |
Kraiburg TPE THERMOLAST® K TC6CSZ Thermoplastic Elastomer, Optimized compression set The CS Series is recommended for sealing applications, providing an excellent compression set. The compounds are available in natural and black colors. Typical applications: FasteningsGrommetsMembra.. |
|||
Die Temperature | 190 - 210 °C | 374 - 410 °F | Extrusion |
Kraiburg TPE THERMOLAST® K TP6CDZ Thermoplastic Elastomer, Adhesion to PP The EX Series is recommended for extrusion applications such as door seals and window gaskets. The compounds are available in natural and black colors. Typical applications: Edge guardsProfiles for .. |
|||
Die Temperature | 190 - 210 °C | 374 - 410 °F | Extrusion |
Kraiburg TPE THERMOLAST® K TP8CDB Thermoplastic Elastomer, Adhesion to PP The EX Series is recommended for extrusion applications such as door seals and window gaskets. The compounds are available in natural and black colors. Typical applications: Edge guardsProfiles for .. |
|||
Die Temperature | 200 - 210 °C | 392 - 410 °F | |
Lubrizol Advanced Materials Pearlthane® 12H92E Thermoplastic Polyurethane Elastomer Pearlthane® 12H92E is a special polyester-based TPU, supplied in form of translucent, colorless pellets, combining hardness with excellent processability and excellent low temperature performance.. |
|||
Die Temperature | 200 - 210 °C | 392 - 410 °F | Extrusion |
Huntsman IROGRAN® A 92 E 4860 TPU-Polyester Introduction: IROGRAN A92E 4860 is a high performance polyester based thermoplastic polyurethane intended for extrusion and injection molding applications. IROGRAN A92E 4860 is part of the HUNTSMAN .. |
|||
Die Temperature | 190 - 210 °C | 374 - 410 °F | Extrusion |
Kraiburg TPE THERMOLAST® K TC0TPZ Thermoplastic Elastomer, General Purpose, Technical Performance The GP/AP Series is recommended for technical applications with excellent adhesion to PP. The compounds are available in natural and black colors. Typical applications:Function and design elements H.. |
|||
Die Temperature | 190 - 210 °C | 374 - 410 °F | Extrusion |
Kraiburg TPE THERMOLAST® K TC8CSZ Thermoplastic Elastomer, Optimized compression set The CS Series is recommended for sealing applications, providing an excellent compression set. The compounds are available in natural and black colors. Typical applications: FasteningsGrommetsMembra.. |
|||
Die Temperature | 190 - 210 °C | 374 - 410 °F | |
Teknor Apex Telcar® CR-92-E2555A-92 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Die Temperature | 190 - 210 °C | 374 - 410 °F | |
Teknor Apex Telcar® TL EF-6177B-UV Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Die Temperature | 190 - 210 °C | 374 - 410 °F | |
Teknor Apex Telcar® TL-1000-105 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Die Temperature | 190 - 210 °C | 374 - 410 °F | |
Teknor Apex Telcar® TL-1446G Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Die Temperature | 190 - 210 °C | 374 - 410 °F | |
Teknor Apex Telcar® TL-1522G Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Die Temperature | 190 - 210 °C | 374 - 410 °F | |
Teknor Apex Telcar® TL-2575A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Die Temperature | 190 - 210 °C | 374 - 410 °F | |
Teknor Apex Telcar® TL-2580F Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Die Temperature | 190 - 210 °C | 374 - 410 °F | |
Teknor Apex Telcar® TL-2635B Thermoplastic Elastomer Uses: Building Materials; Flexible Grips; General Purpose; Handles; Safety Equipment; Toys Injection Notes: Injection Rate: Moderate-Fast Extrusion Notes: Screw Speed: 30 to 100 rpmInformation Provi.. |
|||
Die Temperature | 200 - 210 °C | 392 - 410 °F | |
Borealis Borstar® HE3410 HDPE for Sewage Pipes Borstar® HE3410 is a bimodal polyethylene compound produced by the advanced Borstar® technology. Well dispersed carbon black gives outstanding UV resistance. Long term stability is ensured by an .. |
|||
Die Temperature | 190 - 210 °C | 374 - 410 °F | |
Teknor Apex Telcar® TL-3954-90 Thermoplastic Elastomer Uses: Appliance Wire Insulation; Appliance Wire Jacketing; Cable Jacketing; Connectors; Flexible Cord Jacketing; Industrial Cable Insulation; Terminal Cable Jacketing; Underground Power Cable; Wire .. |
|||
Die Temperature | 190 - 210 °C | 374 - 410 °F | |
Teknor Apex Telcar® TL-4145A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Die Temperature | 190 - 210 °C | 374 - 410 °F | |
Teknor Apex Telcar® TL-88-N873C BLK 111 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Die Temperature | 190 - 210 °C | 374 - 410 °F | |
Teknor Apex Telcar® TL-91-T3056S-75 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Die Temperature | 190 - 210 °C | 374 - 410 °F | |
Teknor Apex Telcar® TL-94-T0586C-113 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Die Temperature | 190 - 210 °C | 374 - 410 °F | |
Teknor Apex Telcar® TL-2365A Thermoplastic Polyolefin Elastomer Uses: Automotive Applications; Flexible Grips; Gaskets; General Purpose; Industrial Applications; Roof Vents Forms: Pellets Processing Method: Extrusion; Injection Molding Injection Notes: Injectio.. |
|||
Die Temperature | 190 - 210 °C | 374 - 410 °F | |
Celanese Hostaform® C 9021 GV1/20 XGM POM, 20% Tribological
(Unverified Data**) Chemical abbreviation according to ISO 1043-1: POMlow wear, 20% fiberglass reinforced, PTFE containing gradeInformation provided by Celanese |
|||
Die Temperature | 199 - 210 °C | 390 - 410 °F | Zone 1 |
Lubrizol ESTANE® 58212 Ether Based Thermoplastic Polyurethane Features: Excellent clarity and UV stable with good melt strength. Pre-drying: 2 hours at 104°C (220°F) in dehumidifying hopper dryerUses: Extrusion: Cable jacket, hose/tube, profile and film and .. |
|||
Die Temperature | 190 - 210 °C | 374 - 410 °F | |
Celanese Hostaform® C 13031 K POM, Tribological Chemical abbreviation according to ISO 1043-1: POMInformation provided by Celanese |
|||
Die Temperature | 190 - 210 °C | 374 - 410 °F | |
Celanese Hostaform® C 13031 XAP POM, Unfilled Polyacetal copolymer, reduced emissionInformation provided by Celanese |