Overview of materials for Polyphenylene Sulfide (PPS) with 40% Glass Fiber Filler

Category Polymer , Thermoplastic , Polyphenylene Sulfide (PPS) , Polyphenylene Sulfide (PPS) with 40% Glass Fiber Filler
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Overview of materials for Polyphenylene Sulfide (PPS) with 40% Glass Fiber Filler.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS)- 40% Glass filled; Molded". Specific grades with glass content between 35% and 44% are included. Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 0.000926 - 1.80 g/cc
0.0000335 - 0.0650 lb/in³
Average value: 1.57 g/cc Grade Count:92
Filler Content 35.0 - 40.0 %
35.0 - 40.0 %
Average value: 39.8 % Grade Count:29
Water Absorption 0.0100 - 0.600 %
0.0100 - 0.600 %
Average value: 0.0488 % Grade Count:56
Water Absorption at Saturation 0.0200 - 0.100 %
0.0200 - 0.100 %
Average value: 0.0247 % Grade Count:19
Additive Loading 40.0 %
40.0 %
Average value: 40.0 % Grade Count:4
Linear Mold Shrinkage 0.000500 - 0.00600 cm/cm
0.000500 - 0.00600 in/in
Average value: 0.00243 cm/cm Grade Count:68
Linear Mold Shrinkage, Transverse 0.00400 - 0.0110 cm/cm
0.00400 - 0.0110 in/in
Average value: 0.00555 cm/cm Grade Count:47
Mechanical Properties Metric English Comments
Hardness, Rockwell M 94.0 - 104
94.0 - 104
Average value: 101 Grade Count:33
Hardness, Rockwell R 100 - 125
100 - 125
Average value: 120 Grade Count:30
Hardness, Shore D 86.0 - 88.0
86.0 - 88.0
Average value: 87.3 Grade Count:3
Tensile Strength, Ultimate 32.4 - 207 MPa
4700 - 30000 psi
Average value: 167 MPa Grade Count:84
59.2949 - 180 MPa

@Temperature -40.0 - 204 °C
8600.01 - 26100 psi

@Temperature -40.0 - 400 °F
Average value: 115 MPa Grade Count:5
Tensile Strength, Yield 124 - 185 MPa
18000 - 26800 psi
Average value: 148 MPa Grade Count:9
Elongation at Break 0.500 - 3.00 %
0.500 - 3.00 %
Average value: 1.56 % Grade Count:89
1.16 - 3.40 %

@Temperature -40.0 - 204 °C
1.16 - 3.40 %

@Temperature -40.0 - 400 °F
Average value: 2.00 % Grade Count:5
Modulus of Elasticity 3.10 - 37.3 GPa
450 - 5410 ksi
Average value: 15.1 GPa Grade Count:49
3.24054 - 17.7885 GPa

@Temperature -40.0 - 204 °C
470.007 - 2580.04 ksi

@Temperature -40.0 - 400 °F
Average value: 10.7 GPa Grade Count:6
Flexural Yield Strength 49.6 - 343 MPa
7200 - 49700 psi
Average value: 240 MPa Grade Count:83
126.864 - 256.485 MPa

@Temperature -40.0 - 204 °C
18400.0 - 37200.1 psi

@Temperature -40.0 - 400 °F
Average value: 181 MPa Grade Count:2
Flexural Modulus 6.89 - 34.9 GPa
1000 - 5060 ksi
Average value: 14.1 GPa Grade Count:83
6.20528 - 14.9616 GPa

@Temperature -40.0 - 204 °C
900.014 - 2170.03 ksi

@Temperature -40.0 - 400 °F
Average value: 9.58 GPa Grade Count:2
Compressive Yield Strength 35.0 - 285 MPa
5080 - 41300 psi
Average value: 235 MPa Grade Count:29
Poissons Ratio 0.370 - 0.430
0.370 - 0.430
Average value: 0.396 Grade Count:17
Shear Strength 55.8 - 97.0 MPa
8100 - 14100 psi
Average value: 80.9 MPa Grade Count:3
Izod Impact, Notched 0.374 - 4.48 J/cm
0.700 - 8.39 ft-lb/in
Average value: 1.06 J/cm Grade Count:63
3.41696 - 3.41696 J/cm

@Temperature -40.0 - -40.0 °C
6.40137 - 6.40137 ft-lb/in

@Temperature -40.0 - -40.0 °F
Average value: 3.42 J/cm Grade Count:2
Izod Impact, Unnotched 0.854 - 8.00 J/cm
1.60 - 15.0 ft-lb/in
Average value: 4.97 J/cm Grade Count:42
Izod Impact, Notched (ISO) 8.00 - 44.0 kJ/m²
3.81 - 20.9 ft-lb/in²
Average value: 14.6 kJ/m² Grade Count:32
7.00 - 10.0 kJ/m²

@Temperature -30.0 - -30.0 °C
3.33 - 4.76 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 9.07 kJ/m² Grade Count:7
Izod Impact, Unnotched (ISO) 20.0 - 48.0 kJ/m²
9.52 - 22.8 ft-lb/in²
Average value: 34.1 kJ/m² Grade Count:24
Charpy Impact Unnotched 2.80 - 5.30 J/cm²
13.3 - 25.2 ft-lb/in²
Average value: 4.40 J/cm² Grade Count:24
2.80 - 5.30 J/cm²

@Temperature -30.0 - -20.0 °C
13.3 - 25.2 ft-lb/in²

@Temperature -22.0 - -4.00 °F
Average value: 4.68 J/cm² Grade Count:8
Charpy Impact, Notched 0.700 - 2.20 J/cm²
3.33 - 10.5 ft-lb/in²
Average value: 1.01 J/cm² Grade Count:28
0.700 - 1.20 J/cm²

@Temperature -30.0 - -20.0 °C
3.33 - 5.71 ft-lb/in²

@Temperature -22.0 - -4.00 °F
Average value: 0.985 J/cm² Grade Count:10
Coefficient of Friction 0.160 - 0.500
0.160 - 0.500
Average value: 0.318 Grade Count:4
Thermal Properties Metric English Comments
CTE, linear 8.00 - 230 µm/m-°C
4.44 - 128 µin/in-°F
Average value: 25.5 µm/m-°C Grade Count:49
10.0 - 100 µm/m-°C

@Temperature -100 - 250 °C
5.56 - 55.6 µin/in-°F

@Temperature -148 - 482 °F
Average value: 21.2 µm/m-°C Grade Count:23
CTE, linear, Transverse to Flow 32.0 - 2780 µm/m-°C
17.8 - 1540 µin/in-°F
Average value: 118 µm/m-°C Grade Count:36
22.0 - 100 µm/m-°C

@Temperature -100 - 250 °C
12.2 - 55.6 µin/in-°F

@Temperature -148 - 482 °F
Average value: 81.8 µm/m-°C Grade Count:23
Specific Heat Capacity 1.00 - 1.50 J/g-°C
0.239 - 0.359 BTU/lb-°F
Average value: 1.33 J/g-°C Grade Count:6
Thermal Conductivity 0.200 - 0.340 W/m-K
1.39 - 2.36 BTU-in/hr-ft²-°F
Average value: 0.306 W/m-K Grade Count:25
Melting Point 278 - 285 °C
532 - 545 °F
Average value: 282 °C Grade Count:29
Maximum Service Temperature, Air 180 - 260 °C
356 - 500 °F
Average value: 215 °C Grade Count:25
Deflection Temperature at 0.46 MPa (66 psi) 250 - 282 °C
482 - 540 °F
Average value: 275 °C Grade Count:18
Electrical Properties Metric English Comments
Electrical Resistivity 1000 - 1.00e+17 ohm-cm
1000 - 1.00e+17 ohm-cm
Average value: 1.16e+16 ohm-cm Grade Count:54
Surface Resistance 1e+05 - 1.00e+16 ohm
1e+05 - 1.00e+16 ohm
Average value: 5.67e+15 ohm Grade Count:29
1.00e+12 - 1.00e+13 ohm

@Temperature 90.0 - 90.0 °C
1.00e+12 - 1.00e+13 ohm

@Temperature 194 - 194 °F
Average value: 5.50e+12 ohm Grade Count:2
Insulation Resistance 1.00e+11 - 1.00e+12 ohm

@Temperature 90.0 - 90.0 °C
1.00e+11 - 1.00e+12 ohm

@Temperature 194 - 194 °F
Average value: 5.15e+11 ohm Grade Count:13
Dielectric Constant 3.00 - 4.70
3.00 - 4.70
Average value: 3.92 Grade Count:46
Dielectric Strength 9.17 - 30.0 kV/mm
233 - 762 kV/in
Average value: 19.8 kV/mm Grade Count:49
Dissipation Factor 0.000200 - 0.0200
0.000200 - 0.0200
Average value: 0.00256 Grade Count:42
Arc Resistance 100 - 134 sec
100 - 134 sec
Average value: 126 sec Grade Count:33
Comparative Tracking Index 125 - 275 V
125 - 275 V
Average value: 145 V Grade Count:39