Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Specific Gravity = 0.920 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Specific Gravity 0.920 g/cc
0.920 g/cc
ASTM D792
Polimeri Europa Europrene® SOL T 9131 Styrene - Isoprene Block Copolymer
Europrene® SOL T 9131 is a linear block copolymer obtained by anionic polymerization. The polymer is based on styrene and isoprene, where bound styrene content is 15% weight and diblock content is..
Specific Gravity 0.920 g/cc
0.920 g/cc
ISO 1183
Solvay Engineered Polymers DEXFLEX® 990 TPO  (discontinued **)
Description: DEXFLEX® 990 is a thermoplastic olefinic elastomer (TPO) designed for automotive exterior applications that require a combination of stiffness, low-temperature impact, and excellent pr..
Specific Gravity 0.920 g/cc
0.920 g/cc
ASTM D792
LTL Color Compounds ColorRxâ„¢ PE3-0202ARX Biocompatible, Antimicrobial LDPE
A biocompatible Low Density Polyethylene for healthcare applications containing antimicrobial protection.All information provided by LTL Color Compounders, Inc.
Specific Gravity 0.920 g/cc
0.920 g/cc
ASTM D792
LTL Color Compounds ColorRxâ„¢ PE3-0205ARX Biocompatible, Antimicrobial LDPE
A biocompatible Low Density Polyethylene for healthcare applications containing a high level of antimicrobial protection for FDA regulated medical devices.All information provided by LTL Color Compo..
Specific Gravity 0.920 g/cc
0.920 g/cc
ASTM D4025
Kraton® D1117 P (SIS) Linear Triblock Copolymer
Description: Kraton D1117 P is a clear, linear triblock copolymer based on styrene and isoprene with a polystyrene content of 17%. It is supplied from North America in the physical form identified: ..
Specific Gravity 0.920 g/cc
0.920 g/cc
ASTM D4025
Kraton® D1161 P (SIS) Linear Triblock Copolymer
Description: Kraton D1161 P is a clear, linear triblock copolymer based on styrene and isoprene, with a polystyrene content of 15%. It is supplied from North America in the physical form identified:..
Specific Gravity 0.920 g/cc
0.920 g/cc
ASTM D4025
Kraton® D1183 P (SIS) Linear Block Copolymer
Description: Kraton D1183 P is a clear, linear block copolymer based on styrene and isoprene with a polystyrene content of 16%. It is supplied from North America in the physical form identified: Kra..
Specific Gravity 0.920 g/cc
0.920 g/cc
ISO 2781
Kraton® G1654 E (SEBS) Linear Triblock Copolymer
Description: Kraton G1654 E polymer is a clear, linear triblock copolymer based on styrene and ethylene/butylene, S-E/B-S, with bound styrene of 30% mass. It is supplied from Europe in the physical ..
Specific Gravity 0.920 g/cc
0.920 g/cc
ASTM D4025
Kraton® D1114 P (SIS) Linear Triblock Copolymer
Description: Kraton D1114 P is a clear, linear triblock copolymer based on styrene and isoprene with a polystyrene content of 19%. It is supplied from North America in the physical form identified: ..
Specific Gravity 0.920 g/cc
0.920 g/cc
ISO 1183
Kuraray SEPTON® S8006 Thermoplastic Rubber
SEPTON® is a series of high performance thermoplastic rubbers developed by Kuraray Co. Ltd. using its isoprene technology. SEPTON® resins are hydrogenated styrenic block copolymers, which exhi..
Specific Gravity 0.920 g/cc
0.920 g/cc
ASTM 792
Multibase Multi-Flex® A 7606 TPE Thermoplastic Elastomer
Features: Chemical Resistance, Good Heat StabilizedOzone ResistantGeneral Purpose Friction, Low Processability, Good Forms:PelletsProcessing Method:ExtrusionInjection Molding Uses: Automotive App..
Specific Gravity 0.920 g/cc
0.920 g/cc
ASTM D792
STAR Thermoplastic Alloys & Rubbers StarTUFF TF 45-LR-9 TPE
Product Description: StarTUFF TF 45-LR-9 is an easy processing TPE designed for injection molding Features:Soft TouchRubbery FeelHigh Tear strengthHigh Tensile strengthProcessing Method: Injection M..
Specific Gravity 0.920 g/cc
0.920 g/cc
+/- 0.02; ASTM D792
Teknor Apex TELCAR® 1000-92 Thermoplastic Elastomer
Information provided by Teknor Apex Company
Specific Gravity 0.920 g/cc
0.920 g/cc
ASTM D792
Teknor Apex Telcar® 95-T0769V-90NT Ethylene Vinyl Acetate Copolymer
Notes: The Specialty Compounding Division offers a proprietary line of cap-liner compounds designed for carbonated soft drinks. These are proven products that have been used commercially for several..
Specific Gravity 0.920 g/cc
0.920 g/cc
ASTM D792
Teknor Apex Telcar® TL-1000-105 Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P..
Specific Gravity 0.920 g/cc
0.920 g/cc
ASTM D792
Teknor Apex Uniprene® UN-2028A UMB Thermoplastic Elastomer
Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex..
Specific Gravity 0.920 g/cc
0.920 g/cc
ASTM D792
A. Schulman POLYBATCH™ Green 30394 Concentrate Based In LDPE
DescriptionPOLYBATCH® 30394 is a green color concentrate based in LDPE. This concentrate was designed to provide color in blow molding applications. POLYBATCH® 30394 is typically recommended for..
Specific Gravity 0.920 g/cc
0.920 g/cc
15.6°C; ASTM D1298
ExxonMobil Mobil Vaculine 548
Mobil Vacuoline 500 Series are extra high performance heavy duty circulating oils specifically designed to meet the critical requirements of the Morgan Construction Companys high speed No-Twist® Ro..
Specific Gravity 0.920 g/cc
0.920 g/cc
ASTM D5
Westlake Epolene® N-15 Nonemulsifiable - Low Molecular Weight Polypropylene Polymer
Product Description: Epolene N-15 is a low viscosity polypropylene homopolymer with a high melt point and excellent hardness. Epolene N-15 is used in color concentrates, toner compounds, and as a pi..
Specific Gravity 0.920 g/cc
0.920 g/cc
ISO 1183/1
A. Schulman INVISION™ VX-5170UE Soft Touch Polyolefin Thermoplastic
DescriptionInvision™ VX-5170UE is a UV-stabilized polyolefin-based thermoplastic elastomer of 70 Shore A durometer, which has been formulated for easy processability, soft touch, low gloss, and exc..
Specific Gravity 0.920 g/cc
0.920 g/cc
ASTM D792
A. Schulman POLYBATCH™ CE-505-E Concentrate Based In Polyethylene
DescriptionPOLYBATCH® CE-505-E is a 5% erucamide slip concentrate based in polyethylene. This concentrate is designed to reduce film COF in LDPE, LLDPE, and mPE cast and blown films. POLYBATCH® ..
Specific Gravity 0.920 g/cc
0.920 g/cc
ASTM D792
Teknor Apex Telcar® TL-86-K986T-98 Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
Specific Gravity 0.920 g/cc
0.920 g/cc
ASTM D 792
RTP Company PermaStat® 100 LE Polypropylene (PP), Permanently Anti-static - ESD Protection - Low Extractables
Specific Gravity 0.920 g/cc
0.920 g/cc
23°C; ASTM D792
ExxonMobil Santoprene® 121-55W241 Thermoplastic Elastomer
A soft, black, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in difficult ..
Specific Gravity 0.920 g/cc
0.920 g/cc
23°C; ASTM D792
ExxonMobil Santoprene® 8223-30M300 Thermoplastic Elastomer
A hard, colorable, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material is designed for automotive interior applications requiring low fogging and ..
Specific Gravity 0.920 g/cc
0.920 g/cc
15.6°C; ASTM D1298
ExxonMobil Mobil Vaculine 548
Mobil Vacuoline 500 Series are extra high performance heavy duty circulating oils specifically designed to meet the critical requirements of the Morgan Construction Companys high speed No-Twist® Ro..
Specific Gravity 0.920 g/cc
0.920 g/cc
ASTM D792
Cheng Yu Plastic 3276 TPE Rubber
Specific Gravity 0.920 g/cc
0.920 g/cc
ASTM D1505/D792
Braskem Green PE SLH0820/30AF Blow Film Extrusion and Cast Film Extrusion Linear Low Density Polyethylene
Description: SLH0820/30AF is a LLDPE hexene copolymer produced by Braskem. It offers outstanding processability combined with excellent mechanical properties. Very low gel amount. The minimum biobas..
Specific Gravity 0.920 - 0.926 g/cc
0.920 - 0.926 g/cc
ASTM D792
Aaron Industries AVPE LD 300-1 Virgin Polyethylene
Melt flow index may be specified.
Specific Gravity 0.920 g/cc
0.920 g/cc
ASTM D792
A. Schulman POLYTROPE™ TPP 504 Injection Molding Grade Olefinic Thermoplastic Elastomer
DescriptionPolytrope TPP 504 is an injection molding grade olefinic thermoplastic elastomer. This product is recommended for parts requiring flexibility and high impact strength at sub-ambient temp..
Copyright © lookpolymers.com All Rights Reserved