Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 7.50 J/cm² | 35.7 ft-lb/in² | ISO 179 |
PolyOne OnForce™ LFT NN-50LGF/000 HS UV Black Polyamide 66 (Nylon 66) PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. .. |
|||
Charpy Impact Unnotched | 7.50 J/cm² @Temperature -30.0 °C |
35.7 ft-lb/in² @Temperature -22.0 °F |
ISO 179/2C |
SABIC Innovative Plastics Lexan® BFL2015 PC (Europe-Africa-Middle East) Non-brominated, non-chlorinated flame retardant, glass reinforced PC. Opaque colors only |
|||
Charpy Impact Unnotched | 7.50 J/cm² @Temperature -30.0 °C |
35.7 ft-lb/in² @Temperature -22.0 °F |
ISO 179/2C |
SABIC Innovative Plastics Lexan® BFL2015HF PC (Asia Pacific) Non-brominated, non-chlorinated flame retardant, glass reinforced PC. Opaque colors only. UL94 V0 1.5 mm for BLACK; V1 1.5 mm for OTHER Color. |
|||
Charpy Impact Unnotched | 7.50 J/cm² @Temperature 23.0 °C |
35.7 ft-lb/in² @Temperature 73.4 °F |
|
Radici Radilon® S RV330 (cond.) Nylon 6 Radilon® S is a range of polyamide 6 (PA6) products obtained through the polymerization of caprolactam and used for injection, extrusion and blow-molding.Information provided by Radici group. |
|||
Charpy Impact Unnotched | 7.50 J/cm² @Temperature 23.0 °C |
35.7 ft-lb/in² @Temperature 73.4 °F |
DAM; ISO 179/1eU |
DuPont Performance Polymers Zytel® HTN 54G35HSLR NC010 Polyphthalamide (PPA)
(Unverified Data**) Zytel® HTN54G35HSLR NC010 is a 35% glass reinforced, toughened, heat stabilized, lubricated high performance polyamide resin. It is also a PPA resin.Information provided by DuPont Performance Polym.. |
|||
Charpy Impact Unnotched | 7.50 J/cm² | 35.7 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics Lexan® HFD4211 PC (Europe-Africa-Middle East) Lexan* HFD4211 is a 10% glass filled, injection moldable grade designed for high flow and superior surface appearance. Internal mold release. |
|||
Charpy Impact Unnotched | 7.50 J/cm² | 35.7 ft-lb/in² | edgewise; ISO 179 1eU |
Lehmann & Voss LUVOCOM® 20-0778 Polyphthalamide, with glass fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Low influence from moisture an.. |
|||
Charpy Impact Unnotched | 7.50 J/cm² | 35.7 ft-lb/in² | flatwise; ISO 179 1fU |
Lehmann & Voss LUVOCOM® 50/TF/15/BK7284 Polycarbonate, with PTFE, easy flowing Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Improved friction and wear behaviour. Emergency running proper.. |
|||
Charpy Impact Unnotched | 7.50 J/cm² | 35.7 ft-lb/in² | |
LATI Latamid 6 H2 G/35 PA 6, 35% Glass Fiber Reinforced, Heat Stabilized Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibersAvailability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplast.. |
|||
Charpy Impact Unnotched | 7.50 J/cm² | 35.7 ft-lb/in² | flatwise; ISO 179 1fU |
Lehmann & Voss LUVOCOM® 1/GF/40/TF/13 Polyamide 66, with glass fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec.. |
|||
Charpy Impact Unnotched | 7.50 J/cm² | 35.7 ft-lb/in² | ISO 179/1eU |
Solvay TECHNYL® A 218HP V35 PA66, 35% glass fiber, DRY Description: TECHNYL® A 218HP V35 is a polyamide 6.6, reinforced with 35% of glass fiber, heat stabilized, for injection molding. This product is available in black color.Benefits: The product of.. |
|||
Charpy Impact Unnotched | 7.50 J/cm² | 35.7 ft-lb/in² | ISO 179 |
Polyram Polytron P50N07 Polypropylene, 50% Long Glass Fiber, UV Stabilized A chemically coupled 50% long glass fiber reinforced natural polypropylene, heat stabilized, UV stabilized for injection molding applications.Information provided by Polyram. |
|||
Charpy Impact Unnotched | 7.50 J/cm² @Temperature 30.0 °C |
35.7 ft-lb/in² @Temperature 86.0 °F |
conditioned; ISO 179/1eU |
EMS-Grivory Grivory® BG-40 FC PA6-GF40 Product description: Grilon BG-40 FC is a heat stabilized PA6 injection molding grade with 40% glass fibers. Grilon BG-40 FC has the following important properties: High stiffnessExcellent surface f.. |
|||
Charpy Impact Unnotched | 7.50 J/cm² | 35.7 ft-lb/in² | dry; ISO 179/1eU |
EMS-Grivory Grivory® BS EC PA6 Product description: Grilon BS 23 is an unreinforced, low viscosity and fine crystalline PA 6 injection molding grade. Grilon BS 23 has the following important properties: Good flow behaviorEasy pro.. |
|||
Charpy Impact Unnotched | 7.50 J/cm² @Temperature 23.0 °C |
35.7 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
CP-Polymer-Technik Wellamid® 6000 MRGV 20/10 HWCP 20% Mineral and 10% Glass Fiber Nylon 6, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Charpy Impact Unnotched | 7.50 J/cm² @Temperature -30.0 °C |
35.7 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
DSM Stanyl® TW200F8 (COND) Nylon 46 40% Glass Reinforced, Heat Stabilized (North America) Information provided by DSM Engineering Plastics. |
|||
Charpy Impact Unnotched | 7.50 J/cm² | 35.7 ft-lb/in² | dry; ISO 179/1eU |
EMS-Grivory Grivory® GVX-65 H nat PA*-GF65 Product description: Grivory GVX-65H natural is a 65% glass-fiber reinforced engineering thermoplastic material based on a combination of semi-crystalline polyamide with partially aromatic copolyami.. |
|||
Charpy Impact Unnotched | 7.50 J/cm² | 35.7 ft-lb/in² | dry; ISO 179/1eU |
EMS-Grivory Grivory® TSG-30 PA666-GF30 Product description: Grilon TSG-30 is a heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 30% glass fibers. Grilon TSG-30 has the following important properties: Excellent fl.. |
|||
Charpy Impact Unnotched | 7.50 J/cm² @Temperature 30.0 °C |
35.7 ft-lb/in² @Temperature 86.0 °F |
conditioned; ISO 179/1eU |
EMS-Grivory Grivory® TSGL-50-4 nat PA666-GF50 Product description: Grilon TSGL-50/4 natural is based on a heat stabilized semi-crystalline Polyamide PA66+PA6 and 50% long glass fibers. Grilon TSGL-50/4 natural is characterized by the following .. |
|||
Charpy Impact Unnotched | 7.50 J/cm² | 35.7 ft-lb/in² | dry; ISO 179/1eU |
EMS-Grivory Grivory® TSGZ-15 PA666-GF15 Product description: Grilon TSGZ-15 is a heat stabilized, normal viscosity, and impact modified PA66 + PA6 injection molding grade with 15% glass fibers. Grilon TSGZ-15 has the following important p.. |
|||
Charpy Impact Unnotched | 7.50 J/cm² @Temperature 30.0 °C |
35.7 ft-lb/in² @Temperature 86.0 °F |
conditioned; ISO 179/1eU |
EMS-Grivory Grivory® XE 4108 nat PA612-GF50 Product description: Grilamid XE 4108 natural is a 50% glass fiber reinforced, heat stabilized polyamide 612 injection molding grade. The main features of Grilamid XE 4108 are: low water absorptiong.. |
|||
Charpy Impact Unnotched | 7.50 J/cm² | 35.7 ft-lb/in² | conditioned; ISO 179/1eU |
EMS-Grivory Grivory® XE 4116 nat PA1010-GF55 Product description: Grilamid XE 4116 natural is a 55% glass fiber reinforced Polyamide 1010 injection molding grade. This grade is especially suitable for the manufacturing of thin-walled, painted .. |
|||
Charpy Impact Unnotched | 7.50 J/cm² | 35.7 ft-lb/in² | dry; ISO 179/1eU |
EMS-Grivory Grivory® XE 5052 (BGZ-15 FC) PA6-GF15 Product description: Grilon XE 5052 is a impact modified, heat stabilized PA 6 injection molding grade with 15% glass fiber: High impact resistanceGood surface qualityShort cycle timeGood flowabilit.. |
|||
Charpy Impact Unnotched | 7.50 J/cm² @Temperature -30.0 °C |
35.7 ft-lb/in² @Temperature -22.0 °F |
50%RH; ISO 179/1eU |
DuPont Performance Polymers Zytel® 70G33L NC010 Nylon 66
(Unverified Data**) 33% Glass Reinforced Polyamide 66Zytel 70G33L NC010 is a 33% glass fiber reinforced polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Charpy Impact Unnotched | 7.50 J/cm² @Temperature 30.0 °C |
35.7 ft-lb/in² @Temperature 86.0 °F |
dry; ISO 179/1eU |
EMS-Grivory Grivory® HT1V-6 FWA black 9225 PA6T/6I-GF60 Product description: Grivory HT1V-6 FWA black 9225 is a 60 wt.- % glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: .. |
|||
Charpy Impact Unnotched | 7.50 J/cm² @Temperature 23.0 °C |
35.7 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
BASF Ultramid® KR 4365 G5 BK 00100 35% Glass Filled PA6/6T FR (Dry) Description: Partially aromatic polyamide; flame retardant based on red phosphorus; low water absorption, high melting point (295°C); low tendency to form deposits on electrical contacts, very resi.. |
|||
Charpy Impact Unnotched | 7.50 J/cm² | 35.7 ft-lb/in² | cond.; ISO 179 1eU |
Azoty Tarnow™ Tarnamid® T-27 GF20 GB10 Polyamide 6 - Glass Beads Reinforced 20% Glass fiber and 10% glass beads reinforced, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following .. |
|||
Charpy Impact Unnotched | 7.50 J/cm² | 35.7 ft-lb/in² | |
Polimeri Europa EDISTIR PD RK6223N High Impact Polystyrene (HIPS)
(discontinued **) Symbol according to ISO 1043-1: S/B Designation: Thermoplastic ISO 2897-SB,M,083-12-07-23 Halogen and Antimony free, medium impact polystyrene. This grade complies at 2 mm with IEC 65-20-2 and BSI.. |
|||
Charpy Impact Unnotched | 7.50 J/cm² | 35.7 ft-lb/in² | Conditioned; ISO 179/IeU |
Addiplast Addinyl B2 ZV40 Nylon 6, 40% Glass Filled Glass fiber reinforced, increased thermal aging stabilityInformation provided by Addiplast. |
|||
Charpy Impact Unnotched | 7.50 J/cm² @Temperature 30.0 °C |
35.7 ft-lb/in² @Temperature 86.0 °F |
conditioned; ISO 179/1eU |
EMS-Grivory Grivory® BGZ-15/2 PA6-GF15 Product description: Grilon BGZ-15/2 is a heat stabilized and impact modified PA6 injection molding grade with 15% glass fibers. Grilon BGZ-15/2 has the following important properties: Good impact s.. |