Processing Properties | Metric | English | Comments |
---|---|---|---|
Zone 2 | 177 - 193 °C | 350 - 380 °F | |
LyondellBasell Petrothene® GA808091 Linear Low Density Polyethylene ApplicationsPETROTHENE GA 808-091 is a broad molecular weight, linear low density polyethylene resin designed for use as a base resin in wire and cable jacketing. An antioxidant package is added to.. |
|||
Zone 2 | 177 - 193 °C | 350 - 380 °F | |
LyondellBasell Petrothene® HR92953 Medium Density Polyethylene ApplicationsPETROTHENE HR 92953 is a medium density polyethylene-based resin designed for use as jacketing for communications cable, including CATV and FOC. HR 92953 has a nominal carbon black cont.. |
|||
Zone 2 | 177 - 193 °C | 350 - 380 °F | |
LyondellBasell Petrothene® PR92735 Linear Low Density Polyethylene ApplicationsPETROTHENE PR 92735 is a high molecular weight, linear low density-based compound designed for cable jacketing. PR 92735 contains a nominal carbon black content of 2.6% and antioxidant .. |
|||
Zone 2 | 171 - 193 °C | 340 - 380 °F | |
Teknor Apex Telcar® OBC 4530A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Zone 2 | 171 - 193 °C | 340 - 380 °F | |
Teknor Apex Telcar® TL EF-6123 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Zone 2 | 171 - 193 °C | 340 - 380 °F | |
Teknor Apex Telcar® TL-1025-72 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; Closures; General Purpose; Grommets; Weatherstripping Forms:.. |
|||
Zone 2 | 171 - 193 °C | 340 - 380 °F | |
Teknor Apex Telcar® TL-1050-75 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Zone 2 | 171 - 193 °C | 340 - 380 °F | |
Teknor Apex Telcar® TL-1120E Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Zone 2 | 171 - 193 °C | 340 - 380 °F | |
Teknor Apex Telcar® TL-1183A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Zone 2 | 171 - 193 °C | 340 - 380 °F | |
Teknor Apex Telcar® TL-1435A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Zone 2 | 171 - 193 °C | 340 - 380 °F | |
Teknor Apex Telcar® TL-1520C Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Zone 2 | 171 - 193 °C | 340 - 380 °F | |
Teknor Apex Telcar® TL-1522B Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Zone 2 | 171 - 193 °C | 340 - 380 °F | |
Teknor Apex Telcar® TL-1524F Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Zone 2 | 171 - 193 °C | 340 - 380 °F | |
Teknor Apex Telcar® TL-1536D Thermoplastic Elastomer Uses: Consumer Applications; General Purpose; Household Goods; Food Containers; Handles; Lids Forms: Pellets Processing Method: Extrusion; Injection Molding Injection Notes: Injection Rate: Moderat.. |
|||
Zone 2 | 171 - 193 °C | 340 - 380 °F | |
Teknor Apex Telcar® TL-1934C Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Zone 2 | 171 - 193 °C | 340 - 380 °F | |
Teknor Apex Telcar® TL-2439D Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Zone 2 | 171 - 193 °C | 340 - 380 °F | |
Teknor Apex Telcar® TL-2448G Thermoplastic Elastomer Uses: Consumer Applications; Flexible Grips; General Purpose; Handles; Safety Equipment; Toys Forms: Pellets Processing Method: Extrusion; Injection Molding Injection Notes: Injection Rate: Moderat.. |
|||
Zone 2 | 171 - 193 °C | 340 - 380 °F | |
Teknor Apex Telcar® TL-2452L Thermoplastic Elastomer Uses: Consumer Applications; Flexible Grips; General Purpose; Handles; Safety Equipment; Toys Forms: Pellets Processing Method: Extrusion; Injection Molding Injection Notes: Injection Rate: Moderat.. |
|||
Zone 2 | 171 - 193 °C | 340 - 380 °F | |
Teknor Apex Telcar® TL-2535F Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Zone 2 | 171 - 193 °C | 340 - 380 °F | |
Teknor Apex Telcar® TL-2590F Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Zone 2 | 171 - 193 °C | 340 - 380 °F | |
Teknor Apex Telcar® TL-2651A Thermoplastic Elastomer Uses: Flexible Grips; Footwear; General Purpose; Grommets; Handles; Industrial Applications; Soft Touch Applications; Toys Injection Notes: Injection Rate: Moderate-Fast Extrusion Notes: Screw Speed.. |
|||
Zone 2 | 171 - 193 °C | 340 - 380 °F | |
Teknor Apex Telcar® TL-2683A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Zone 2 | 171 - 193 °C | 340 - 380 °F | |
Teknor Apex Telcar® TL-3260R Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Zone 2 | 171 - 193 °C | 340 - 380 °F | |
Teknor Apex Telcar® TL-340-S Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Zone 2 | 171 - 193 °C | 340 - 380 °F | |
Teknor Apex Telcar® TL-4001 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Zone 2 | 171 - 193 °C | 340 - 380 °F | |
Teknor Apex Telcar® TL-83-F912-G Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Zone 2 | 171 - 193 °C | 340 - 380 °F | |
Teknor Apex Telcar® TL-86-K875-F Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Zone 2 | 171 - 193 °C | 340 - 380 °F | |
Teknor Apex Telcar® TL-91-T3056S-75 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Zone 2 | 171 - 193 °C | 340 - 380 °F | |
Teknor Apex Telcar® TL-97-T0207A-110 Thermoplastic Elastomer Uses: Automotive Applications; Industrial Cable Insulation Forms: Pellets Processing Method: Extrusion; Injection Molding Injection Notes: Injection Rate: Moderate-Fast Extrusion Notes: Screw Speed:.. |
|||
Zone 2 | 171 - 193 °C | 340 - 380 °F | |
Teknor Apex Telcar® TELC 1025-70 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |