Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.16 g/cc | 0.0419 lb/in³ | ASTM D792 |
Plaskolite Optix® CA-927 Impact Modified Acrylic Resin Injection Molding Grade Pellets. Better impact strength than CA-924. Excellent surface gloss, optical clarity, and practical toughness. |
|||
Density | 1.16 g/cc | 0.0419 lb/in³ | |
Plastcom SLOVAMID 6/66 FRc 3 TS PA6/66, flame retardant FeaturesDetermined for electrotechnical use. Delivered in natural colour. PA 6 + PA 66 alloy for injection moulding with increased flammability resistance, with nonhalogen flame retardant. Excellent.. |
|||
Density | 1.16 g/cc | 0.0419 lb/in³ | ISO 1183 |
SABIC Innovative Plastics GELOY HRA170D ASA+PC (Europe-Africa-Middle East) GELOY HRA170D resin is a PC-ASA blend with permanent antistatic behavior. It is typically used in applications that require antidust properties and high impact retention. Geloy HRA170D resin is typi.. |
|||
Density | 1.16 g/cc | 0.0419 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP COLORCOMP AX03654 ABS (Asia Pacific) LNP COLORCOMP* AX03654 is a compound based on Acrylonitrile Butadiene Styrene resin containing Flame Retardant, Unfilled Custom Color. Added features of this material include: Flame Retardant. |
|||
Density | 1.16 g/cc | 0.0419 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP FARADEX AS003 ABS LNP* Faradex* AS003 is a compound based on Acrylonitrile Butadiene Styrene resin containing 15% Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding... |
|||
Density | 1.16 g/cc | 0.0419 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP LUBRICOMP AL004 ABS (Asia Pacific) LNP* Lubricomp* AL004 is a compound based on Acrylonitrile Butadiene Styrene resin containing Lubricants. Added features of this material include: Internally Lubricated. |
|||
Density | 1.16 g/cc | 0.0419 lb/in³ | |
Polycasa Acryl® KR 2008/1 Acrylic, Impact Grade Impact grade for extruded tubes and profiles; e.g. strip light diffusers; good scratch and abrasion resistance.Data was collected by ISO methods.Quinn Manufacturing Group rebranded its Plastics Divi.. |
|||
Density | 1.16 g/cc | 0.0419 lb/in³ | ISO 1183 |
Polimeri Europa Edistir RK Polystyrene
(discontinued **) UL94 V-0, flame retarded, high impact polystyrene. This grade is suitable for injection moulding. It combines high mechanical strength, heat resistance and good processability.
Designation: Thermopl.. |
|||
Density | 1.16 g/cc | 0.0420 lb/in³ | Yield Density |
Honeywell Capran® Emblem™ 2500M M-Coated Bi-Axially Oriented Nylon Film Description: Capran® Emblem™ 2500M is a bi-axially oriented nylon film. It is a versatile and robust film that satisfies many packaging needs, and has superior resistance to oils, fats, hyd.. |
|||
Density | 1.16 g/cc | 0.0420 lb/in³ | Yield Density |
Honeywell Capran® Oxyshield™ OEB (0.60 mil) Monoaxially Oriented, Co-Extruded Nylon 6/EVOH/Nylon 6 Clear Film Description: Oxyshield™ Oriented Extra Barrier is a 0.60 mil (15 micron) monoaxially oriented, co-extruded nylon 6/EVOH/nylon 6 clear film having excellent gas barrier through a broad range of .. |
|||
Density | 1.16 g/cc | 0.0419 lb/in³ | ISO 1183 |
Lucite International Diakon® ST35G8 Toughened Acrylic Polymer The Diakon® impact PMMA series offer the best combination of impact, chemical and heat resistance and provide rigidity and surface hardness. The grades in the Diakon® series can be processed b.. |
|||
Density | 1.16 g/cc | 0.0419 lb/in³ | ISO 1183 |
Lucite International Perspexâ„¢ XT IM60 Acrylic Impact Modified Extruded Sheet PERSPEX extruded sheet has a lower molecular weight making it easy to vacuum form and the extrusion process gives excellent thickness tolerance and is economical for long production runs.Information.. |
|||
Density | 1.16 - 1.20 g/cc | 0.0419 - 0.0434 lb/in³ | |
Taiwan Sheen Soon Sheenthane® A8510L TPU for Ink Thermoplastic polyurethane elastomer for inkAbrasion resistant, flexible, soft, excellent adhesion, high solubility in MEK and Anone. Used for transfer coating, screen printing, and spray applicati.. |
|||
Density | 1.16 g/cc | 0.0419 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP Lubricomp QP003 PA 6/10 (Asia Pacific) LNP* Lubricomp* QP003 is a compound based on Nylon 6/10 resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the As.. |
|||
Density | 1.16 g/cc | 0.0419 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP THERMOCOMP AF003 ABS LNP* THERMOCOMP* AF003 is a compound based on ABS resin containing 15% Glass Fiber. |
|||
Density | 1.16 g/cc | 0.0419 lb/in³ | ASTM D792 |
Techmer ES Luriblend® PA6 E ML2 MB Availability: North AmericaForms: PelletsAdditive: Molybdenum Disulfide LubricantFeatures: LubricatedAppearance: Natural ColorInformation provided by TP Composites, Inc. |
|||
Density | 1.16 g/cc | 0.0420 lb/in³ | |
Sika Industry SikaFlex 252 One Part Polyurethane Adhesive Sika 252 SikaFlex One Part Polyurethane AdhesiveA high viscous, high strength adhesive, this product can replace rivets, screws, welds, and other mechanical fasteners. Seals and bonds in one step. 4.. |
|||
Density | 1.16 g/cc | 0.0419 lb/in³ | ISO 1183/A |
Solvay TECHNYL® B 50 H1 PA66/6, Conditioned Description: TECHNYL® B 50H1 is an unreinforced melamine cyanurate flame retarded copolyamide 66/6. This product has been heat stabilized and is suitable for injection molding. This product is av.. |
|||
Density | 1.16 g/cc | 0.0419 lb/in³ | ASTM D792 |
Borealis PC0798 Polyethylene Insulation Compound, Crosslinkable PC0798 is a flame retardant crosslinking polyethylene compound for low voltage insulation. PC0798 is a halogenated, colorable, chemically crosslinkable copolymer compound which contains flame retar.. |
|||
Density | 1.16 g/cc | 0.0419 lb/in³ | ISO 1183 |
Covestro Desmopan® 955 U Polyurethane PreprocessingMax. Water content |
|||
Density | 1.16 g/cc | 0.0419 lb/in³ | ISO 1183 |
DSM Arnitel® PL381 Polyether Ester Elastomer (European and Asian Grade) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Density | 1.16 g/cc | 0.0419 lb/in³ | ISO 1183 |
DSM Arnitel® PM381 Polyether Ester Elastomer (European Grade) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Density | 1.16 g/cc | 0.0419 lb/in³ | ISO 1183 |
DSM Arnitel® VT3104 TPC-ET Extrusion Grade |
|||
Density | 1.16 g/cc @Temperature 25.0 °C |
0.0419 lb/in³ @Temperature 77.0 °F |
|
DSM Somos® ProtoGen™ O-XT 18120 Epoxy Resin for Stereolithography, UV Postcure at HOC -2 DescriptionDSM Somos® ProtoGen O-XT 18120 is a liquid photopolymer that produces accurate parts ideal for general purpose applications. ProtoGen resins are the first SL resins to demonstrate diffe.. |
|||
Density | 1.16 g/cc | 0.0419 lb/in³ | ISO 1183 |
Eurostar Staramide AG3X3 PA66, Glass Fiber Reinforced, Impact Modified, Injection Molding Staramide AG3X3 is an Impact Modified, Glass Fiber Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Density | 1.16 g/cc | 0.0419 lb/in³ | ISO 1183 |
Eurostar Starflam PX06091 PA6, Flame Retardant, Injection Molded Starflam PX06091 is an Unfilled, Halogen Free and Red Phosphorous Free, Flame Retardant, Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Density | 1.16 g/cc | 0.0419 lb/in³ | ISO 1183 |
Eurostar Star L PA6 D36 PA6, Injection Molded Star L PA6 D36 is a MOS2 Lubricated Unreinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Density | 1.16 g/cc | 0.0419 lb/in³ | |
A. Schulman ComAlloy Hiloy® 123 Polypropylene, Glass Reinforced, Chemically Coupled, UL Data provided by the manufacturer, ComAlloy International Company.30% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Density | 1.16 g/cc | 0.0419 lb/in³ | ASTM D792 |
Cast Nylons Nycast® XHA Heat Stabilized Nylon 6 Heat stabilized Cast Nylon 6 adds up to 20 degrees F higher continuous operation temperature for those applications that require additional temperature resistance beyond the standard resistance. Dat.. |
|||
Density | 1.16 g/cc | 0.0419 lb/in³ | ASTM D-792 |
Bhansali Engineering Abstron AN480V2 Flame Retardant ABS Grade Information provided by Bhansali |