Overview of materials for Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled

Category Polymer , Thermoplastic , Liquid Crystal Polymer (LCP) , Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Overview of materials for Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled". Specific grades with glass content between 45% and 54% are included. Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 1.45 - 1.89 g/cc
0.0524 - 0.0683 lb/in³
Average value: 1.74 g/cc Grade Count:14
Filler Content 45.0 %
45.0 %
Average value: 45.0 % Grade Count:5
Water Absorption 0.0100 - 0.100 %
0.0100 - 0.100 %
Average value: 0.0700 % Grade Count:3
Moisture Absorption at Equilibrium 0.00600 - 1.10 %
0.00600 - 1.10 %
Average value: 0.372 % Grade Count:3
Linear Mold Shrinkage 0.000 - 0.00200 cm/cm
0.000 - 0.00200 in/in
Average value: 0.000869 cm/cm Grade Count:12
Linear Mold Shrinkage, Transverse 0.00100 - 0.00500 cm/cm
0.00100 - 0.00500 in/in
Average value: 0.00425 cm/cm Grade Count:12
Mechanical Properties Metric English Comments
Hardness, Rockwell M 58.0 - 93.0
58.0 - 93.0
Average value: 72.3 Grade Count:3
Tensile Strength, Ultimate 88.0 - 160 MPa
12800 - 23200 psi
Average value: 124 MPa Grade Count:14
20.0 - 190 MPa

@Temperature -40.0 - 250 °C
2900 - 27600 psi

@Temperature -40.0 - 482 °F
Average value: 85.1 MPa Grade Count:3
20.0 - 190 MPa

@Thickness 1.00 - 4.00 mm
2900 - 27600 psi

@Thickness 0.0394 - 0.157 in
Average value: 85.1 MPa Grade Count:3
Elongation at Break 0.600 - 3.30 %
0.600 - 3.30 %
Average value: 1.46 % Grade Count:14
0.300 - 0.900 %

@Temperature -40.0 - 250 °C
0.300 - 0.900 %

@Temperature -40.0 - 482 °F
Average value: 0.633 % Grade Count:2
0.300 - 0.900 %

@Thickness 1.00 - 4.00 mm
0.300 - 0.900 %

@Thickness 0.0394 - 0.157 in
Average value: 0.633 % Grade Count:2
Modulus of Elasticity 12.0 - 24.5 GPa
1740 - 3550 ksi
Average value: 18.5 GPa Grade Count:13
6.00 - 27.0 GPa

@Temperature -40.0 - 250 °C
870 - 3920 ksi

@Temperature -40.0 - 482 °F
Average value: 15.6 GPa Grade Count:3
6.00 - 27.0 GPa

@Thickness 1.00 - 4.00 mm
870 - 3920 ksi

@Thickness 0.0394 - 0.157 in
Average value: 15.6 GPa Grade Count:3
Flexural Yield Strength 158 - 250 MPa
22900 - 36300 psi
Average value: 192 MPa Grade Count:14
10.0 - 300 MPa

@Temperature -40.0 - 250 °C
1450 - 43500 psi

@Temperature -40.0 - 482 °F
Average value: 121 MPa Grade Count:3
10.0 - 300 MPa

@Thickness 0.790 - 4.00 mm
1450 - 43500 psi

@Thickness 0.0311 - 0.157 in
Average value: 121 MPa Grade Count:3
Flexural Modulus 10.0 - 24.0 GPa
1450 - 3480 ksi
Average value: 16.8 GPa Grade Count:14
5.00 - 25.5 GPa

@Temperature -40.0 - 250 °C
725 - 3700 ksi

@Temperature -40.0 - 482 °F
Average value: 13.8 GPa Grade Count:3
5.00 - 25.5 GPa

@Thickness 0.790 - 4.00 mm
725 - 3700 ksi

@Thickness 0.0311 - 0.157 in
Average value: 13.8 GPa Grade Count:3
Compressive Yield Strength 21.3 - 152 MPa
3090 - 22000 psi
Average value: 88.4 MPa Grade Count:5
Compressive Modulus 18.0 - 21.0 GPa
2610 - 3050 ksi
Average value: 19.8 GPa Grade Count:3
Izod Impact, Notched 0.588 - 2.50 J/cm
1.10 - 4.68 ft-lb/in
Average value: 1.38 J/cm Grade Count:5
Izod Impact, Unnotched 3.16 - 6.53 J/cm
5.92 - 12.2 ft-lb/in
Average value: 4.80 J/cm Grade Count:4
Izod Impact, Notched (ISO) 8.00 - 16.0 kJ/m²
3.81 - 7.61 ft-lb/in²
Average value: 10.9 kJ/m² Grade Count:6
Charpy Impact Unnotched 1.00 - 1.90 J/cm²
4.76 - 9.04 ft-lb/in²
Average value: 1.61 J/cm² Grade Count:7
1.20 - 1.30 J/cm²

@Temperature -30.0 - -30.0 °C
5.71 - 6.19 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 1.27 J/cm² Grade Count:4
Charpy Impact, Notched 0.360 - 1.20 J/cm²
1.71 - 5.71 ft-lb/in²
Average value: 0.866 J/cm² Grade Count:10
0.800 - 1.00 J/cm²

@Temperature -30.0 - -30.0 °C
3.81 - 4.76 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 0.950 J/cm² Grade Count:4
Thermal Properties Metric English Comments
CTE, linear 2.00 - 15.0 µm/m-°C
1.11 - 8.33 µin/in-°F
Average value: 4.82 µm/m-°C Grade Count:12
-1.00 - 7.00 µm/m-°C

@Temperature 55.0 - 260 °C
-0.556 - 3.89 µin/in-°F

@Temperature 131 - 500 °F
Average value: 2.88 µm/m-°C Grade Count:4
-1.00 - 7.00 µm/m-°C

@Thickness 2.00 - 4.00 mm
-0.556 - 3.89 µin/in-°F

@Thickness 0.0787 - 0.157 in
Average value: 2.88 µm/m-°C Grade Count:4
CTE, linear, Transverse to Flow 17.0 - 80.0 µm/m-°C
9.44 - 44.4 µin/in-°F
Average value: 55.4 µm/m-°C Grade Count:12
76.0 - 100 µm/m-°C

@Temperature 55.0 - 260 °C
42.2 - 55.6 µin/in-°F

@Temperature 131 - 500 °F
Average value: 83.8 µm/m-°C Grade Count:4
76.0 - 100 µm/m-°C

@Thickness 2.00 - 4.00 mm
42.2 - 55.6 µin/in-°F

@Thickness 0.0787 - 0.157 in
Average value: 83.8 µm/m-°C Grade Count:4
Specific Heat Capacity 1.50 J/g-°C
0.359 BTU/lb-°F
Average value: 1.50 J/g-°C Grade Count:3
Thermal Conductivity 0.320 - 0.400 W/m-K
2.22 - 2.78 BTU-in/hr-ft²-°F
Average value: 0.357 W/m-K Grade Count:3
Melting Point 280 - 357 °C
536 - 675 °F
Average value: 337 °C Grade Count:13
Deflection Temperature at 1.8 MPa (264 psi) 240 - 315 °C
464 - 599 °F
Average value: 286 °C Grade Count:14
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+12 - 1.00e+16 ohm-cm
1.00e+12 - 1.00e+16 ohm-cm
Average value: 2.42e+15 ohm-cm Grade Count:11
Surface Resistance 1.00e+11 - 1.00e+17 ohm
1.00e+11 - 1.00e+17 ohm
Average value: 9.84e+15 ohm Grade Count:11
Dielectric Constant 3.40 - 5.00
3.40 - 5.00
Average value: 4.32 Grade Count:12
5.20 - 5.60

@Temperature 120 - 200 °C
5.20 - 5.60

@Temperature 248 - 392 °F
Average value: 5.37 Grade Count:2
5.20 - 5.60

@Frequency 60.0 - 1.00e+6 Hz
5.20 - 5.60

@Frequency 60.0 - 1.00e+6 Hz
Average value: 5.37 Grade Count:2
Dielectric Strength 21.0 - 45.0 kV/mm
533 - 1140 kV/in
Average value: 30.4 kV/mm Grade Count:10
20.0 - 40.0 kV/mm

@Temperature 100 - 200 °C
508 - 1020 kV/in

@Temperature 212 - 392 °F
Average value: 27.6 kV/mm Grade Count:3
20.0 - 40.0 kV/mm

@Thickness 0.800 - 3.20 mm
508 - 1020 kV/in

@Thickness 0.0315 - 0.126 in
Average value: 27.6 kV/mm Grade Count:3
Dissipation Factor 0.00600 - 0.0310
0.00600 - 0.0310
Average value: 0.0171 Grade Count:12
0.00800 - 0.0830

@Temperature 120 - 200 °C
0.00800 - 0.0830

@Temperature 248 - 392 °F
Average value: 0.0226 Grade Count:2
0.00800 - 0.0830

@Frequency 60.0 - 1.00e+6 Hz
0.00800 - 0.0830

@Frequency 60.0 - 1.00e+6 Hz
Average value: 0.0226 Grade Count:2
Comparative Tracking Index 150 - 250 V
150 - 250 V
Average value: 191 V Grade Count:10