Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 10.3 MPa | 1490 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Wire & Cable W7400 Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Tensile Strength, Yield | 10.3 MPa | 1490 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Gravi-Tech™ GRV-UR-080-W Polyurethane, Unspecified (PUR, Unspecified) Information provided by PolyOne |
|||
Tensile Strength, Yield | 10.3 MPa | 1490 psi | ASTM D412 |
Polymax® Maxelast® F02-129E-1C TPE, Halogen Free Extrusion Grade Characteristics: Good melt strengthSoft touchSmooth surface with dry feelGood weather and heat resistanceWide range of hardnessEasy processing Halogen FreeLow smoke emissionRoHs compliantDesigned to.. |
|||
Tensile Strength, Yield | 10.3 MPa | 1490 psi | ASTM D412 |
Precision Polymer Engineering H70B Epichlorohydrin Peroxide Cured, Epichlorohydrin Rubber, 65-75 °IRHD. Terpolymer of epichlorohydrin, ethylene oxide and an unsaturated monomer. ASTM and ISO designation = GECO.Applications: Excellent resistance t.. |
|||
Tensile Strength, Yield | 10.3 MPa | 1490 psi | ASTM D638 |
NOVA Chemicals Novapol® LA-0224-A LDPE Foam Resin Excellent stiffness, Moderate toughness, Easy processabilityApplications: Industrial packaging, Liners, Blends with LLDPE, Foam articlesAdditives: Base resinFilm properties are typical of blown film.. |
|||
Tensile Strength, Yield | 10.3 MPa | 1490 psi | ASTM D638 |
NOVA Chemicals Sclair® 31E LLDPE Extrusion Resin Features: Excellent tensile properties, excellent impact toughness, outstanding gloss and clarity, excellent processability.Applications: Coating and sheathing.Data provided by the manufacturer. |
|||
Tensile Strength, Yield | 10.3 MPa | 1490 psi | 500 mm/min (20 in./min.); ASTM D638, Type IV Specimen |
Eastman 1870A Polyethylene
(discontinued **) Polyethylene 1870A is a low density formulation with excellent flow characteristics for injection molding. It is used for such applications as container closures that require stress-crack resistanc.. |
|||
Tensile Strength, Yield | 10.3 MPa | 1490 psi | ASTM D638 |
NOVA Chemicals Novapol® LF-0222-A LDPE Wire and Cable Resin
(discontinued **) NOVA Chemicals NOVAPOL® LF-0222-A is a medium molecular weight low density polyethylene. Resin consistency and purity are very high which make it suitable as a base resin in Wire and Cable applicat.. |
|||
Tensile Strength, Yield | 10.3 MPa | 1490 psi | ASTM D638 |
LG Chemical LUTENE MB9500 LDPE Injection Molding Grade Description: The physical and structural characteristics of LUTENE MB9500 give it excellent flow properties and good productivity, clarity and surface gloss.Main Application: Powder coating, artific.. |
|||
Tensile Strength, Yield | 10.3 - 22.5 MPa | 1490 - 3260 psi | ISO/R 527E |
Mikro-Technik Reproflon PTFE Reproflon is reclaimed PTFE scraps. The powder can be reused for the usual manufacturing procedures.Information provided by Mikro-Technik GmbH |
|||
Tensile Strength, Yield | 10.3 MPa | 1490 psi | ASTM D412 |
Teknor Apex APEX® 94-A0098C-60 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-General Purpose Uses-General PurposeAppearance-ClearForms-PelletsProcessing Method-Injection Molding.. |
|||
Tensile Strength, Yield | 10.3 MPa | 1490 psi | ASTM D412 |
Teknor Apex TELCAR® 1000-92 Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
Tensile Strength, Yield | 10.3 MPa | 1490 psi | ASTM D412 |
Teknor Apex TELCAR® 1000-92UV Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
Tensile Strength, Yield | 10.3 MPa | 1490 psi | 2.0 in/min; ASTM D638 |
Teknor Apex Telcar® TL-1000-92 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Automotive Spec.. |
|||
Tensile Strength, Yield | 10.3 MPa | 1490 psi | 2.0 in/min; ASTM D638 |
Teknor Apex Telcar® TL-1000-92-UV Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Automotive Spec.. |
|||
Tensile Strength, Yield | 10.3 MPa | 1490 psi | |
Zylog Hipolyene® 2703 MS EX 3 Thermoplastic Polyolefin & PP Compound Information provided by Zylog Plastalloys Pvt. Ltd. |
|||
Tensile Strength, Yield | 10.3 MPa | 1490 psi | |
Zylog Hipolyene® 2703 MS Thermoplastic Polyolefin & PP Compound Information provided by Zylog Plastalloys Pvt. Ltd. |
|||
Tensile Strength, Yield | 10.3 MPa | 1490 psi | Molded property |
Dow DOWLEX™ 2047A Linear Low Density Polyethylene, Cast Film Grade DOWLEX® 2047A Polyethylene resin is a cast film polymer for high performance stretch cling applications. It provides outstanding tear strength, impact strength and toughness. It complies with U.S. .. |
|||
Tensile Strength, Yield | 10.3 MPa | 1490 psi | Molded property |
Dow DOWLEX™ 2247A Linear Low Density Polyethylene, Cast Film Grade DOWLEX® 2247A Polyethylene resin is a cast film polymer for applications requiring outstanding tear strength, impact strength and toughness. This material complies with U.S. FDA Regulation 21 CFR 1.. |
|||
Tensile Strength, Yield | 10.3 MPa | 1490 psi | |
Dow LDPE 779I Low Density Polyethylene DOW LDPE 779I resin is a broad molecular weight distribution homopolymer designed to offer good impact strength and stress crack resistance with excellent rigidity. Typical applications include caps.. |
|||
Tensile Strength, Yield | 10.3 MPa | 1490 psi | 2 in/min (50 mm/min); ASTM D638 |
Bapolene® 1052 Polyethylene, Injection Grade A medium flow general purpose injection molding resin with good gloss, toughness and good chemical resistance. This product meets FDA standards for food contact applications.Applications: Caps and .. |