Plastcom SLOVALEN PC 99 GF 30/1M Polypropylene reinforced with glass fiber, improved flowing

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 30% Glass Fiber Filler
Manufacturer Plastcom spol. s r.o.
Trade Name SLOVALEN
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plastcom SLOVALEN PC 99 GF 30/1M Polypropylene reinforced with glass fiber, improved flowing.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Modified copolymer PP for injection molding, reinforced with 30% glass fiber, improved flowing. Applied in all industry branches. Delivered in natural mode and in the full RAL color scale.Information Provided by Plastcom spol. s r.o.
Physical Properties Metric English Comments
Density 1.11 g/cc
0.0401 lb/in³
STN EN ISO 1183-1
Filler Content 30 %
30 %
Linear Mold Shrinkage 0.0058 cm/cm
0.0058 in/in
STN EN ISO 294-4
Linear Mold Shrinkage, Transverse 0.0127 cm/cm
0.0127 in/in
STN EN ISO 294-4
Melt Flow 23 g/10 min

@Load 2.16 kg,
Temperature 230 °C
23 g/10 min

@Load 4.76 lb,
Temperature 446 °F
STN EN ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength at Break 75.0 MPa
10900 psi
STN EN ISO 527-2
Elongation at Break 3.0 %
3.0 %
STN EN ISO 527-2
Tensile Modulus 5.00 GPa
725 ksi
STN EN ISO 527-2
Flexural Strength 95.0 MPa
13800 psi
STN EN ISO 178
Flexural Modulus 4.20 GPa
609 ksi
STN EN ISO 178
Charpy Impact Unnotched 4.00 J/cm²

@Temperature -20.0 °C
19.0 ft-lb/in²

@Temperature -4.00 °F
STN EN ISO 179
4.80 J/cm²

@Temperature 23.0 °C
22.8 ft-lb/in²

@Temperature 73.4 °F
STN EN ISO 179
Charpy Impact, Notched 0.250 J/cm²

@Temperature -20.0 °C
1.19 ft-lb/in²

@Temperature -4.00 °F
STN EN ISO 179
0.600 J/cm²

@Temperature 23.0 °C
2.86 ft-lb/in²

@Temperature 73.4 °F
STN EN ISO 179
Thermal Properties Metric English Comments
Melting Point 145 °C
293 °F
STN EN 11357-1
Deflection Temperature at 1.8 MPa (264 psi) 125 °C
257 °F
STN EN ISO 75-2 (A)
Vicat Softening Point 145 °C
293 °F
STN EN ISO 306
Processing Properties Metric English Comments
Melt Temperature 200 - 250 °C
392 - 482 °F
Mold Temperature 40.0 - 80.0 °C
104 - 176 °F
Drying Temperature 80.0 °C

@Time 14400 sec
176 °F

@Time 4.00 hour
Injection Pressure 70.0 - 120 MPa
10200 - 17400 psi