Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 8.55 MPa @Strain 300 % |
1240 psi @Strain 300 % |
ASTM D412 |
Polymax® Maxelast® F02-081A-6C TPE, Halogen Free Extrusion Grade Characteristics: Good melt strengthSoft touchSmooth surface with dry feelGood weather and heat resistanceWide range of hardnessEasy processing Halogen FreeLow smoke emissionRoHs compliantDesigned to.. |
|||
Tensile Stress | 8.55 MPa @Strain 100 % |
1240 psi @Strain 100 % |
ASTM D412 |
Polymax® Maxelast® P3890 TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Tensile Stress | 8.55 MPa @Strain 300 % |
1240 psi @Strain 300 % |
2.0 in/min; ASTM D412 |
Teknor Apex Telcar® TL-1000-92 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Automotive Spec.. |
|||
Tensile Stress | 8.55 MPa @Strain 300 % |
1240 psi @Strain 300 % |
2.0 in/min; ASTM D412 |
Teknor Apex Telcar® TL-1000-92-UV Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Automotive Spec.. |
|||
Tensile Stress | 8.55 MPa @Strain 0.250 %, Temperature 40.0 °C |
1240 psi @Strain 0.250 %, Temperature 104 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® SK601 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) 10% Glass Reinforced Polybutylene Terephthalate Crastin SK601 NC010 is a 10% glass fiber reinforced lubricated polybutylene terephthalate resin for injection molding.Information provided by DuPont P.. |
|||
Tensile Stress | 8.55 MPa @Strain 133.56 %, Temperature 120 °C |
1240 psi @Strain 133.56 %, Temperature 248 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® G5544 Polyester Elastomer TPC-ET
(Unverified Data**) 55 Shore D Standard Performance Polyester Elastomer with Heat Ageing ProtectionHytrel G5544 is a medium modulus grade with nominal hardness of 55D. It contains discoloring stabilizer. It can be proc.. |