EMS-Grivory Grivory® TS V0 PA666

Category Polymer , Thermoplastic , Nylon , Nylon 6/66
Manufacturer EMS-Grivory (EMS-CHEMIE)
Trade Name Grivory®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF EMS-Grivory Grivory® TS V0 PA666.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product description: Grilon TS V0 is an unreinforced, normal viscosity, self-extinguishing Polyamid 66 + Polyamide 6 injection molding grade. Grilon TS V0 is halogen free and free of red phosphorous. The unpigmented material has a light inherent color. RoHS: Grilon TS V0 is in compliance with RoHS (2002/95/EC, Restriction of hazardous Substances).WEEE: Parts produced from Grilon TS V0 are not subject to “selective treatment” according the Directive 2002/96/EC on Waste Electrical and Electronic Equipment. Grilon TS V0 has the following important properties: halogen free and free of red phosphorous.UL-94 V0 at 0.4 mm wall thicknessHigh toughnessSuitable for molded Integral hinges Grilon TS V0 is used typically for fuses, strips, cable binders, print terminals and coil former bobbins.Information provided by EMS Grivory
Physical Properties Metric English Comments
Density 1.16 g/cc
0.0419 lb/in³
ISO 1183
Water Absorption 8.0 %
8.0 %
ISO 62
Moisture Absorption 2.50 %
2.50 %
ISO 62
Linear Mold Shrinkage, Flow 0.0070 cm/cm
0.0070 in/in
ISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0080 cm/cm
0.0080 in/in
ISO 294-4, 2577
Mechanical Properties Metric English Comments
Tensile Strength at Break 50.0 MPa
7250 psi
conditioned; ISO 527-1/-2
75.0 MPa
10900 psi
dry; ISO 527-1/-2
Tensile Strength, Yield 50.0 MPa
7250 psi
conditioned; ISO 527-1/-2
85.0 MPa
12300 psi
dry; ISO 527-1/-2
Elongation at Break 10 %
10 %
dry; ISO 527-1/-2
10 %
10 %
dry; ISO 527-1/-2
>= 50 %
>= 50 %
conditioned; ISO 527-1/-2
Elongation at Yield 4.0 %
4.0 %
dry; ISO 527-1/-2
15 %
15 %
conditioned; ISO 527-1/-2
Tensile Modulus 1.60 GPa
232 ksi
conditioned; ISO 527-1/-2
3.60 GPa
522 ksi
dry; ISO 527-1/-2
Charpy Impact Unnotched 7.50 J/cm²
35.7 ft-lb/in²
dry; ISO 179/1eU
10.0 J/cm²
47.6 ft-lb/in²
conditioned; ISO 179/1eU
7.00 J/cm²

@Temperature 30.0 °C
33.3 ft-lb/in²

@Temperature 86.0 °F
dry; ISO 179/1eU
Charpy Impact, Notched 0.400 J/cm²
1.90 ft-lb/in²
dry; ISO 179/1eA
1.50 J/cm²
7.14 ft-lb/in²
conditioned; ISO 179/1eA
0.300 J/cm²

@Temperature 30.0 °C
1.43 ft-lb/in²

@Temperature 86.0 °F
dry; ISO 179/1eU
0.300 J/cm²

@Temperature 30.0 °C
1.43 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 70.0 µm/m-°C
38.9 µin/in-°F
ISO 11359-1/-2
CTE, linear, Transverse to Flow 90.0 µm/m-°C
50.0 µin/in-°F
ISO 11359-1/-2
Melting Point 260 °C
500 °F
10°C/min; ISO 11357-1/-3
Maximum Service Temperature, Air 100 - 120 °C
212 - 248 °F
long term; EMS
200 °C
392 °F
short term; EMS
Deflection Temperature at 0.46 MPa (66 psi) 210 °C
410 °F
ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 70.0 °C
158 °F
ISO 75-1/-2
Flammability, UL94 V-0
V-0
IEC 60695-11-10
V-0

@Thickness 1.50 mm
V-0

@Thickness 0.0591 in
IEC 60695-11-10
Oxygen Index 35 %
35 %
ISO 4589-1/-2
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+11 ohm-cm
1.00e+11 ohm-cm
conditioned; IEC 60093
1.00e+13 ohm-cm
1.00e+13 ohm-cm
dry; IEC 60093
Surface Resistance 1.00e+10 ohm
1.00e+10 ohm
IEC 60093
Dielectric Constant 3.0

@Frequency 100 Hz
3.0

@Frequency 100 Hz
dry; IEC 60250
3.0

@Frequency 1.00e+6 Hz
3.0

@Frequency 1.00e+6 Hz
dry; IEC 60250
4.0

@Frequency 1.00e+6 Hz
4.0

@Frequency 1.00e+6 Hz
conditioned; IEC 60250
8.0

@Frequency 100 Hz
8.0

@Frequency 100 Hz
conditioned; IEC 60250
Dielectric Strength 26.0 kV/mm
660 kV/in
conditioned; IEC 60243-1
28.0 kV/mm
711 kV/in
dry; IEC 60243-1
Comparative Tracking Index 600 V
600 V
conditioned; IEC 60112
Descriptive Properties Value Comments
Automotive Automotive electr. and electronics, lighting
Electricals & Electronics Cables & Tubes
Connectors
Electrical appliances
Electrical equipment
Energy distribution
Lighting
Form Granules
Processing Injection Molding
Special Characteristics Flame retardant