Processing Properties | Metric | English | Comments |
---|---|---|---|
Mold Temperature | 25.0 - 50.0 °C | 77.0 - 122 °F | |
Huntsman AVALON® 80 ABU Thermoplastic Polyurethane Introduction: AVALON 80 ABU is a high performance UV-stabilized polyester based thermoplastic polyurethane for injection molding. AVALON 80 ABU is part of the AVALON Perform Range and offers a premi.. |
|||
Mold Temperature | 25.0 - 50.0 °C | 77.0 - 122 °F | Injection |
Huntsman IROGRAN® A 85 H 4827 TPU-Polyester Introduction: IROGRAN A 85 H 4827 is a thermoplastic polyester polyurethane for injection molding applications. IROGRAN A 85 H 4827 is part of the HUNTSMAN technical injection molding product range .. |
|||
Mold Temperature | 25.0 - 40.0 °C | 77.0 - 104 °F | |
Kraiburg TPE THERMOLAST® K TA8HAI Injection Molding TPE Compound easy printable, paintable, glueable without pretreatmentColorable in any shadeSubstitution for PVC and silicone rubberTypical Applications: ToysBaby productsPromotion articlesMaterial Advan.. |
|||
Mold Temperature | 25.0 - 40.0 °C | 77.0 - 104 °F | Injection |
Kraiburg TPE THERMOLAST® K TC4GPN Thermoplastic Elastomer, General purpose The GP/FG Series is recommended for a variety of different applications. It is particularly appropriate for passenger compartments. The compounds are available in natural and black colors. Typical a.. |
|||
Mold Temperature | 25.0 - 40.0 °C | 77.0 - 104 °F | Injection |
Kraiburg TPE THERMOLAST® K TC7FRZ Thermoplastic Elastomer, Flame retardant The FR Series is recommended for applications requiring high flame retardance. The compounds are halogen free and available in natural and black colors. Typical applications: Cable holders Seals for.. |
|||
Mold Temperature | 25.0 - 40.0 °C | 77.0 - 104 °F | Injection |
Kraiburg TPE THERMOLAST® K TP6CDB Thermoplastic Elastomer, Adhesion to PP The EX Series is recommended for extrusion applications such as door seals and window gaskets. The compounds are available in natural and black colors. Typical applications: Edge guardsProfiles for .. |
|||
Mold Temperature | 25.0 - 40.0 °C | 77.0 - 104 °F | Injection |
Kraiburg TPE THERMOLAST® K TP6CDZ Thermoplastic Elastomer, Adhesion to PP The EX Series is recommended for extrusion applications such as door seals and window gaskets. The compounds are available in natural and black colors. Typical applications: Edge guardsProfiles for .. |
|||
Mold Temperature | 25.0 - 40.0 °C | 77.0 - 104 °F | Injection |
Kraiburg TPE THERMOLAST® K TC6GPN Thermoplastic Elastomer, General purpose The GP/FG Series is recommended for a variety of different applications. It is particularly appropriate for passenger compartments. The compounds are available in natural and black colors. Typical a.. |
|||
Mold Temperature | 25.0 - 40.0 °C | 77.0 - 104 °F | |
Kraiburg TPE THERMOLAST® K TF3BNA Thermoplastic Elastomer The FC/AP Series is a natural-colored and translucent material solution for applications with food contact. The series’ features include excellent adhesion to PP. Typical applications: Function.. |
|||
Mold Temperature | 25.0 - 40.0 °C | 77.0 - 104 °F | |
Kraiburg TPE THERMOLAST® K TF8BNA Thermoplastic Elastomer The FC/AP Series is a natural-colored and translucent material solution for applications with food contact. The series’ features include excellent adhesion to PP. Typical applications: Function.. |
|||
Mold Temperature | 25.0 - 40.0 °C | 77.0 - 104 °F | Injection Molding |
Stellarchem AB-860LG TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Mold Temperature | 25.0 - 40.0 °C | 77.0 - 104 °F | Injection Molding |
Stellarchem GP-930 TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Mold Temperature | 25.0 - 40.0 °C | 77.0 - 104 °F | Injection Molding |
Stellarchem GP-980 TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Mold Temperature | 25.0 - 65.6 °C | 77.0 - 150 °F | |
Teknor Apex Telcar® OBC 4465A Thermoplastic Elastomer Uses: Blow Molding Applications; General Purpose; Soft Touch Applications Forms: Pellets Processing Method: Blow Molding; Profile Extrusion; Sheet Extrusion; Thermoforming; Wire and Cable Extrusion;.. |
|||
Mold Temperature | 25.0 - 65.6 °C | 77.0 - 150 °F | |
Teknor Apex Telcar® OBC 4530A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Mold Temperature | 25.0 - 65.6 °C | 77.0 - 150 °F | |
Teknor Apex Telcar® OBC 4560A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Mold Temperature | 25.0 - 65.6 °C | 77.0 - 150 °F | |
Teknor Apex Telcar® TL EF-6177B-UV Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Mold Temperature | 25.0 - 65.6 °C | 77.0 - 150 °F | |
Teknor Apex Telcar® TL-1140D BLK Thermoplastic Elastomer Uses: Automotive Applications; Automotive Interior Parts; Blow Molding Applications; Carpet Backing; General Purpose; Grommets; Weatherstripping Forms: Pellets Processing Method: Extrusion; Injectio.. |
|||
Mold Temperature | 25.0 - 65.6 °C | 77.0 - 150 °F | |
Teknor Apex Telcar® TL-1431A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Mold Temperature | 25.0 - 65.6 °C | 77.0 - 150 °F | |
Teknor Apex Telcar® TL-1431F Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Mold Temperature | 25.0 - 65.6 °C | 77.0 - 150 °F | |
Teknor Apex Telcar® TL-1446G Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Mold Temperature | 25.0 - 65.6 °C | 77.0 - 150 °F | |
Teknor Apex Telcar® TL-2596C Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Mold Temperature | 25.0 - 65.6 °C | 77.0 - 150 °F | |
Teknor Apex Telcar® TL-83-F912-G Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Mold Temperature | 25.0 - 65.6 °C | 77.0 - 150 °F | |
Teknor Apex Telcar® TL-88-N873K BLK 111 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Mold Temperature | 25.0 - 65.6 °C | 77.0 - 150 °F | |
Teknor Apex Telcar® TL-3954-45 Thermoplastic Elastomer Uses: Appliance Wire Insulation; Appliance Wire Jacketing; Cable Jacketing; Connectors; Flexible Cord Jacketing; Industrial Cable Insulation; Terminal Cable Jacketing; Underground Power Cable; Wire .. |
|||
Mold Temperature | 25.0 - 60.0 °C | 77.0 - 140 °F | |
Arkema Group Pebax® 6333 SP 01 Polyether Block Amide (PEBA) Polyether block amide PEBAX® 6333 SP 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This SP grade has been developed to be heat and UV resistant.Information provide.. |
|||
Mold Temperature | 25.0 - 60.0 °C | 77.0 - 140 °F | Injection |
Alliance Polymers Zythane™ 5080A Thermoplastic Polyurethane Elastomer Zythane™ 5080A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Mold Temperature | 25.0 - 60.0 °C | 77.0 - 140 °F | Injection |
Alliance Polymers Zythane™ 6055D Thermoplastic Polyurethane Elastomer Zythane™ 6055D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Mold Temperature | 25.0 - 60.0 °C | 77.0 - 140 °F | Injection |
Alliance Polymers Zythane™ 6065D Thermoplastic Polyurethane Elastomer Zythane™ 6065D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Mold Temperature | 25.0 - 70.0 °C | 77.0 - 158 °F | Injection |
Huntsman IROGRAN® A 92 K 4107 TPU-High Temperature Performance Introduction: IROGRAN A92K 4107 is a caprolactone-based thermoplastic polyurethane. The material has been developed for injection molding applications requiring exceptional performance in terms of c.. |