Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 28.0 kV/mm | 711 kV/in | IEC 60112 |
Proto3000 ABS-M30i Fused Deposition Modeling Polymer Description: ABS-M30i is a high strength material well suited for the medical, pharmaceutical and food packaging industries. Parts manufactured with ABS-M30i material are biocompatible (ISO 10993 ce.. |
|||
Dielectric Strength | 28.0 kV/mm | 711 kV/in | |
Quadrant EPP Quadrant PC 1000 extruded (ISO Data) Quadrant Engineering Plastic Products is marketing non-UV-stabilized polycarbonate stock shapes under the trade name Quadrant PC 1000. It is a natural, “non-optical” industrial quality (clear, tra.. |
|||
Dielectric Strength | 28.0 kV/mm | 711 kV/in | 1.6mm; ASTM D149 |
Kingfa LONOY 1200 PC/PBT Alloy Features:Excellent balance propertiesGood weather resistanceGood size stabilitySmooth surfaceUniform colorApplications:Injection moldingAutomobile bumperAutomobile interior/exterior trim partsBusine.. |
|||
Dielectric Strength | 28.0 kV/mm | 711 kV/in | ASTM D149/DIN 53481 |
Kolon KOLEFIN® KO133MT20 M/F Reinforced Polypropylene KOLEFIN® has excellent mechanical properties and its cost is lower than other engineering plastics. KOLEFIN® is widely used in the automotive industry and business applications.Good mechanica.. |
|||
Dielectric Strength | 28.0 kV/mm | 711 kV/in | ASTM D149/DIN 53481 |
Kolon KOLEFIN® KO133MT30 M/F Reinforced Polypropylene KOLEFIN® has excellent mechanical properties and its cost is lower than other engineering plastics. KOLEFIN® is widely used in the automotive industry and business applications.Good mechanica.. |
|||
Dielectric Strength | 28.0 kV/mm | 711 kV/in | VDE 0303 |
GEHR Plastics PPS-40GF Polyphenylene Sulfide, 40% Glass Fiber The linear polyphenylensulfide belongs to the semi-crystalline materials and offers a very high mechanical capacity, thermal and chemical resistance distinguished at the same time, high dimensional .. |
|||
Dielectric Strength | 28.0 kV/mm | 711 kV/in | ASTM D149 |
Kolon SPESIN® KP270BL General Purpose PBT Compound Resin Excellent waterproofnessApplications: ConnectorsInformation provided by API-Kolon. |
|||
Dielectric Strength | 28.0 kV/mm | 711 kV/in | Conditioned; IEC 60243-1 |
Lanxess Durethan® AKV 30 G H2.0 SR1 900051 Nylon 66, 30% Glass Fiber PA 66, injection molding grade, 30% glass fibers, better surface than AKV 30 H2.0, good heat-ageing resistance |
|||
Dielectric Strength | 28.0 kV/mm | 711 kV/in | Conditioned; IEC 60243-1 |
Lanxess Durethan® T 40 ZS 000000 Partially aromatic polyamide Partially aromatic polyamide, injection molding and extrusion grade, easy release, transparent in all wall thicknesses, isotropic shrinkage, mechanical and electrical properties largely unaffected b.. |
|||
Dielectric Strength | 28.0 kV/mm | 711 kV/in | IEC 60243-1 |
Lanxess Pocan® B 3225 901510 PBT, 20% Glass Fiber PBT, 20% glass fibers, injection molding |
|||
Dielectric Strength | 28.0 kV/mm | 711 kV/in | Conditioned; IEC 60243-1 |
Lanxess Durethan® T 40 000000 Partially aromatic polyamide Partially aromatic polyamide, injection molding and extrusion grade, transparent in all wall thicknesses, isotropic shrinkage, mechanical and electrical properties largely unaffected by conditioning.. |
|||
Dielectric Strength | 28.0 kV/mm | 711 kV/in | IEC 60243 |
Solvay TECHNYL® A 218 V20 Black 21N PA66, 20% glass fiber, Conditioned Description: Polyamide PA66, reinforced with 20% of glass fiber, heat stabilized, for injection molding.Available in: EuropeProduct Applications: TECHNYL A 218 V20 is used in all sectors of industry.. |
|||
Dielectric Strength | 28.0 kV/mm @Thickness 1.50 mm |
711 kV/in @Thickness 0.0591 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics NORYL WCA871A PPE (Asia Pacific) Flame retardant performance and mechanical properties capable of meeting UL VW-1 requirement and 105C temperature rating as defined UL1581. UL1581 tests conducted on 1.0mmD wire with AWG28 conductor.. |
|||
Dielectric Strength | 28.0 kV/mm | 711 kV/in | IEC 60243 |
Solvay TECHNYL® A 230 V13 PA66, 13% glass fiber, Conditioned Description: Modified polyamide 66, reinforced with 13% of glass fiber, with improved impact resistance, for injection molding.Available in: Europe and North AmericaProduct Applications: In addition.. |
|||
Dielectric Strength | 28.0 kV/mm | 711 kV/in | ASTM D149 |
Solvay Specialty Polymers Polidiemme® G/450 Thermoset Elastomer (TSE) Polidiemme® XLPO -Cross-linkable Polyolefin. Elastomer based compound crosslinkable by ambient moisture, consisting of a silane pregrafted base compound to be used with a catalyst masterbatch (S.. |
|||
Dielectric Strength | 28.0 kV/mm | 711 kV/in | IEC 60243 |
Solvay TECHNYL® A 216 V20 PA66, 20% glass fiber, Conditioned Description: Polyamide 66, reinforced with 20% of glass fiber, for injection molding.Available in: Europe Product Applications: TECHNYL® A 216 V20 is used in all sectors of industry, offering and.. |
|||
Dielectric Strength | 28.0 kV/mm | 711 kV/in | |
Covestro Makroblend® UT-620 G Polycarbonate + Polyester Blend Key Features:Contains FillerHigh impact or high impact modifiedLight stabilized or stable to lightSuitable processing methods:Injection moldingInformation provided by Bayer Polymers.As of 1 Septembe.. |
|||
Dielectric Strength | 28.0 kV/mm | 711 kV/in | conditioned; IEC 60243-1 |
EMS-Grivory Grivory® BZ 3 PA6 Information provided by EMS Grivory |
|||
Dielectric Strength | 28.0 kV/mm | 711 kV/in | CEI 60243-1 |
Addiplast Addinyl A2 E Flame Retardant Nylon 66 Flame retardant, halogen freeInformation provided by Addiplast. |
|||
Dielectric Strength | 28.0 kV/mm @Thickness 0.500 mm |
711 kV/in @Thickness 0.0197 in |
|
Advanced Ceramics ALC 1082 (C-786) Alumina Information provided by Advanced Ceramics Limited (ACL) |
|||
Dielectric Strength | 28.0 kV/mm | 711 kV/in | IEC 60243-1 |
DSM Arnite® TV4 260 S PBT-30% Glass Reinforced (European and Asian Grade) Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame .. |
|||
Dielectric Strength | 28.0 kV/mm | 711 kV/in | IEC 60243-1 |
Vyncolit Neopreg Kinel® SK60 L8G Glass Fiber Reinforced Molding Compound High flow, epoxy based molding compound long glass fiber reinforced with excellent long term property retention over a wide temperature range and climate conditions. It is particularly suited fo.. |
|||
Dielectric Strength | 28.0 kV/mm @Thickness 2.00 mm |
711 kV/in @Thickness 0.0787 in |
ASTM D149 |
Beijing Chemical Industry KAIFA® MN301-G25 Nylon 66 Resin 25% glass fiber reinforced, flame retardantInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Dielectric Strength | >= 28.0 kV/mm | >= 711 kV/in | Transformer Oil; Ø 93x3mm; IEC 243-1 |
SYNTHOS Krasten® 552M High Impact Polystyrene High impact grade with a wide range of Applications. Processed mainly by injection moulding. Production of consumer goods and technical parts subjected to increased mechanical stress. Good results i.. |
|||
Dielectric Strength | 28.0 kV/mm | 711 kV/in | IEC 60243-1 |
Solvay Specialty Polymers Ixef® 5002 Polyarylamide (PARA), 20% GlassPTFE
(discontinued **) Ixef 5002 is a 20% glass-fiber reinforced, PTFE modified polyarylamide which exhibits very good mechanical performance, very good surface gloss, and superior wear properties.- Natural: Ixef 5002/008.. |