Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 3.60 GPa | 522 ksi | |
Plastcom SLOVALEN PH 72 T 40 PP, 40% mineral filling FeaturesModified homopolymer PP for injection moulding with the content of 40% microground, floated, thermo stable, chemically modified talc. General application in all industry branches - covers of.. |
|||
Tensile Modulus | 3.60 GPa | 522 ksi | |
Plastcom SLOVALEN PH 92 T 40 PP, 40% mineral filling FeaturesModified homopolymer PP for injection moulding with the content of 40% microground, floated, chemically modified talc. Stable towards oxidants. General application in all industry branches -.. |
|||
Tensile Modulus | 3.60 GPa | 522 ksi | 50 mm/min; ASTM D638 |
Ovation Polymers RIGITRON 10020 GF Polycarbonate, 20% Glass Reinforced PC - Glass reinforced (20 %), high tensile strength, stiffness and HDT. *All properties are measured after 48 hours of conditioning at 23°C and 50% relative humidity. All samples are prepared accor.. |
|||
Tensile Modulus | 3.60 GPa | 522 ksi | ISO 527, ASTM D638 |
Nilit Nilamid A H2 FR HF2 Unfilled, Flame Retardant PA66/6 Co-Polymer Description: Nilamid A H2 FR HF2 is an unfilled, flame retardant NYLON 66/6 co-polymer that does not contain halogen or red phosphorous. This product combines excellent flow characteristics and extr.. |
|||
Tensile Modulus | 3.60 GPa | 522 ksi | ISO 527-1/-2 |
Quadrant EPP Ertalon® 6 PLA PA 6, cast (ISO Data) Unmodified cast nylon 6 grade exhibiting characteristics which come very close to those of Ertalon 66 SA. It combines high strength, stiffness and hardness with good creep and wear resistance, heat .. |
|||
Tensile Modulus | 3.60 GPa | 522 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® 505RU PC Lexan* 505RU is a glass reinforced,flame retardant(FR)grade with non brominated and non chlorinated FR systems and UV stablization packages. This product is intended for applications to meet WEEE/Ro.. |
|||
Tensile Modulus | 3.60 GPa | 522 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® ML7667 PC Copolymer Lexan* ML7667 specialty polycarbonate (PC) resin is a 9% GF reinforced, UV stabilized, flame retarded injection molding grade. This medium flow specialty PC resin combines UL94 V0 @ 1.5mm, 5VB @ 3.. |
|||
Tensile Modulus | 3.60 GPa | 522 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® ML7667 PC Copolymer (Asia Pacific) Lexan* ML7667 specialty polycarbonate (PC) resin is a 9% GF reinforced, UV stabilized, flame retarded injection molding grade. This medium flow specialty PC resin combines UL94 V0 @ 1.5mm, 5VB @ 3.. |
|||
Tensile Modulus | 3.60 GPa | 522 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Faradex NS0039XP PC+ABS (Europe-Africa-Middle East) LNP* FARADEX* NS0039XP is a compound based on PC/ABS resin containing Stainless Steel Fiber, Flame Retardant. Added features include: Electrically Conductive, EMI/RFI Shielding, Flame retardant.Thi.. |
|||
Tensile Modulus | 3.60 GPa | 522 ksi | ASTM D638 |
Solvay Specialty Polymers KetaSpire® KT-820P Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-820P is a low flow grade of unreinforced polyetheretherketone (PEEK) supplied in a natural-color coarse powder form. KetaSpire PEEK is produced to the highest industry standards and is .. |
|||
Tensile Modulus | 3.60 GPa | 522 ksi | 1.0 mm/min; ASTM D638 |
Solvay Specialty Polymers KetaSpire® KT-851 Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-851 resin is a depth-filtered grade of polyetheretherketone (PEEK) specially designed for use in extruded wire insulation coating. KT-851 offers the needed balance of properties and pro.. |
|||
Tensile Modulus | 3.60 GPa | 522 ksi | DIN 53457 |
Isoflon PEEK Polyetheretherketone Materials with strong mechanical and electrical performances under high temperatures.Information provided by Isoflon. |
|||
Tensile Modulus | 3.60 GPa | 522 ksi | conditioned, 1 mm/min; ISO 527-1,-2 |
Lanxess Durethan® AKV 15 FN 00 000000 Nylon 66, 12% Glass Fiber PA 66, 12% glass fiber, injection molding, halogen free flame retardantInformation provided by LANXESS. |
|||
Tensile Modulus | 3.60 GPa | 522 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL V02570 PPE+HIPS Noryl* V02570 is a 25% milled fiber reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
Tensile Modulus | 3.60 GPa | 522 ksi | ISO 527 Type 1A |
Solvay TECHNYL® B 50 H1 PA66/6, DRY Description: TECHNYL® B 50H1 is an unreinforced melamine cyanurate flame retarded copolyamide 66/6. This product has been heat stabilized and is suitable for injection molding. This product is av.. |
|||
Tensile Modulus | 3.60 GPa | 522 ksi | 50 mm/min; ASTM D638 |
Solvay Specialty Polymers KetaSpire® KT-820 SL10 Polyetheretherketone (PEEK) KetaSpire® KT-820 SL10 is a polyetheretherketone (PEEK) based compound designed to offer enhanced lubricity and reduced friction compared to standard PEEK. Unlike other grades formulated for wear.. |
|||
Tensile Modulus | 3.60 GPa | 522 ksi | ASTM D638 |
Solvay Specialty Polymers KetaSpire® KT-820P Polyetheretherketone (PEEK) KetaSpire® KT-820P is a low flow grade of unreinforced polyetheretherketone (PEEK) supplied in a natural-color coarse powder form. KetaSpire® PEEK is produced to the highest industry standards.. |
|||
Tensile Modulus | 3.60 GPa | 522 ksi | 1.0 mm/min; ASTM D638 |
Solvay Specialty Polymers KetaSpire® KT-851 NL Polyetheretherketone (PEEK) KetaSpire® KT-851 NL resin is a depth-filtered grade of polyetheretherketone (PEEK) supplied in non-lubricated, natural-color pellet form and is specially designed for use in extruded wire insula.. |
|||
Tensile Modulus | 3.60 GPa | 522 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP DX05477 PC LNP THERMOCOMP* DX05477 is a compound based on Polycarbonate resin containing Glass Fiber. Added features of this material include: Easy Molding, Mold Release, Flame Retardant. |
|||
Tensile Modulus | 3.60 GPa | 522 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL NH7111E PPE+HIPS (Asia Pacific) Noryl* EXNL0280 is a glass fiber reinforced, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and low warpage, this resin also uses non-halogenated FR a.. |
|||
Tensile Modulus | 3.60 GPa | 522 ksi | ISO 527 |
Polyram RamOfin PPH343T8 Polypropylene, 40% Mineral Filled 40% Mineral filled polypropylene for injection molding applications.Information provided by Polyram. |
|||
Tensile Modulus | 3.60 GPa | 522 ksi | ISO 527-1/-2 |
DSM Akulon® S223-DH Nylon 66 (European and Asian Grade) (Dry) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Tensile Modulus | 3.60 GPa | 522 ksi | ISO 527 |
CP-Polymer-Technik Wellamid® 6000 GVS 10/20 HWCP 10% Glass Fiber and 20% Glass Sphere Nylon 6, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Tensile Modulus | 3.60 GPa | 522 ksi | 1 mm/min; ISO 527 |
Eurostar Staramide PK005EI2 PA6, Mineral Fiber Filled, Impact Modified Injection Molded Staramide PK005EI2 is an Impact Modified Mineral Filled Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Tensile Modulus | 3.60 GPa | 522 ksi | ASTM D638 |
Aclo Accutech Polypropylene Homopolymer HP0336M40CL Mica Reinforced Coupled |
|||
Tensile Modulus | 3.60 GPa | 522 ksi | ASTM D638 |
Aclo Accutech Polypropylene Homopolymer HP0339G20M10CL Glass/Mineral Reinforced Coupled |
|||
Tensile Modulus | 3.60 GPa | 522 ksi | ASTM D638 |
Azdel SuperLite® SL551800-100 PP Resin Matrix / 55% Glass Fiber (4 mm Molded Thickness) AZDEL SuperLite® SL551800-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic.. |
|||
Tensile Modulus | 3.60 GPa | 522 ksi | ASTM D638 |
Cast Nylons Nycast® 6PA-Blue Nylon 6 NYCAST® 6 PA-Blue along with NYCAST® 6 PA-Natural have replaced bronze, brass, steel, and aluminum in various mechanical applications.Data provided by the manufacturer, Cast Nylons Limited.The dat.. |
|||
Tensile Modulus | 3.60 GPa | 522 ksi | ISO 527-1/-2 |
DSM Stanyl® TE350 Nylon 46 (European and Asian Grade) (Dry)
(discontinued **) Stanyl is a high performance polyamide providing unmatched performance and value across an amazingly broad range of automotive and electronic applications. Stanyl offers:Highest mechanical propertie.. |
|||
Tensile Modulus | 3.60 GPa | 522 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® TS V0 PA666 Product description: Grilon TS V0 is an unreinforced, normal viscosity, self-extinguishing Polyamid 66 + Polyamide 6 injection molding grade. Grilon TS V0 is halogen free and free of red phosphorous.. |