Processing Properties | Metric | English | Comments |
---|---|---|---|
Zone 3 | 171 - 199 °C | 340 - 390 °F | |
Lubrizol Advanced Materials PEARLTHANE® 12K85LB Thermoplastic Polyurethane Elastomer
(discontinued **) PEARLTHANE® 12K85 LB is a standard polyester-based TPU with a lubricating additive, supplied in form of translucent, colourless or slightly yellowish pellets, combining hardness with excellent mech.. |
|||
Zone 3 | 177 - 199 °C | 350 - 390 °F | |
Teknor Apex Telcar® OBC 4555A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Zone 3 | 177 - 199 °C | 350 - 390 °F | |
Teknor Apex Telcar® OBC 4560A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Zone 3 | 177 - 199 °C | 350 - 390 °F | |
Teknor Apex Telcar® OBC 4565A Thermoplastic Elastomer Uses: Flexible Grips; Overmolding Forms: Pellets Processing Method: Blow Molding; Profile Extrusion; Sheet Extrusion; Thermoforming; Wire and Cable Extrusion; Extrusion; Injection Molding Injection .. |
|||
Zone 3 | 177 - 199 °C | 350 - 390 °F | |
Teknor Apex Telcar® OBC 4773A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Zone 3 | 177 - 199 °C | 350 - 390 °F | |
Teknor Apex Telcar® OBC 4855A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Zone 3 | 177 - 199 °C | 350 - 390 °F | |
Teknor Apex Telcar® TL EF-6123 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Zone 3 | 177 - 199 °C | 350 - 390 °F | |
Teknor Apex Telcar® TL EF-6155 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Zone 3 | 177 - 199 °C | 350 - 390 °F | |
Teknor Apex Telcar® TL EF-6162 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Zone 3 | 177 - 199 °C | 350 - 390 °F | |
Teknor Apex Telcar® TL EF-6177B-UV Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Zone 3 | 177 - 199 °C | 350 - 390 °F | |
Teknor Apex Telcar® TL-1000-92-UV Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Automotive Spec.. |
|||
Zone 3 | 177 - 199 °C | 350 - 390 °F | |
Teknor Apex Telcar® TL-1025-72 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; Closures; General Purpose; Grommets; Weatherstripping Forms:.. |
|||
Zone 3 | 177 - 199 °C | 350 - 390 °F | |
Teknor Apex Telcar® TL-1025-85 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Zone 3 | 177 - 199 °C | 350 - 390 °F | |
Teknor Apex Telcar® TL-1081A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Zone 3 | 177 - 199 °C | 350 - 390 °F | |
Teknor Apex Telcar® TL-1155B Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Zone 3 | 177 - 199 °C | 350 - 390 °F | |
Teknor Apex Telcar® TL-1268A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Zone 3 | 177 - 199 °C | 350 - 390 °F | |
Teknor Apex Telcar® TL-1269B Thermoplastic Elastomer Uses: Consumer Applications; Handles; Packaging; General Purpose; Kitchenware; Toothbrush Handles Forms: Pellets Processing Method: Extrusion; Injection Molding Injection Notes: Injection Rate: Mode.. |
|||
Zone 3 | 177 - 199 °C | 350 - 390 °F | |
Teknor Apex Telcar® TL-1427A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Zone 3 | 177 - 199 °C | 350 - 390 °F | |
Teknor Apex Telcar® TL-1472A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Zone 3 | 177 - 199 °C | 350 - 390 °F | |
Teknor Apex Telcar® TL-2535F Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Zone 3 | 177 - 199 °C | 350 - 390 °F | |
Teknor Apex Telcar® TL-2590F Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Zone 3 | 177 - 199 °C | 350 - 390 °F | |
Teknor Apex Telcar® TL-2635A Thermoplastic Elastomer Uses: Building Materials; Flexible Grips; General Purpose; Handles; Safety Equipment; Toys Injection Notes: Injection Rate: Moderate-Fast Extrusion Notes: Screw Speed: 30 to 100 rpmInformation Provi.. |
|||
Zone 3 | 177 - 199 °C | 350 - 390 °F | |
Teknor Apex Telcar® TL-3260-1 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Zone 3 | 177 - 199 °C | 350 - 390 °F | |
Teknor Apex Telcar® TL-3954-80 Thermoplastic Elastomer Uses: Appliance Wire Insulation; Appliance Wire Jacketing; Cable Jacketing; Connectors; Flexible Cord Jacketing; Industrial Cable Insulation; Terminal Cable Jacketing; Underground Power Cable; Wire .. |
|||
Zone 3 | 177 - 199 °C | 350 - 390 °F | |
Teknor Apex Telcar® TL-6075 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Zone 3 | 177 - 199 °C | 350 - 390 °F | |
Teknor Apex Telcar® TL-86-K875-F Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Zone 3 | 177 - 199 °C | 350 - 390 °F | |
Teknor Apex Telcar® TL-8712R Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Zone 3 | 177 - 199 °C | 350 - 390 °F | |
Teknor Apex Telcar® TL-87-L832A Thermoplastic Elastomer Notes: UV Stabilized Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstrip.. |
|||
Zone 3 | 177 - 199 °C | 350 - 390 °F | |
Teknor Apex Telcar® TL-2270A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Zone 3 | 177 - 199 °C | 350 - 390 °F | |
Teknor Apex Telcar® TL-8732 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |