Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 70.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
38.9 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® 101R PC (Europe-Africa-Middle East) LEXAN 101R is a high viscosity multi purpose grade and contains a release agent to ensure easy processing. LEXAN 101R is available in transparent, translucent and opaque colours. |
|||
CTE, linear, Parallel to Flow | 70.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
38.9 µin/in-°F @Temperature 73.4 - 176 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® DMX3415M PC Copolymer (Europe-Africa-Middle East) Lexan* DMX3415M is a co-polycarbonate resin with improved scratch and abrasion resistance compared to standard polycarbonate. Lexan* DMX3415M is available in transparent colors. |
|||
CTE, linear, Parallel to Flow | 70.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
38.9 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® FXE171R PC (Europe-Africa-Middle East) LEXAN FXE171R is a transparent/translucent high flow grade for special effects colors with a fluorescent appearance. Color package may affect performance. |
|||
CTE, linear, Parallel to Flow | 70.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
38.9 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® FXE174R PC (Europe-Africa-Middle East) LEXAN FXE174R is a high flow visualFx Energy grade, suitable for steam sterilization and compliant with medical and food contact regulations. This material is especially developed for applications t.. |
|||
CTE, linear, Parallel to Flow | 70.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
38.9 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® HPS2R PC (Europe-Africa-Middle East) Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, e-beam and gamma sterilizable.. |
|||
CTE, linear, Parallel to Flow | 70.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
38.9 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® IFX2420Z PC (Asia Pacific) Lexan* IFX2420Z is a medium viscosity, release containing, injection moldable polycarbonate grade suitable for use in industry protective eye-ware applications specifically for welding. This grades .. |
|||
CTE, linear, Parallel to Flow | 70.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
38.9 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® OQ4120R PC (Europe-Africa-Middle East) Optical grade with UV cut-off up to 400 nm, greater optical purity than standard grades. For needs of sunglass and sunvisor markets. MFR of 25. |
|||
CTE, linear, Parallel to Flow | 70.0 µm/m-°C @Temperature 20.0 °C |
38.9 µin/in-°F @Temperature 68.0 °F |
|
Polycasa Acryl® G 77 E Acrylic, Extrusion Grade Extrusion grade for semi-finished products such as profile, sheet and tubes; TV-, HiFi - and video-windows.Data was collected by ISO methods.Quinn Manufacturing Group rebranded its Plastics Division.. |
|||
CTE, linear, Parallel to Flow | 70.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
38.9 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® EX2078X PC (Europe-Africa-Middle East) Lexan* EX2078X polycarbonate resin, MVR (300°C/1.2kg) 3 cm3/10min, high viscosity, branched, extrusion, flame retardant, halogen free per DIN VDE 0472 Part 815, mold release, UV stabilized, translu.. |
|||
CTE, linear, Parallel to Flow | 70.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
38.9 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® HP4 PC (Europe-Africa-Middle East) Medium flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains mold .. |
|||
CTE, linear, Parallel to Flow | 70.0 µm/m-°C @Temperature 20.0 °C |
38.9 µin/in-°F @Temperature 68.0 °F |
|
Covestro Apec® DP 1-9379/5 Polycarbonate
(discontinued **) Key Features:Release agentUnfilledSuitable processing methods:Injection moldingThermoformingInformation provided by Bayer Polymers.As of 1 September 2015, Bayer MaterialScience was separated from Ba.. |
|||
CTE, linear, Parallel to Flow | 70.0 µm/m-°C @Temperature 20.0 °C |
38.9 µin/in-°F @Temperature 68.0 °F |
|
Covestro Apec® DP 1-9379/7 Polycarbonate
(discontinued **) Key Features:Release agentUnfilledU.V. stabilized or stable to weatherSuitable processing methods:Injection moldingThermoformingInformation provided by Bayer Polymers.As of 1 September 2015, Bayer M.. |
|||
CTE, linear, Parallel to Flow | 70.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
38.9 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D 696 |
SABIC Innovative Plastics LNP Lubricomp DP0039 PC LNP* Lubricomp* DP0039 is a Polycarbonate base resin containing PTFE and Silicone lubricants. Characteristics are: Flame Retardant.This data was supplied by SABIC-IP for the Americas region. |
|||
CTE, linear, Parallel to Flow | 70.0 µm/m-°C @Temperature 23.0 - 85.0 °C |
38.9 µin/in-°F @Temperature 73.4 - 185 °F |
ISO 11359 |
Solvay TECHNYL® B 230 PA66/6, DRY Description: Unreinforced and modified copolyamide 66/6, with high flexibility and improved impact resistance, for injection molding.Available in: Asia Pacific and EuropeProduct Applications: TECHN.. |
|||
CTE, linear, Parallel to Flow | 70.0 µm/m-°C @Temperature 23.0 - 85.0 °C |
38.9 µin/in-°F @Temperature 73.4 - 185 °F |
ISO 11359 |
Solvay TECHNYL® C 216 PA6, DRY Description: Unreinforced polyamide PA6, standard nucleation for fast cycling, for injection molding.Available in: Asia PacificProduct Applications: This grade has a high fluidity and good mould rel.. |
|||
CTE, linear, Parallel to Flow | 70.0 - 110 µm/m-°C @Temperature 23.0 - 80.0 °C |
38.9 - 61.1 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-1/-2 |
Styrolution Terluran® HH-112 Q42 Gray 10072 ABS Description: Injection-molding grade with highest heat resistance, high rigidity and medium impact strength.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS |
|||
CTE, linear, Parallel to Flow | 70.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
38.9 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Noryl PX1115 PPE+HIPS (Europe-Africa-Middle East) NORYL PX1115 is an unfilled, flame retardant material with a Vicat B/120 of 140°C according ISO 306. NORYL PX1115 is V1 at 1.2 mm according UL94 and halogen free according VDE/DIN 472 part 815.Th.. |
|||
CTE, linear, Parallel to Flow | 70.0 µm/m-°C | 38.9 µin/in-°F | ISO 11359-1/-2 |
Covestro Apec® 1803 Polycarbonate UV-stabilizedsoftening temperature (VST/B 120)=184 °CPreprocessingMax. Water content |
|||
CTE, linear, Parallel to Flow | 70.0 µm/m-°C @Temperature 20.0 °C |
38.9 µin/in-°F @Temperature 68.0 °F |
|
Covestro Apec® HT KU 1-9363 High-Heat Polycarbonate, UV-Stabilized Transparent and opaque shades possible, UV-stabilized.Applications: Lighting, automotive and household goods, light covers.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience.. |
|||
CTE, linear, Parallel to Flow | 70.0 µm/m-°C @Temperature 20.0 °C |
38.9 µin/in-°F @Temperature 68.0 °F |
|
Covestro Makrolon® 2858 Polycarbonate, Injection Grade Medium flowing BgVV- and FDA injection molding grade, for food contact applications, better resistance to hot water.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was se.. |
|||
CTE, linear, Parallel to Flow | 70.0 µm/m-°C @Temperature 20.0 °C |
38.9 µin/in-°F @Temperature 68.0 °F |
|
Covestro Makrolon® 3103 Polycarbonate Injection molding and extrusion grade with high viscosity, UV stabilized, special grade for sheets.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Baye.. |
|||
CTE, linear, Parallel to Flow | 70.0 µm/m-°C @Temperature 20.0 °C |
38.9 µin/in-°F @Temperature 68.0 °F |
|
Covestro Makrolon® 3108 Polycarbonate, Extrusion Grade Injection molding and extrusion grade with high viscosity, BgVV- and FDA grade for food contact applications.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated.. |
|||
CTE, linear, Parallel to Flow | 70.0 µm/m-°C | 38.9 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® BM-30 FR PA6-MD30 FR Information provided by EMS Grivory |
|||
CTE, linear, Parallel to Flow | 70.0 µm/m-°C | 38.9 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® BT 40 Z PA6 Product description: Grilon BT 40 Z is an unreinforced, normal viscosity, impact modified polyamide blend with amorphous and semi-crystalline components. Grilon BT 40 Z has the following important p.. |
|||
CTE, linear, Parallel to Flow | 70.0 µm/m-°C | 38.9 µin/in-°F | dry; ISO 11359-1/-2 |
DSM EcoPaXX® Q150-D PA410 Low/Medium Viscosity |
|||
CTE, linear, Parallel to Flow | 70.0 µm/m-°C @Temperature 20.0 °C |
38.9 µin/in-°F @Temperature 68.0 °F |
DAM |
Ineos ABS Triax® DP 3155 ABS + Polyamide Blend (Conditioned)
(discontinued **) Key Features:Contains FillerSuitable processing methods:Injection moldingInformation provided by Bayer Polymers.LANXESS was spun-off from Bayer in early 2005. Business renamed Ineos ABS after INEOS.. |
|||
CTE, linear, Parallel to Flow | 70.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
38.9 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® 144 PC (Europe-Africa-Middle East) LEXAN 144 is a medium viscosity multi purpose grade. FDA food contact compliant in limited colors. |
|||
CTE, linear, Parallel to Flow | 70.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
38.9 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® 953A PC (Europe-Africa-Middle East) LEXAN 953A is a high viscosity flame retardant, UV-stabilized grade, especially suitable for electrical applications. |
|||
CTE, linear, Parallel to Flow | 70.0 - 80.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
38.9 - 44.4 µin/in-°F @Temperature 73.4 - 176 °F |
DIN 53752 |
BASF Ultradur® B 4300 K6 30% Glass Bead Filled PBT Description: Is a PBT + ASA, Injection-molding grades containing 30% of glass beads for industrial parts with low warpage.Applications: Precision parts for optical instruments, fuel tank sensor unit.. |
|||
CTE, linear, Parallel to Flow | 70.0 µm/m-°C @Temperature 20.0 °C |
38.9 µin/in-°F @Temperature 68.0 °F |
ISO 11359-1/-2 |
DSM Arnite® T06 202 PBT (European and Asian Grade) Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame .. |