Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 1.60 GPa | 232 ksi | |
Plastcom SLOVALEN PC 79 T 20 PP/C reinforced with 20% mineral filler Features: Modified PP for injection moulding with the content of 20% mineral filling. Increased rigidity, strength and thermal. Decreased shrinkage. Antistatic agent. Delivered in natural mode and i.. |
|||
Tensile Modulus | 1.60 GPa | 232 ksi | ASTM D638 |
Shell Carilon® D26CX100 Polyketone, Advanced Extrusion Grade
(discontinued **) Shell announced in Feb. 2000 that the Carilon product line is being discontinued. CARILON Polymer D26CX100 is an extrusion grade with mechanical properties that classify it as an engineering thermo.. |
|||
Tensile Modulus | 1.60 GPa @Thickness 0.100 mm |
232 ksi @Thickness 0.00394 in |
TD; ISO 527 |
Victrex® APTIV® 2000-050 Polyetheretherketone (PEEK) Polymer Film, Amorphous APTIV PEEK 2000 series films are the unfilled amorphous films made from VICTREX® PEEK polymer. The film provides a material solution for engineers in ultra-high performance applications.APTIV PEEK .. |
|||
Tensile Modulus | 1.60 GPa | 232 ksi | |
Imerys ImerPlastâ„¢ 10WPCT Recycled Polyolefin Resin A black, UV stabilized, recycled resin with no significant odor, for compounding with wood flour for extruded decking applications. With added reinforcing filler and wood flour dispersant, ImerPlast.. |
|||
Tensile Modulus | 1.60 GPa | 232 ksi | ASTM D638 |
Iran Petrochemical (PCC) HIPS 8350 High Impact Polystyrene HIPS 8350 is a very high impact polystyrene used in the extrusion industry. This grade has an improved environmental stress crack resistance (ESCR) in comparison with standard high impact polystyre.. |
|||
Tensile Modulus | 1.60 GPa | 232 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics XYLEX HX8300HP PC+POLYESTER Medium flow, Transparent PC/Polyester alloy. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contact compliant... |
|||
Tensile Modulus | 1.60 GPa | 232 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics XYLEX HX8300HP PC+POLYESTER (Asia Pacific) Medium flow, Transparent PC/Polyester alloy. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contact compliant... |
|||
Tensile Modulus | 1.60 GPa | 232 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics XYLEX HX8300HP PC+POLYESTER (Europe-Africa-Middle East) Medium flow, Transparent PC/Polyester alloy. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contact compliant... |
|||
Tensile Modulus | 1.60 GPa | 232 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP STAT-LOY A3000LTH ABS LNP* STAT-LOY* A3000LTH is a compound based on ABS resin. Added features of this material include: Transparent, Antistatic, Formulation Locked. |
|||
Tensile Modulus | 1.60 GPa | 232 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics XYLEX X8300 PC+POLYESTER PC+Polyester, UV Stabilized, Transparent |
|||
Tensile Modulus | 1.60 GPa | 232 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Xylex X8300HP PC+POLYESTER (Asia Pacific) Transparent, US Food Contact compliant, chemically resistant.
This grade will no longer be supported with biocompatibility information and should not be used for medical applications which require b.. |
|||
Tensile Modulus | 1.60 GPa | 232 ksi | 1mm/min; ISO 527 |
Styrolution Terblend® N NM-13 ABS/PA6 (Dry) Terblend N NM-13 is a new experimental ABS/PA6-Blend with improved impact strength at low temperatures. It can be easily processed on any standard injection molding machine.Information provided by .. |
|||
Tensile Modulus | 1.60 GPa | 232 ksi | 1mm/min; ISO 527-2 |
Borealis Bormed™ DM55pharm Polypropylene Bormed™ DM55pharm is a low melt flow rate polypropylene homopolymer intended for extrusion and thermoforming. Its very good organoleptic properties allows this grade to be used with any master bat.. |
|||
Tensile Modulus | 1.60 GPa | 232 ksi | ISO 527-2 |
Total PPC 11642 Polypropylene, Heterophasic Copolymer, Injection Molding Polypropylene PPC 11642 is a nucleated antistatic heterophasic copolymer with high Melt Flow index of 60 g/10 min.Polypropylene PPC 11642 is characterized by high fluidity with good mechanical prope.. |
|||
Tensile Modulus | 1.60 GPa | 232 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® L 20 G PA12 Product Description: Grilamid L 20 LG is a normal viscosity, heat stabilized polyamide 12 non-reinforced injection molding grade. This product has very good flow characteristics Low moisture absorpt.. |
|||
Tensile Modulus | 1.60 GPa | 232 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® TR 90 PAMACM12 Product description: Grilamid TR 90 natural is a high purity transparent thermoplastic polyamide, based on aliphatic and cycloaliphatic monomers. Grilamid TR 90 natural offers outstanding properties.. |
|||
Tensile Modulus | 1.60 GPa | 232 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® XE 3817 black 9992 PA12 Product description: Grilamid XE 3817 black 9992 is a medium viscosity, heat and UV-stabilized Polyamid 12. Grilamid XE 3817 black 9992 is especially suitable for the coating of metal tubes and offe.. |
|||
Tensile Modulus | 1.60 GPa | 232 ksi | ASTM D638 |
Aclo Accutech Polypropylene Homopolymer HP0339T10L1 Talc Reinforced |
|||
Tensile Modulus | 1.60 GPa | 232 ksi | |
BASF Novolen® 1184 L Polypropylene Nucleated grade with high processing stability containing antistatic for thermoformed parts.Data was collected by ISO methods and provided by BASF. |
|||
Tensile Modulus | 1.60 GPa | 232 ksi | 1mm/min; ISO 527 |
BASF Ultramid® A27 E 01 PA66 (Conditioned) Ultramid A27 E 01 is a low-viscosity, general-purpose PA66 grade for compounding. It conforms to FDA requirements including, 21 CFR 177.1500,EU Directive 2002/72/EC, the German BfR recommendation ".. |
|||
Tensile Modulus | 1.60 GPa | 232 ksi | ASTM D638 |
Aclo Accutech Polypropylene Copolymer CP0436C30L Calcium Reinforced |
|||
Tensile Modulus | 1.60 GPa | 232 ksi | cond.; ISO 527 |
Azoty Tarnow™ Tarnamid® T-27 MCS 850 Polyamide 6 - Flame Retarded, Unreinforced Glow wire resistance 850°C, bromine and red phosphorus free, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has .. |
|||
Tensile Modulus | 1.60 - 1.70 GPa @Thickness 2.00 mm, Temperature 23.0 °C |
232 - 247 ksi @Thickness 0.0787 in, Temperature 73.4 °F |
Type IV, 1.0 mm/min; ASTM D638 |
Solvay Specialty Polymers Solef® 6020 Polyvinylidene Fluoride (PVDF)
(Unverified Data**) Solef® 6020 PVDF homopolymer has very high viscosity for membranes and lithium batteries. It is available exclusively as powder.Information provided by Solvay Specialty Polymers. |
|||
Tensile Modulus | 1.60 GPa | 232 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® TR 55 LZ PA12/MACMI Product description: Grilamid TR grades are transparent thermoplastic polyamides based on aliphatic and cycloaliphatic blocks. Grilamid TR 55 LZ offers a variety of interesting properties such as: c.. |
|||
Tensile Modulus | 1.60 GPa | 232 ksi | |
Radici Radilon® A 42 (cond.) Nylon 66 Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov.. |
|||
Tensile Modulus | 1.60 GPa | 232 ksi | ASTM D638 |
Azdel SuperLite® SL551400-100 PP Resin Matrix / 55% Glass Fiber (6 mm Molded Thickness) AZDEL SuperLite® SL551400-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic.. |
|||
Tensile Modulus | 1.60 GPa | 232 ksi | |
LATI Latimass 53/11-02 D030 PP Homopolymer, Impact Modified Specific density compound based on Polypropylene homopolymer (PPh), impact modified. Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation.. |
|||
Tensile Modulus | 1.60 GPa | 232 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® TS V0 PA666 Product description: Grilon TS V0 is an unreinforced, normal viscosity, self-extinguishing Polyamid 66 + Polyamide 6 injection molding grade. Grilon TS V0 is halogen free and free of red phosphorous.. |
|||
Tensile Modulus | 1.60 GPa | 232 ksi | Secant; ISO527-2/1 |
ExxonMobil PP7064L1 Polypropylene Impact Copolymer Product Description: A nucleated impact copolymer resin with medium flow, high stiffness and antistatic properties. It is suitable for molding applications like consumer products, closures, contain.. |
|||
Tensile Modulus | 1.60 GPa | 232 ksi | ISO 527 |
Manifattura Cattaneo PP-s Polypropylene Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a. |