Processing Properties | Metric | English | Comments |
---|---|---|---|
Zone 3 | 177 - 199 °C | 350 - 390 °F | |
Teknor Apex Telcar® OBC 4465A Thermoplastic Elastomer Uses: Blow Molding Applications; General Purpose; Soft Touch Applications Forms: Pellets Processing Method: Blow Molding; Profile Extrusion; Sheet Extrusion; Thermoforming; Wire and Cable Extrusion;.. |
|||
Zone 3 | 177 - 199 °C | 350 - 390 °F | |
Teknor Apex Telcar® OBC 4555A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Zone 3 | 177 - 199 °C | 350 - 390 °F | |
Teknor Apex Telcar® TL-1000-95 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Zone 3 | 177 - 199 °C | 350 - 390 °F | |
Teknor Apex Telcar® TL-1017A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Zone 3 | 177 - 199 °C | 350 - 390 °F | |
Teknor Apex Telcar® TL-1120E Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Zone 3 | 177 - 199 °C | 350 - 390 °F | |
Teknor Apex Telcar® TL-1137 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Zone 3 | 177 - 199 °C | 350 - 390 °F | |
Teknor Apex Telcar® TL-1267A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Zone 3 | 177 - 199 °C | 350 - 390 °F | |
Teknor Apex Telcar® TL-2318G Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Zone 3 | 177 - 199 °C | 350 - 390 °F | |
Teknor Apex Telcar® TL-2433A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Zone 3 | 177 - 199 °C | 350 - 390 °F | |
Teknor Apex Telcar® TL-2478K Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Zone 3 | 177 - 199 °C | 350 - 390 °F | |
Teknor Apex Telcar® TL-2545A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Zone 3 | 177 - 199 °C | 350 - 390 °F | |
Teknor Apex Telcar® TL-2555A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Zone 3 | 177 - 199 °C | 350 - 390 °F | |
Teknor Apex Telcar® TL-2575A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Zone 3 | 177 - 199 °C | 350 - 390 °F | |
Teknor Apex Telcar® TL-2580F Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Zone 3 | 177 - 199 °C | 350 - 390 °F | |
Teknor Apex Telcar® TL-2585A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Zone 3 | 177 - 199 °C | 350 - 390 °F | |
Teknor Apex Telcar® TL-2635B Thermoplastic Elastomer Uses: Building Materials; Flexible Grips; General Purpose; Handles; Safety Equipment; Toys Injection Notes: Injection Rate: Moderate-Fast Extrusion Notes: Screw Speed: 30 to 100 rpmInformation Provi.. |
|||
Zone 3 | 177 - 199 °C | 350 - 390 °F | |
Teknor Apex Telcar® TL-2635D Thermoplastic Elastomer Uses: Building Materials; Flexible Grips; General Purpose; Handles; Safety Equipment; Toys Injection Notes: Injection Rate: Moderate-Fast Extrusion Notes: Screw Speed: 30 to 100 rpmInformation Provi.. |
|||
Zone 3 | 177 - 199 °C | 350 - 390 °F | |
Teknor Apex Telcar® TL-2696A Thermoplastic Elastomer Uses: Cell Phones; Consumer Applications; General Purpose; Handles; Toys Forms: Pellets Processing Method: Extrusion; Injection Molding Injection Notes: Injection Rate: Moderate-Fast Extrusion Notes.. |
|||
Zone 3 | 177 - 199 °C | 350 - 390 °F | |
Teknor Apex Telcar® TL-3954-50 Thermoplastic Elastomer Uses: Appliance Wire Insulation; Appliance Wire Jacketing; Cable Jacketing; Connectors; Flexible Cord Jacketing; Industrial Cable Insulation; Terminal Cable Jacketing; Underground Power Cable; Wire .. |
|||
Zone 3 | 177 - 199 °C | 350 - 390 °F | |
Teknor Apex Telcar® TL-4001A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Zone 3 | 177 - 199 °C | 350 - 390 °F | |
Teknor Apex Telcar® TL-6045 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Zone 3 | 177 - 199 °C | 350 - 390 °F | |
Teknor Apex Telcar® TL-6085 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Zone 3 | 177 - 199 °C | 350 - 390 °F | |
Teknor Apex Telcar® TL-87-L832A Thermoplastic Elastomer Notes: UV Stabilized Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstrip.. |
|||
Zone 3 | 177 - 199 °C | 350 - 390 °F | |
Teknor Apex Telcar® TL-91-T3056S-75 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Zone 3 | 177 - 199 °C | 350 - 390 °F | |
Teknor Apex Telcar® TL-2468A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Zone 3 | 177 - 199 °C | 350 - 390 °F | |
Teknor Apex Telcar® TL-2519F Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Zone 3 | 177 - 199 °C | 350 - 390 °F | |
Teknor Apex Telcar® TL-2683D Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Zone 3 | 177 - 199 °C | 350 - 390 °F | |
Teknor Apex Telcar® TL-86-K986T-98 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Zone 3 | 177 - 199 °C | 350 - 390 °F | |
Teknor Apex Telcar® TL-8732R Thermoplastic Elastomer Notes: RoHS Compliant Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstri.. |
|||
Zone 3 | 193 - 199 °C | 379 - 390 °F | Extrusion |
Lubrizol Estane® 58280 Thermoplastic Polyurethane Type: Estane® 58280 is a polyether-type thermoplastic polyurethane (TPU) compound.Features: High resiliency compound, with unique physical properties such as low tensile and compression set, high r.. |