Processing Properties | Metric | English | Comments |
---|---|---|---|
Injection Pressure | 4.83 - 6.89 MPa | 700 - 1000 psi | |
Ravago Manufacturing Americas Hylac® PL75 ABS Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Injection Pressure | 1.38 - 6.89 MPa | 200 - 1000 psi | |
Teknor Apex Telcar® OBC 4560A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Injection Pressure | 1.38 - 6.89 MPa | 200 - 1000 psi | |
Teknor Apex Telcar® TELC 302 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Injection Pressure | 1.38 - 6.89 MPa | 200 - 1000 psi | |
Teknor Apex Telcar® TL EF-6133L2 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Injection Pressure | 1.38 - 6.89 MPa | 200 - 1000 psi | |
Teknor Apex Telcar® TL-1138 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Injection Pressure | 1.38 - 6.89 MPa | 200 - 1000 psi | |
Teknor Apex Telcar® TL-1336A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Injection Pressure | 1.38 - 6.89 MPa | 200 - 1000 psi | |
Teknor Apex Telcar® TL-1336B Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Injection Pressure | 1.38 - 6.89 MPa | 200 - 1000 psi | |
Teknor Apex Telcar® TL-1402G Thermoplastic Elastomer Notes: Non-halogenated, Flame Retardant TPE; RoHS Compliant Uses: Connectors; Electrical/Electronic Applications Forms: Pellets Processing Method: Extrusion; Injection Molding Injection Notes: Injec.. |
|||
Injection Pressure | 1.38 - 6.89 MPa | 200 - 1000 psi | |
Teknor Apex Telcar® TL-1420C Thermoplastic Elastomer Uses: Consumer Applications; Flexible Grips; General Purpose; Grommets; Industrial Soft; Sporting Goods; Toys; Weatherstripping Forms: Pellets Processing Method: Extrusion; Injection Molding Injecti.. |
|||
Injection Pressure | 1.38 - 6.89 MPa | 200 - 1000 psi | |
Teknor Apex Telcar® TL-1431F Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Injection Pressure | 1.38 - 6.89 MPa | 200 - 1000 psi | |
Teknor Apex Telcar® TL-1524E Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Injection Pressure | 1.38 - 6.89 MPa | 200 - 1000 psi | |
Teknor Apex Telcar® TL-1524F Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Injection Pressure | 1.38 - 6.89 MPa | 200 - 1000 psi | |
Teknor Apex Telcar® TL-1654D Thermoplastic Elastomer Notes: Non-halogenated; RoHS Compliant; MBDC: Green Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General .. |
|||
Injection Pressure | 1.38 - 6.89 MPa | 200 - 1000 psi | |
Teknor Apex Telcar® TL-1934A Styrenic Thermoplastic Elastomer Notes: RoHS Compliant Uses: Appliance Wire Insulation; Cable Jacketing; Flexible Cord Insulation; Flexible Cord Jacketing; Wire and Cable Applications; Wire Jacketing Agency Ratings: UL 1581Forms: P.. |
|||
Injection Pressure | 1.38 - 6.89 MPa | 200 - 1000 psi | |
Teknor Apex Telcar® TL-2363B Thermoplastic Elastomer Availability: North America Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weath.. |
|||
Injection Pressure | 1.38 - 6.89 MPa | 200 - 1000 psi | |
Teknor Apex Telcar® TL-2540F Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Injection Pressure | 1.38 - 6.89 MPa | 200 - 1000 psi | |
Teknor Apex Telcar® TL-2580F Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Injection Pressure | 1.38 - 6.89 MPa | 200 - 1000 psi | |
Teknor Apex Telcar® TL-2596B Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Injection Pressure | 1.38 - 6.89 MPa | 200 - 1000 psi | |
Teknor Apex Telcar® TL-2625C Thermoplastic Elastomer Uses: Consumer Applications; General Purpose; Gaskets; Handles; Personal Care; Toys Forms: Pellets Processing Method: Extrusion; Injection Molding Injection Notes: Injection Rate: Moderate-Fast Ext.. |
|||
Injection Pressure | 1.38 - 6.89 MPa | 200 - 1000 psi | |
Teknor Apex Telcar® TL-2683A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Injection Pressure | 1.38 - 6.89 MPa | 200 - 1000 psi | |
Teknor Apex Telcar® TL-340-S Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Injection Pressure | 1.38 - 6.89 MPa | 200 - 1000 psi | |
Teknor Apex Telcar® TL-3954-90 Thermoplastic Elastomer Uses: Appliance Wire Insulation; Appliance Wire Jacketing; Cable Jacketing; Connectors; Flexible Cord Jacketing; Industrial Cable Insulation; Terminal Cable Jacketing; Underground Power Cable; Wire .. |
|||
Injection Pressure | 1.38 - 6.89 MPa | 200 - 1000 psi | |
Teknor Apex Telcar® TL-4002 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Injection Pressure | 1.38 - 6.89 MPa | 200 - 1000 psi | |
Teknor Apex Telcar® TL-6055 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Injection Pressure | 1.38 - 6.89 MPa | 200 - 1000 psi | |
Teknor Apex Telcar® TL-88-N873K BLK 111 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Injection Pressure | 1.38 - 6.89 MPa | 200 - 1000 psi | |
Teknor Apex Uniprene® UN-1674C Thermoplastic Vulcanizate Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex.. |
|||
Injection Pressure | 1.38 - 6.89 MPa | 200 - 1000 psi | |
Teknor Apex Telcar® TL-2270A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Injection Pressure | 1.38 - 6.89 MPa | 200 - 1000 psi | |
Teknor Apex Telcar® TL-2519F Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Injection Pressure | 1.38 - 6.89 MPa | 200 - 1000 psi | |
Teknor Apex Uniprene® UN-7100-64 Thermoplastic Vulcanizate Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex.. |
|||
Injection Pressure | 2.07 - 6.89 MPa | 300 - 1000 psi | |
CPT C-Flex® R70-003 Opaque Biocompatible TPE C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current.. |