Processing Properties | Metric | English | Comments |
---|---|---|---|
Injection Pressure | 1.38 - 5.52 MPa | 200 - 800 psi | |
Teknor Apex Monprene® MP 1061 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Injection Pressure | 1.38 - 5.52 MPa | 200 - 800 psi | |
Teknor Apex Monprene® MP 1079E Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Injection Pressure | 1.38 - 5.52 MPa | 200 - 800 psi | |
Teknor Apex Monprene® MP 1097 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Injection Pressure | 1.38 - 5.52 MPa | 200 - 800 psi | |
Teknor Apex Monprene® MP 1097D Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Injection Pressure | 1.38 - 5.52 MPa | 200 - 800 psi | |
Teknor Apex Monprene® MP-1766B Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Injection Pressure | 1.38 - 5.52 MPa | 200 - 800 psi | |
Teknor Apex Monprene® MP-1848R Thermoplastic Elastomer Uses: Wire and Cable ApplicationsForms: Pellets Processing Method: Extrusion; Injection Molding Injection Notes: Drying is not necessary. However, if moisture is a problem, dry the pellets for 2 to.. |
|||
Injection Pressure | 1.38 - 5.52 MPa | 200 - 800 psi | |
Teknor Apex Monprene® MP-1871 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Injection Pressure | 1.38 - 5.52 MPa | 200 - 800 psi | |
Teknor Apex Monprene® MP-1888 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Injection Pressure | 1.38 - 5.52 MPa | 200 - 800 psi | |
Teknor Apex Monprene® MP-2024A Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Injection Pressure | 1.38 - 5.52 MPa | 200 - 800 psi | |
Teknor Apex Monprene® MP-2132 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Injection Pressure | 1.38 - 5.52 MPa | 200 - 800 psi | |
Teknor Apex Monprene® MP-2322UV Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Injection Pressure | 1.38 - 5.52 MPa | 200 - 800 psi | |
Teknor Apex Monprene® MP-2328 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Injection Pressure | 1.38 - 5.52 MPa | 200 - 800 psi | |
Teknor Apex Monprene® MP-1349A Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Injection Pressure | 1.38 - 5.52 MPa | 200 - 800 psi | |
Teknor Apex Monprene® MP-2455S Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Injection Pressure | 1.38 - 5.52 MPa | 200 - 800 psi | |
Teknor Apex Monprene® MP-2664A Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Injection Pressure | 1.38 - 5.52 MPa | 200 - 800 psi | |
Teknor Apex Monprene® MP-2676 UV Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Injection Pressure | 1.38 - 5.52 MPa | 200 - 800 psi | |
Teknor Apex Monprene® MP-2720 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Injection Pressure | 1.38 - 5.52 MPa | 200 - 800 psi | |
Teknor Apex Monprene® MP-2955 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Injection Pressure | 1.38 - 6.89 MPa | 200 - 1000 psi | |
Teknor Apex Telcar® OBC 4876N Thermoplastic Elastomer Uses: Flexible Grips; Overmolding; Soft Touch Applications Forms: Pellets Processing Method: Extrusion; Injection Molding Injection Notes: Injection Rate: Moderate-Fast Extrusion Notes: Screw Speed:.. |
|||
Injection Pressure | 1.38 - 6.89 MPa | 200 - 1000 psi | |
Teknor Apex Telcar® TL-1154A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Injection Pressure | 1.38 - 6.89 MPa | 200 - 1000 psi | |
Teknor Apex Telcar® TL-1425A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Injection Pressure | 1.38 - 6.89 MPa | 200 - 1000 psi | |
Teknor Apex Telcar® TL-2635B Thermoplastic Elastomer Uses: Building Materials; Flexible Grips; General Purpose; Handles; Safety Equipment; Toys Injection Notes: Injection Rate: Moderate-Fast Extrusion Notes: Screw Speed: 30 to 100 rpmInformation Provi.. |
|||
Injection Pressure | 1.38 - 6.89 MPa | 200 - 1000 psi | |
Teknor Apex Telcar® TL-83-F912-UV Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Injection Pressure | 1.38 - 6.89 MPa | 200 - 1000 psi | |
Teknor Apex Telcar® TL-91-T3056S-75 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Injection Pressure | 1.38 - 6.89 MPa | 200 - 1000 psi | |
Teknor Apex Uniprene® UN-7010-45NT Thermoplastic Vulcanizate Notes: Injection Rate: Fast Uses: Gaskets; Glazing; Grommets; Medical Pump Seals; Medical/Healthcare Applications; Plugs; Shock Absorbing Pads; Tubing Agency Ratings: NSF 61 Forms: Pellets Processin.. |
|||
Injection Pressure | 1.38 - 6.89 MPa | 200 - 1000 psi | |
Teknor Apex Uniprene® UN-7100-87 Thermoplastic Vulcanizate Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex.. |
|||
Injection Pressure | 1.38 - 6.89 MPa | 200 - 1000 psi | |
Teknor Apex Telcar® TL-86-K986T-98 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Injection Pressure | 1.38 - 6.89 MPa | 200 - 1000 psi | |
Teknor Apex Uniprene® UN-2420A Thermoplastic Vulcanizate Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex.. |
|||
Injection Pressure | 1.38 - 5.52 MPa | 200 - 800 psi | |
Teknor Apex Monprene® MP-2830M UV Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |