Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.100 J/cm² | 0.476 ft-lb/in² | ISO 179/2C |
SABIC Innovative Plastics Cycolac® INP222 ABS Bulk MMASAN. Provides an economical option for achieving greater melt strength in polymers. |
|||
Charpy Impact, Notched | 0.100 J/cm² | 0.476 ft-lb/in² | ISO 179/2C |
SABIC Innovative Plastics Cycolac® INP562 ABS+SAN SABIC INP562 provides compatibility with a wider range of ABS grades than many color concentrate bases; allows better dispersion than pellets; allows concentrate manufacturers to produce both pellet.. |
|||
Charpy Impact, Notched | 0.100 J/cm² @Temperature 23.0 °C |
0.476 ft-lb/in² @Temperature 73.4 °F |
ISO 179/2C |
SABIC Innovative Plastics Cycolac® INP563 ABS SABIC INP563 provides compatibility with a wider range of ABS grades than many color concentrate bases; allows better dispersion than pellets; allows concentrate manufacturers to produce both pellet.. |
|||
Charpy Impact, Notched | 0.100 J/cm² | 0.476 ft-lb/in² | ISO 179/2C |
SABIC Innovative Plastics Cycolac® INP563 ABS+SAN SABIC INP563 provides compatibility with a wider range of ABS grades than many color concentrate bases; allows better dispersion than pellets; allows concentrate manufacturers to produce both pellet.. |
|||
Charpy Impact, Notched | 0.100 J/cm² | 0.476 ft-lb/in² | ISO 179/2C |
SABIC Innovative Plastics Cycolac® INP630 ABS+SAN INP630 is a specialty polymer that increases the service temperature of products. Can be used with a impact modifier to provide impact strength as well as high heat resistance. Provides excellent hi.. |
|||
Charpy Impact, Notched | 0.100 - 1.80 J/cm² | 0.476 - 8.57 ft-lb/in² | Average value: 0.967 J/cm² Grade Count:6 |
Overview of materials for PET + PBT Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "PET + PBT Unreinforced". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Charpy Impact, Notched | 0.100 J/cm² | 0.476 ft-lb/in² | ISO Data, Low Temp |
Americas Styrenics Styron® 666D Polystyrene
(discontinued **) STYRON® 666D general purpose polystyrene resin is used in injection molding applications, particularly for medical, pharmaceutical and food uses. It offers excellent clarity, intermediate flow char.. |
|||
Charpy Impact, Notched | 0.100 J/cm² | 0.476 ft-lb/in² | ISO 179/1eU |
Total Lacqrene® 4240(EU) High Impact Polystyrene
(discontinued **) LACQRENE® 4240 is a high heat resistance, high impact polystyrene for the extrusion industry. Good mechanical and thermal properties leads to the production of thermoformed articles of good rigidi.. |
|||
Charpy Impact, Notched | 0.100 - 4.80 J/cm² @Temperature -40.0 - 0.000 °C |
0.476 - 22.8 ft-lb/in² @Temperature -40.0 - 32.0 °F |
Average value: 0.394 J/cm² Grade Count:108 |
Overview of materials for Polypropylene with 20% Talc Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Talc Filler".Specific grades with primary filler content between 15% and 24% are .. |
|||
Charpy Impact, Notched | 0.100 - 1.80 J/cm² | 0.476 - 8.57 ft-lb/in² | Average value: 0.707 J/cm² Grade Count:60 |
Overview of materials for Nylon 6, Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum and max.. |
|||
Charpy Impact, Notched | 0.100 - 1.00 J/cm² @Temperature -30.0 - 30.0 °C |
0.476 - 4.76 ft-lb/in² @Temperature -22.0 - 86.0 °F |
Average value: 0.430 J/cm² Grade Count:22 |
Overview of materials for Nylon 6, 30% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 30% Mineral Filled". Specific grades with primary filler content between 25% and 34% are includ.. |
|||
Charpy Impact, Notched | 0.100 J/cm² | 0.476 ft-lb/in² | |
LATI Laticonther 52/11 CP1/600 F3 PP Homopolymer High thermal conductivity product based on Polypropylene homopolymer (PPh). Special filler. Potentially suitable for food/medical contact application.Availability: Africa & Middle East; Asia Pacific.. |
|||
Charpy Impact, Notched | 0.100 J/cm² @Temperature -30.0 °C |
0.476 ft-lb/in² @Temperature -22.0 °F |
80*10*4mm, Cut; ISO 179/1eA |
SABIC Innovative Plastics SABIC PPCOMPOUND 19T1020 PP SABIC® PPcompound 19T1020 is a general purpose, talc filled, heat stabilized homopolymer polypropylene compound. This compound exhibits high flow and is suitable for injection molding application.. |
|||
Charpy Impact, Notched | 0.100 J/cm² @Temperature -30.0 °C |
0.476 ft-lb/in² @Temperature -22.0 °F |
80*10*4mm, Cut; ISO 179/1eA |
SABIC Innovative Plastics SABIC PPCOMPOUND 19T1040 PP SABIC® PPcompound 19T1040 is a general purpose, talc filled, heat stabilized homopolymer polypropylene compound. This compound exhibits high flow and is suitable for injection molding application.. |
|||
Charpy Impact, Notched | 0.100 J/cm² @Temperature -30.0 °C |
0.476 ft-lb/in² @Temperature -22.0 °F |
80*10*4mm, Cut; ISO 179/1eA |
SABIC Innovative Plastics SABIC PPCOMPOUND 37T1020 PP SABIC® PPcompound 37T1020 is a general purpose, talc filled, heat stabilized copolymer polypropylene compound. This compound exhibits high impact and high flow, and is suitable for injection mold.. |
|||
Charpy Impact, Notched | 0.100 J/cm² | 0.476 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Valox® EH7025AG PBT+PET (Asia Pacific) Valox EH7025AG is a mineral filled PBT/PET that offers good surface appearance, good flow and good heat performance. EH7025AG was developed for automotiove bezel application. |
|||
Charpy Impact, Notched | 0.100 J/cm² | 0.476 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Valox® EH7025AG PBT+PET (Europe-Africa-Middle East) Valox EH7025AG is a mineral filled PBT/PET that offers good surface appearance, good flow and good heat performance. EH7025AG was developed for automotiove bezel application. |
|||
Charpy Impact, Notched | 0.100 - 0.200 J/cm² | 0.476 - 0.952 ft-lb/in² | ISO 179 |
Vyncolit 3640 CG Novolac Phenolic Graphite filled phenolic molding compound with excellent dimensional stability. Self-lubricating and has a low coefficient of friction. Not suitable for electrical applications.USES: Gas meter par.. |
|||
Charpy Impact, Notched | 0.100 J/cm² | 0.476 ft-lb/in² | ISO Data, Low Temp |
Dow Tyril® 125 SAN Dow TYRIL® 125 resin is specially formulated for blending and is an ideal carrier material for use in making color concentrates. It offers high melt flow and excellent chemical resistance.Data prov.. |
|||
Charpy Impact, Notched | 0.100 J/cm² | 0.476 ft-lb/in² | ISO Data, Low Temp |
Dow Tyril® 1000B SAN TYRIL® 1000B SAN copolymer offers the best balance of physical properties of all TYRIL grades. It also provides excellent processability and chemical resistance, superior heat resistance, and good .. |
|||
Charpy Impact, Notched | 0.100 J/cm² | 0.476 ft-lb/in² | DIN 53453 |
3A Composites Core Materials AIREX® R82.60 High Performance Structural Foam AIREX® R82 is a closed-cell, thermoplastic polymer foam that combines fire resistance with low smoke and toxicity, along with good dielectric properties. It has a good strength to weight ratio, ver.. |
|||
Charpy Impact, Notched | 0.100 - 1.20 J/cm² @Temperature -30.0 - -20.0 °C |
0.476 - 5.71 ft-lb/in² @Temperature -22.0 - -4.00 °F |
Average value: 0.500 J/cm² Grade Count:5 |
Overview of materials for Nylon 66, 20% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Mineral Filled". Specific grades with primary filler content between 15% and 24% are inclu.. |
|||
Charpy Impact, Notched | 0.100 J/cm² @Temperature 23.0 °C |
0.476 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Noryl CRX2201 PPE+HIPS (Europe-Africa-Middle East) Noryl* CRX2201 resin is a 25% mineral reinforced, injection moldable modified polyphenylene ether resin designed for improved chemical resistance when compared with standard Noryl resins. Noryl CRX.. |
|||
Charpy Impact, Notched | 0.100 - 0.600 J/cm² @Temperature -40.0 - -20.0 °C |
0.476 - 2.86 ft-lb/in² @Temperature -40.0 - -4.00 °F |
Average value: 0.193 J/cm² Grade Count:46 |
Overview of materials for Polypropylene with 40% Talc Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Talc Filler". Specific grades with primary filler content between 35% and 44% are.. |
|||
Charpy Impact, Notched | 0.100 - 20.0 J/cm² @Temperature -40.0 - -20.0 °C |
0.476 - 95.2 ft-lb/in² @Temperature -40.0 - -4.00 °F |
Average value: 2.00 J/cm² Grade Count:24 |
Overview of materials for Nylon 6, 10% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% are included. .. |
|||
Charpy Impact, Notched | 0.100 - 26.0 J/cm² @Temperature -20.0 - 0.000 °C |
0.476 - 124 ft-lb/in² @Temperature -4.00 - 32.0 °F |
Average value: 2.91 J/cm² Grade Count:16 |
Overview of materials for Polypropylene, Extrusion Grade This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Extrusion Grade". Each property range of values reported is minimum and maximum values of.. |
|||
Charpy Impact, Notched | 0.100 - 12.0 J/cm² @Temperature -30.0 - 0.000 °C |
0.476 - 57.1 ft-lb/in² @Temperature -22.0 - 32.0 °F |
Average value: 1.91 J/cm² Grade Count:27 |
Overview of materials for Polypropylene, Impact Modified; Molded/Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Impact Modified; Molded/Extruded". Each property range of values reported is minimum and .. |
|||
Charpy Impact, Notched | 0.100 - 2.00 J/cm² @Temperature -40.0 - -20.0 °C |
0.476 - 9.52 ft-lb/in² @Temperature -40.0 - -4.00 °F |
Average value: 0.596 J/cm² Grade Count:39 |
Overview of materials for Polypropylene with 20% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Glass Fiber Filler". Specific grades with glass content between 15% and 24% are i.. |
|||
Charpy Impact, Notched | 0.100 - 12.0 J/cm² @Temperature -40.0 - 0.000 °C |
0.476 - 57.1 ft-lb/in² @Temperature -40.0 - 32.0 °F |
Average value: 0.597 J/cm² Grade Count:136 |
Overview of materials for Polypropylene Copolymer This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene Copolymer". Each property range of values reported is minimum and maximum values of approp.. |