Overview of materials for Polycarbonate, 30% Glass Filled

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, 30% Glass Filled
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Overview of materials for Polycarbonate, 30% Glass Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 30% Glass Filled". Specific grades with glass content between 25% and 34% are included. Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 1.11 - 1.57 g/cc
0.0401 - 0.0567 lb/in³
Average value: 1.43 g/cc Grade Count:98
Filler Content 25.0 - 30.0 %
25.0 - 30.0 %
Average value: 29.4 % Grade Count:24
Water Absorption 0.0600 - 0.300 %
0.0600 - 0.300 %
Average value: 0.127 % Grade Count:46
Moisture Absorption at Equilibrium 0.0800 - 0.200 %
0.0800 - 0.200 %
Average value: 0.133 % Grade Count:6
Water Absorption at Saturation 0.100 - 0.400 %
0.100 - 0.400 %
Average value: 0.252 % Grade Count:6
Viscosity 250000 - 250000 cP

@Temperature 260 - 260 °C
250000 - 250000 cP

@Temperature 500 - 500 °F
Average value: 250000 cP Grade Count:1
250000 - 250000 cP

@Shear Rate 1000 - 1000 1/s
250000 - 250000 cP

@Shear Rate 1000 - 1000 1/s
Average value: 250000 cP Grade Count:1
Viscosity Test 48.0 cm³/g
48.0 cm³/g
Average value: 48.0 cm³/g Grade Count:3
Maximum Moisture Content 0.0200
0.0200
Average value: 0.0200 Grade Count:4
Linear Mold Shrinkage 0.000 - 0.0300 cm/cm
0.000 - 0.0300 in/in
Average value: 0.00259 cm/cm Grade Count:88
Linear Mold Shrinkage, Transverse 0.00300 - 0.00600 cm/cm
0.00300 - 0.00600 in/in
Average value: 0.00410 cm/cm Grade Count:15
Melt Flow 3.00 - 25.0 g/10 min
3.00 - 25.0 g/10 min
Average value: 8.86 g/10 min Grade Count:38
Mechanical Properties Metric English Comments
Hardness, Rockwell M 86.0 - 95.0
86.0 - 95.0
Average value: 91.7 Grade Count:12
Hardness, Rockwell R 115 - 123
115 - 123
Average value: 119 Grade Count:27
Tensile Strength, Ultimate 55.0 - 145 MPa
7980 - 21000 psi
Average value: 117 MPa Grade Count:71
50.0 - 80.0 MPa

@Temperature 60.0 - 120 °C
7250 - 11600 psi

@Temperature 140 - 248 °F
Average value: 66.7 MPa Grade Count:1
Tensile Strength, Yield 75.8 - 131 MPa
11000 - 19000 psi
Average value: 116 MPa Grade Count:40
Elongation at Break 1.00 - 9.00 %
1.00 - 9.00 %
Average value: 3.19 % Grade Count:82
1.40 - 1.50 %

@Temperature 60.0 - 120 °C
1.40 - 1.50 %

@Temperature 140 - 248 °F
Average value: 1.47 % Grade Count:1
Elongation at Yield 3.00 - 5.00 %
3.00 - 5.00 %
Average value: 4.00 % Grade Count:7
Modulus of Elasticity 3.80 - 10.5 GPa
551 - 1520 ksi
Average value: 7.73 GPa Grade Count:38
6.20 - 7.50 GPa

@Temperature 60.0 - 120 °C
899 - 1090 ksi

@Temperature 140 - 248 °F
Average value: 6.90 GPa Grade Count:1
Flexural Yield Strength 95.0 - 220 MPa
13800 - 31900 psi
Average value: 167 MPa Grade Count:81
Flexural Modulus 3.33 - 9.65 GPa
484 - 1400 ksi
Average value: 7.20 GPa Grade Count:89
Compressive Yield Strength 110 - 138 MPa
16000 - 20000 psi
Average value: 120 MPa Grade Count:7
Izod Impact, Notched 0.427 - 1.96 J/cm
0.800 - 3.67 ft-lb/in
Average value: 1.22 J/cm Grade Count:76
Izod Impact, Unnotched 0.981 - 11.2 J/cm
1.84 - 21.0 ft-lb/in
Average value: 7.34 J/cm Grade Count:21
Izod Impact, Notched (ISO) 10.0 - 15.0 kJ/m²
4.76 - 7.14 ft-lb/in²
Average value: 12.2 kJ/m² Grade Count:6
11.0 - 12.0 kJ/m²

@Temperature -30.0 - -30.0 °C
5.23 - 5.71 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 11.7 kJ/m² Grade Count:3
Izod Impact, Unnotched (ISO) 40.0 - 40.0 kJ/m²

@Temperature -30.0 - -30.0 °C
19.0 - 19.0 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 40.0 kJ/m² Grade Count:1
Charpy Impact Unnotched 3.00 - 4.50 J/cm²
14.3 - 21.4 ft-lb/in²
Average value: 3.90 J/cm² Grade Count:10
3.20 - 3.20 J/cm²

@Temperature -20.0 - -20.0 °C
15.2 - 15.2 ft-lb/in²

@Temperature -4.00 - -4.00 °F
Average value: 3.20 J/cm² Grade Count:1
Charpy Impact, Notched 0.400 - 1.20 J/cm²
1.90 - 5.71 ft-lb/in²
Average value: 0.842 J/cm² Grade Count:12
0.600 - 0.680 J/cm²

@Temperature -20.0 - -20.0 °C
2.86 - 3.24 ft-lb/in²

@Temperature -4.00 - -4.00 °F
Average value: 0.616 J/cm² Grade Count:5
Thermal Properties Metric English Comments
CTE, linear 10.0 - 50.0 µm/m-°C
5.56 - 27.8 µin/in-°F
Average value: 25.9 µm/m-°C Grade Count:27
CTE, linear, Transverse to Flow 60.0 µm/m-°C
33.3 µin/in-°F
Average value: 60.0 µm/m-°C Grade Count:7
Thermal Conductivity 0.220 - 0.317 W/m-K
1.53 - 2.20 BTU-in/hr-ft²-°F
Average value: 0.272 W/m-K Grade Count:9
Maximum Service Temperature, Air 120 - 140 °C
248 - 284 °F
Average value: 128 °C Grade Count:5
Deflection Temperature at 0.46 MPa (66 psi) 98.9 - 182 °C
210 - 360 °F
Average value: 147 °C Grade Count:63
Deflection Temperature at 1.8 MPa (264 psi) 90.6 - 149 °C
195 - 300 °F
Average value: 142 °C Grade Count:83
Vicat Softening Point 98.9 - 166 °C
210 - 331 °F
Average value: 150 °C Grade Count:29
UL RTI, Electrical 80.0 - 130 °C
176 - 266 °F
Average value: 109 °C Grade Count:13
UL RTI, Mechanical with Impact 80.0 - 130 °C
176 - 266 °F
Average value: 103 °C Grade Count:13
UL RTI, Mechanical without Impact 80.0 - 130 °C
176 - 266 °F
Average value: 107 °C Grade Count:13
Flammability, UL94 HB - 5VA
HB - 5VA
Average value: 2.00 Grade Count:67
Oxygen Index 31.0 - 36.0 %
31.0 - 36.0 %
Average value: 33.8 % Grade Count:6
Glow Wire Test 850 - 960 °C
1560 - 1760 °F
Average value: 919 °C Grade Count:8
Electrical Properties Metric English Comments
Electrical Resistivity 100 - 1.00e+17 ohm-cm
100 - 1.00e+17 ohm-cm
Average value: 1.27e+16 ohm-cm Grade Count:37
Surface Resistance 100 - 1.00e+17 ohm
100 - 1.00e+17 ohm
Average value: 5.52e+15 ohm Grade Count:23
Static Decay 2.00 sec
2.00 sec
Average value: 2.00 sec Grade Count:3
Dielectric Constant 3.20 - 3.80
3.20 - 3.80
Average value: 3.42 Grade Count:22
Dielectric Strength 16.9 - 47.5 kV/mm
430 - 1210 kV/in
Average value: 29.2 kV/mm Grade Count:26
Dissipation Factor 0.000800 - 0.00970
0.000800 - 0.00970
Average value: 0.00501 Grade Count:19
Arc Resistance 60.0 - 120 sec
60.0 - 120 sec
Average value: 114 sec Grade Count:9
Comparative Tracking Index 100 - 249 V
100 - 249 V
Average value: 178 V Grade Count:16