Polymer Property : Volume Resistivity = 1.00e+11 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+11 ohm-cm
1.00e+11 ohm-cm
Plastcom SLOVAMID 6/66 FRc 3 TS PA6/66, flame retardant
FeaturesDetermined for electrotechnical use. Delivered in natural colour. PA 6 + PA 66 alloy for injection moulding with increased flammability resistance, with nonhalogen flame retardant. Excellent..
Volume Resistivity 1.00e+11 ohm-cm
1.00e+11 ohm-cm
Cond. A; IPC 2.5.17.1
Rogers Corporation RO3006 Ceramic-Filled PTFE Composite, High Frequency Circuit Material
Features and Benefits:
Volume Resistivity >= 1.00e+11 ohm-cm
>= 1.00e+11 ohm-cm
Radici Radilon® S RV150 (dry) Nylon 6
Radilon® S is a range of polyamide 6 (PA6) products obtained through the polymerization of caprolactam and used for injection, extrusion and blow-molding.Information provided by Radici group.
Volume Resistivity 1.00e+11 ohm-cm
1.00e+11 ohm-cm
Radici Radilon® S RV250 (cond.) Nylon 6
Radilon® S is a range of polyamide 6 (PA6) products obtained through the polymerization of caprolactam and used for injection, extrusion and blow-molding.Information provided by Radici group.
Volume Resistivity >= 1.00e+11 ohm-cm
>= 1.00e+11 ohm-cm
Radici Radilon® S USZ200 (dry) Nylon 6
Radilon® S is a range of polyamide 6 (PA6) products obtained through the polymerization of caprolactam and used for injection, extrusion and blow-molding.Information provided by Radici group.
Volume Resistivity 1.00e+11 ohm-cm
1.00e+11 ohm-cm
Plastcom SLOVAMID 6 FRC 2 218/1M PA6, flame retardant
Packaging, transport, stockingThe product is packed in hermetically closed thick-walled 25 kg PE bags, on a 1.000 kg palette coated in a stretch foil, in big bags with a thick PE foil fixed on a 1.0..
Volume Resistivity 1.00e+11 ohm-cm
1.00e+11 ohm-cm
Radici Radilon® S RCP3010LK (cond.) Nylon 6
PA6 30% Glass Fiber and mineral filler reinforced injection molding grade. Good stiffness and good dimensional stability. Heat stabilized, good surface finish.Information provided by Radici group.
Volume Resistivity >= 1.00e+11 ohm-cm
>= 1.00e+11 ohm-cm
Radici Radilon® S RV300R (dry) Nylon 6
Radilon® S is a range of polyamide 6 (PA6) products obtained through the polymerization of caprolactam and used for injection, extrusion and blow-molding.Information provided by Radici group.
Volume Resistivity 1.00e+11 ohm-cm
1.00e+11 ohm-cm
IEC 60093
Hexion Bakelite™ PF 2736 Phenolic Formaldehyde Resin, Improved Electrical Properties, Low Shrinkage, UL Listed &nbs
Phenolic molding compound, inorganically/organically filled, increased tracking resistance, UL listed molding compound 0.46 mm/V-0 (BK, Suffix "H"), 0.81 mm/V-0 (NC, GN, BK), 1.5 mm/V-0 (ALL).Applic..
Volume Resistivity 1.00e+11 ohm-cm
1.00e+11 ohm-cm
IEC 60093
Hexion Bakelite™ X22 Phenolic Formaldehyde Resin, UL Listed  (discontinued **)
Phenolic molding compound, mainly organically filled, UL listed molding compound 3.0 mm/V-0 (BN, BK).Application areas: Pot handles, operating controls, electrical isolators, housing parts.Informati..
Volume Resistivity 1.00e+11 ohm-cm
1.00e+11 ohm-cm
IEC 60093
Hexion Bakelite™ X30 Phenolic Formaldehyde Resin  (discontinued **)
Phenolic molding compound, reinforced with cotton and sisal fibers, increased notched impact strength.Application areas: Covers for electrical and electromagnetic devices.Information provided by Bak..
Volume Resistivity 1.00e+11 ohm-cm
1.00e+11 ohm-cm
IEC 60093
Celanese FORTRON 309 PPS  (Unverified Data**)
0309 exhibits a good balance of flow and melt strength for extrusion processes. The material demonstrates excellent heat and chemical resistance. The intended use of this product is for extruding mo..
Volume Resistivity 1.00e+11 ohm-cm
1.00e+11 ohm-cm
Conditioned; IEC 60093
Lanxess Durethan® BKV 140 000000 Copolyamide, 40% Glass Fiber
CoPA, injection molding grade, 40% glass fibers, elastomer-modified, electroplateable, higher notched impact strength and also higher energy absorption under biaxial impact load than BKV 40, even in..
Volume Resistivity 1.00e+11 ohm-cm
1.00e+11 ohm-cm
cond.; IEC 60093
Lanxess Durethan® BKV 40 H2.0 901510 Nylon 6, Glass Fiber Reinforced
PA 6, 40% glass fibers, injection molding, heat-aging stabilizedInformation provided by LANXESS.
Volume Resistivity 1.00e+11 ohm-cm
1.00e+11 ohm-cm
Conditioned; IEC 60093
Lanxess Durethan® BM 240 H2.0 901510 Nylon 6, 40% Mineral
PA 6, injection molding grade, 40% mineral, isotopic properties, good heat-ageing resistance
Volume Resistivity 1.00e+11 ohm-cm
1.00e+11 ohm-cm
ASTM D257
Techmer ES Elastoblend® PA6/6 GF30 IM2 30% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: Heat Stabilizer, Lubricant and Impact ModifierFeatures: Heat Stabilized, Lubri..
Volume Resistivity 1.00e+11 ohm-cm
1.00e+11 ohm-cm
ASTM D257
Techmer ES Luriblend® PA12 TS18
Availability: North AmericaForms: PelletsAdditive: Silicone Lubricant(2%) and PTFE Lubricant(18%)Features: LubricatedInformation provided by TP Composites, Inc.
Volume Resistivity 1.00e+11 ohm-cm
1.00e+11 ohm-cm
IEC 60093
Styrolution Terblend® N NM-21 XP ABS+PA (Conditioned)
Information provided by STYROLUTION, which is a joint venture between BASF and INEOS
Volume Resistivity 1.00e+11 ohm-cm
1.00e+11 ohm-cm
ASTM D257
Tipco Tipcolite® THR 211 Phenolic Compound, Asbestos Wood Flour & Minerals, Soft Flow & High Electrical Properties
Soft Flow Phenolic Compound, Reinforced with Asbestos Wood Flour & MineralsApplications: Switchgear, HRC FusesProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industrie..
Volume Resistivity 1.00e+11 ohm-cm
1.00e+11 ohm-cm
Tra-Con Tra-Bond F118CLR Fiber Optic Epoxy Adhesive
TRA-BOND F118CLR is an impact resistant, fiber-optic adhesive designed for use in any optical connector. This two-part epoxy remains at a constant viscosity for a minimum of 30 minutes. This allows ..
Volume Resistivity 1.00e+11 ohm-cm
1.00e+11 ohm-cm
conditioned; IEC 60093
EMS-Grivory Grivory® TSGZ-15/4 PA666-GF15
Information provided by EMS Grivory
Volume Resistivity 1.00e+11 ohm-cm
1.00e+11 ohm-cm
IEC 60093
BASF Ultraform N 2640 Z6 UNC POM
Ultraform N 2640 Z6 UNC is an elastomer-modified injection molding POM grade with excellent impact strength.
Volume Resistivity 1.00e+11 ohm-cm

@Thickness 0.750 mm
1.00e+11 ohm-cm

@Thickness 0.0295 in
IEC 60093
Ascend Performance Materials Vydyne® 47H BK0501 Nylon 66, Impact Modified, DAM
Vydyne® 47H BK0501 is general-purpose, impact-modified PA66 resin. Available in black, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vyd..
Volume Resistivity 1.00e+11 ohm-cm

@Thickness 0.750 mm
1.00e+11 ohm-cm

@Thickness 0.0295 in
IEC 60093
Ascend Performance Materials Vydyne® 47H Nylon 66, Impact Modified, DAM
Vydyne® 47H is general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vydyne 4..
Volume Resistivity 1.00e+11 ohm-cm
1.00e+11 ohm-cm
ASTM D257
3M Scotch-Weld™ DP125 Gray Epoxy Adhesive
Scotch-Weld epoxy adhesive DP125 Gray is a filled, pigmented version of the Scotch-Weld epoxy adhesive DP125 Translucent and has similar performance and flexibility properties.Information provided b..
Volume Resistivity 1.00e+11 ohm-cm
1.00e+11 ohm-cm
IEC 60093
Celanese Hostaform® S 9244 XAP2 ™ POM, Impact Modified
POM copolymer, modifiedInformation provided by Celanese Corporation.
Volume Resistivity >= 1.00e+11 ohm-cm
>= 1.00e+11 ohm-cm
Radici Radiflam® S RV300AE (dry) Nylon 6
Radiflam® S is a range of flame retardant polyamides 6 (PA 6) used for injection molding and extrusion for all applications where high fire resistance is required.Information provided by Radici gro..
Volume Resistivity 1.00e+11 ohm-cm
1.00e+11 ohm-cm
Radici Radilon® A USX200 (cond.) Nylon 66
Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov..
Volume Resistivity 1.00e+11 ohm-cm
1.00e+11 ohm-cm
IEC 60093
BASF Ultramid® B3UG4 LS BK 23215 20% Glass Filled PA66 FR (Conditioned)
Description: Halogen-free and phosphorus free flame retardant injection-molding grade with outstanding free-flow properties, good electrical properties and low smoke density; resistant to glow wire..
Volume Resistivity 1.00e+11 ohm-cm
1.00e+11 ohm-cm
IEC 60093
BASF Ultraform® N2644 Z9 POM + PUR
Description: Elastomer modified injection molding grade for applications requiring low modulus. Good acoustic damping.Information provided by BASF