Polymer Property : Volume Resistivity = 1.00e+11 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+11 ohm-cm
1.00e+11 ohm-cm
Plastcom SLOVAMID 6/66 FRc 3 TS PA6/66, flame retardant
FeaturesDetermined for electrotechnical use. Delivered in natural colour. PA 6 + PA 66 alloy for injection moulding with increased flammability resistance, with nonhalogen flame retardant. Excellent..
Volume Resistivity 1.00e+11 ohm-cm
1.00e+11 ohm-cm
Radici Radilon® A ERV1906LK (cond.) Nylon 66
Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov..
Volume Resistivity 1.00e+11 ohm-cm
1.00e+11 ohm-cm
Radici Radilon® A RV300 (cond.) Nylon 66
Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov..
Volume Resistivity 1.00e+11 ohm-cm
1.00e+11 ohm-cm
Radici Radilon® A RV330 (cond.) Nylon 66
Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov..
Volume Resistivity >= 1.00e+11 ohm-cm
>= 1.00e+11 ohm-cm
Radici Radilon® S 32HS (dry) Nylon 6
Radilon® S is a range of polyamide 6 (PA6) products obtained through the polymerization of caprolactam and used for injection, extrusion and blow-molding.Information provided by Radici group.
Volume Resistivity 1.00e+11 ohm-cm
1.00e+11 ohm-cm
Radici Radilon® S 35HR (cond.) Nylon 6
PA6 medium-high viscosity injection molding grade. Easy mould release.Information provided by Radici group.
Volume Resistivity >= 1.00e+11 ohm-cm
>= 1.00e+11 ohm-cm
Radici Radilon® S RV150 (dry) Nylon 6
Radilon® S is a range of polyamide 6 (PA6) products obtained through the polymerization of caprolactam and used for injection, extrusion and blow-molding.Information provided by Radici group.
Volume Resistivity >= 1.00e+11 ohm-cm
>= 1.00e+11 ohm-cm
Radici Radilon® S USZ200 (dry) Nylon 6
Radilon® S is a range of polyamide 6 (PA6) products obtained through the polymerization of caprolactam and used for injection, extrusion and blow-molding.Information provided by Radici group.
Volume Resistivity 1.00e+11 - 1.00e+12 ohm-cm
1.00e+11 - 1.00e+12 ohm-cm
IEC 60093
Raschig Group AMPLA® 7250 melamine-modified polyester
Cellulose reinforced melamine-modified Polyester molding compound. Very good electrical values, excellent heat resistance, excellent surface quality, low post shrinkage. This product meets the allow..
Volume Resistivity 1.00e+11 - 1.00e+12 ohm-cm
1.00e+11 - 1.00e+12 ohm-cm
IEC 60093
Raschig Group MELOPLAS® 3025 MF
Cellulose-reinforced and inorganically filled MF molding compound in white and colored shades. High surface hardness, good UV and heat stability, very good resistance to chemicals - also to foodstu..
Volume Resistivity 1.00e+11 ohm-cm
1.00e+11 ohm-cm
IEC 60093
Hexion Bakelite™ PF 2137 Phenolic Formaldehyde Resin, High Surface Quality, Dishwasher Proof  (discontinued **
Phenolic molding compound, inorganically/organically filled, glass fiber reinforced, increased heat resistance, minimal distortion, dish washer proof.Application areas: Iron heat shields, fittings f..
Volume Resistivity 1.00e+11 ohm-cm
1.00e+11 ohm-cm
IEC 60093
Solvay TECHNYL® B 238 Black 21 N PA66/6, Conditioned
Description: Unreinforced and modified copolyamide 66/6, heat stabilized, with improved impact resistance, for injection molding.Available in: EuropeProduct Applications: TECHNYL B 238 is particular..
Volume Resistivity 1.00e+11 ohm-cm
1.00e+11 ohm-cm
ASTM D257
Techmer ES HiFill® PA4/6 GF5 HS BK002 5% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 5% Filler by WeightAdditive: Heat StabilizerFeatures: Heat StabilizedAppearance: BlackInformation provided b..
Volume Resistivity 1.00e+11 ohm-cm
1.00e+11 ohm-cm
ASTM D257
Techmer ES Luriblend® PA11 GF30 TL20 LE 30% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightAdditive: Heat Stabilizer and PTFE LubricantFeatures: Good Wear Resistance, Low Extractables, Lubricat..
Volume Resistivity 1.00e+11 ohm-cm
1.00e+11 ohm-cm
Practical Use (Water Absorption 2.4%); ASTM-D257
Toyobo GLAMIDE® NB-1700 Nylon/Olefin
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Volume Resistivity 1.00e+11 ohm-cm
1.00e+11 ohm-cm
Cotronics Resbond™ 920 High Temperature Ceramic Adhesive, Thermally Conductive
Volume Resistivity 1.00e+11 ohm-cm
1.00e+11 ohm-cm
conditioned; IEC 60093
EMS-Grivory Grivory® AG-30 H PA66
Product description: Grilon AG-30 H black 9836 is a normal viscosity, specially heat stabilized PA 66 injection molding grade with 30% glass fibres. Grilon AG-30 H black 9836 has the following impor..
Volume Resistivity 1.00e+11 ohm-cm
1.00e+11 ohm-cm
conditioned; IEC 60093
EMS-Grivory Grivory® BG-25 HM PA6-GF25
Product description: Grilon BG-25 HM is a heat stabilized, normal viscosity, and adhesion modified PA6 injection molding grade with 25% glass fibers. Grilon BG-25 HM has the following important prop..
Volume Resistivity 1.00e+11 ohm-cm
1.00e+11 ohm-cm
conditioned; IEC 60093
EMS-Grivory Grivory® TSM-30 PA666-MD30
Product description: Grilon TSM-30 is a heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 30% mineral. Grilon TSM-30 has the following important properties: Excellent surface..
Volume Resistivity <= 1.00e+11 ohm-cm
<= 1.00e+11 ohm-cm
ASTM D257
Diamond Polymers TR 5000 AS/P
Description: Transparent ABS, Antistatic GradeInformation provided by Diamond Polymers, Inc.
Volume Resistivity 1.00e+11 ohm-cm
1.00e+11 ohm-cm
IEC 60093
BASF Ultraform N 2640 Z4 UNC Q600 POM
Ultraform N2640 Z4 UNC Q600 is a high toughness, elastomer-modified injection molding POM grade.
Volume Resistivity 1.00e+11 ohm-cm

@Thickness 0.750 mm
1.00e+11 ohm-cm

@Thickness 0.0295 in
IEC 60093
Ascend Performance Materials Vydyne® ECO315 BK06 Nylon 66/6, Flame Retardant, DAM
Vydyne® ECO315 BK06 is a non-halogenated, unfilled, flame-retardant PA66/6 copolymer with excellent toughness and ductility. It is lubricated for machine feed and easy mold release and has Underwri..
Volume Resistivity 1.00e+11 ohm-cm
1.00e+11 ohm-cm
IEC 60093
BASF Ultramid® B3UG4 Grey 22975 20% Glass Filled PA66 FR (Conditioned)
Description: Halogen-free and phosphorus free flame retardant injection-molding grade with outstanding free-flow properties, good electrical properties and low smoke density; resistant to glow wire..
Volume Resistivity 1.00e+11 ohm-cm
1.00e+11 ohm-cm
IEC 60093
BASF Ultramid® B3ZG3 BK30564 15% Glass Filled PA6 (Dry)
Ultramid B3ZG3 BK30564 is an impact-modified, pigmented black, 15% glass fiber reinforced injection molding PA6 grade.
Volume Resistivity 1.00e+11 ohm-cm

@Thickness 0.750 mm
1.00e+11 ohm-cm

@Thickness 0.0295 in
IEC 60093
Ascend Performance Materials Vydyne® 47H BK0644 Nylon 66, Impact Modified, DAM
Vydyne® 47H BK0644 is a high-performance, medium-impact-modified, heat-stabilized PA66 resin with excellent UV stability and outstanding processing characteristics. This product has an UL746C f1 ra..
Volume Resistivity 1.00e+11 - 1.00e+12 ohm-cm
1.00e+11 - 1.00e+12 ohm-cm
IS 3396-1979
Amity Thermosets ATI 102 Phenolic Molding Organic Filler, Injection Molded
Characteristics:Electrical low loss Good mechanical strengthHigh electrical insulationGood mechanical strengthGlossy surfaceLow water absorptionColor-blackVery soft flow Applications: Electric swit..
Volume Resistivity 1.00e+11 ohm-cm
1.00e+11 ohm-cm
50%RH; IEC 60093
DuPont Performance Polymers Zytel® LM70G35HSLX BK314 Nylon 66  (Unverified Data**)
35% Glass Reinforced Heat Stabilized Laser Markable Polyamide 66 Zytel LM70G35HSLX is a 35% glass fiber reinforced heat stabilized lubricated polyamide 66 for injection molding. It is well suited fo..
Volume Resistivity >= 1.00e+11 ohm-cm
>= 1.00e+11 ohm-cm
Radici Radiflam® S RV300AE (dry) Nylon 6
Radiflam® S is a range of flame retardant polyamides 6 (PA 6) used for injection molding and extrusion for all applications where high fire resistance is required.Information provided by Radici gro..
Volume Resistivity 1.00e+11 ohm-cm
1.00e+11 ohm-cm
Radici Radilon® A ERV3012 (cond.) Nylon 66
Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov..
Volume Resistivity 1.00e+11 ohm-cm
1.00e+11 ohm-cm
ASTM D257
Techmer ES HiFill® PA4/6 GF30 FR HS L 30% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Heat Stabilized, Flame Retardant and Lu..