Processing Properties Metric English Comments
Front Barrel Temperature 290 - 310 °C
554 - 590 °F
PolyOne Stat-Tech™ PC-08CF/000 FR V0 Polycarbonate (PC)
Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound..
Front Barrel Temperature 290 - 310 °C
554 - 590 °F
Injection Molding
LG Chemical LUCON CP6062EX PC/ABS+CNT
Description: Sheet Extrusion or Injection Molding, PC/ABS+CNT, Electrostatic Dissipation, Wide Processing Range, Low Surface ResistivityApplication: BLU Carrying TrayCAS No. 103598-77-2, 9003-56-9, ..
Front Barrel Temperature 290 - 330 °C
554 - 626 °F
Injection Molding
LG Chemical LUPOY GP2102 PC+GF10%
Description: Injection Molding, PC+GF10%, General Purpose, Good Toughness, Chemical ResistanceApplication: Mobile Phone HousingCAS: 103598-77-2 and 65997-17-3Information provided by LG Chemical
Front Barrel Temperature 290 - 330 °C
554 - 626 °F
LG Chemical LUPOY GP-2400 General Purpose Modified PC, 40% Glass Fiber Reinforced, High Strength
Among the characteristics of LUPOY polycarbonate resins are excellent mechanical properties, high heat resistance, high impact strength, and dimensional stability.Applications:Automotive: Automotive..
Front Barrel Temperature 290 - 310 °C
554 - 590 °F
Injection Molding
LG Chemical LUPOY SC1004A PC
Description: Injection Molding, PC, General Purpose, High Toughness, Chemical resistance, High Impact (at Low Temperature)Application: Mobile Phone HousingCAS: 103598-77-2 and 143106-82-5Information..
Front Barrel Temperature 290 - 300 °C
554 - 572 °F
Injection Molding
LG Chemical LUPOY SC1004AU PC, High Impact
Description: Injection Molding, PC, High Impact, High Flow, Good WeatherabilityApplication: Electric & Electronic HousingCAS: 103598-77-2 and 143106-82-5Information provided by LG Chemical
Front Barrel Temperature 290 - 305 °C
554 - 581 °F
Injection Molding
LG Chemical LUPOY SC2202 PC+GF20%, High Impact
Description: Injection Molding, PC+GF20%, Good Toughness, Good Impact, Chemical ResistanceApplication: Mobile Phone HousingCAS: 103598-77-2 and 65997-17-3Information provided by LG Chemical
Front Barrel Temperature 290 - 305 °C
554 - 581 °F
Injection Molding
LG Chemical LUPOY SC2302 PC+GF30%, High Impact
Description: Injection Molding, PC+GF30%, Good Toughness, Good Impact, Chemical ResistanceApplication: Mobile Phone HousingCAS: 103598-77-2 and 65997-17-3Information provided by LG Chemical
Front Barrel Temperature 290 - 330 °C
554 - 626 °F
Injection Molding
LG Chemical LUPOY GN2101F PC+GF10%, Halogen Free, Flame Retardant, Heat Resistance
Description: Injection Molding, PC+GF10%, Halogen Free Flame Retardant, Heat ResistanceApplication: IT/OA, Electric & Electronic Housing and ComponentsCAS: 103598-77-2 and 65997-17-3Information prov..
Front Barrel Temperature 290 - 330 °C
554 - 626 °F
Injection Molding
LG Chemical LUPOY GN2201FM PC+GF20%, Halogen Free, Flame Retardant, Heat Resistance
Description: Injection Molding, PC+GF20%, Halogen Free Flame Retardant, Heat ResistanceApplication: IT/OA, Electric & Electronic Housing and ComponentsCAS: 103598-77-2 and 65997-17-3Information prov..
Front Barrel Temperature 290 - 310 °C
554 - 590 °F
Injection Molding
LG Chemical LUSEP SP2300 SPS+GF30%, General Purpose
Feature: Injection Molding, sPS+GF30%, General PurposeApplication: Pump Units, Pick-up Lends Holder, etc.CAS No. 9003-53-6 and 65997-17-3Information provided by LG Chemical
Front Barrel Temperature 290 °C
554 °F
Solvay Specialty Polymers Lavanta® 5115 WH 011 Polyester, High Performance (HPP), 15% Glass Fiber
Lavanta® 5115 WH011 is a 15% glass fiber reinforced, high-performance polyester (HPP) injection molding grade developed specifically for HB LED packaging applications that utilize surface mount ..
Front Barrel Temperature 290 °C
554 °F
Solvay Specialty Polymers Lavanta® 5115 WH 251 Polyester, High Performance (HPP), 15% Glass Fiber
Lavanta® 5115 WH 251 is a high-performance polyester (HPP) is a 15% glass reinforced, injection molding grade developed specifically for HB LED packaging applications that utilize surface mount t..
Front Barrel Temperature 290 °C
554 °F
Solvay Specialty Polymers Lavanta® 5115 WH224 Polyester, High Performance (HPP), 15% Glass Fiber
Lavanta® 5115 WH224 is a 15% glass fiber reinforced, high-performance polyester (HPP) injection molding grade developed specifically for HB LED packaging applications that utilize surface mount t..
Front Barrel Temperature 290 - 295 °C
554 - 563 °F
Solvay TECHNYL® A 20 V35 PA66, 35% glass fiber, DRY
Description: Flame retardant polyamide 66, reinforced with 35% of glass fiber, for injection molding.Available in: Asia Pacific, Europe, Latin America and North America.Product Applications: This ph..
Front Barrel Temperature 290 °C
554 °F
Extrusion lamination
DuPont Elvaloy® 1125 AC Ethylene and 25% Methyl Acrylate Copolymer
Elvaloy® 1125 AC is intended for coextrusion and molding. It can be recommended for blow molding of parts requiring permanent flexibility, stress cracking resistance and softness. Excellent fill..
Front Barrel Temperature 290 °C
554 °F
Extrusion lamination
DuPont Elvaloy® 1209 AC Ethylene and 9% Methyl Acrylate Copolymer
Elvaloy® 1209 AC is intended for film coextrusion and injection molding. It can be recommended in film applications where softness, flexibility and excellent sealing properties are needed.Elvaloy®..
Front Barrel Temperature 290 °C
554 °F
Extrusion lamination
DuPont Elvaloy® 1224 AC Ethylene and 24% Methyl Acrylate Copolymer
Elvaloy® 1224 AC is intended for extrusion, coextrusion, compounding and injection molding. Elvaloy® 1224 AC has good adhesion to various substrates (OPA, OPP, paperboard, etc.), gives excellent ..
Front Barrel Temperature 290 °C
554 °F
Extrusion lamination
DuPont Elvaloy® 1609 AC Ethylene and 9% Methyl Acrylate Copolymer
Elvaloy® 1609 AC is intended for film coextrusion and injection molding. It can be recommended in film applications where softness, flexibility and excellent sealing properties are needed.Elvaloy®..
Front Barrel Temperature 290 °C
554 °F
Extrusion lamination
DuPont Elvaloy® 1820 AC Ethylene and 20% Methyl Acrylate Copolymer
Elvaloy® 1820 AC is intended for film coextrusion, compounding and injection molding. Due to its high melt flow rate, it also can be used in extrusion coating/lamination. Elvaloy® 1820 AC has go..
Front Barrel Temperature 290 °C
554 °F
Extrusion lamination
DuPont Elvaloy® 1913 AC Ethylene and 13% Methyl Acrylate Copolymer
Elvaloy® 1913 AC is intended for film coextrusion and injection molding. It can be recommended in film applications where softness, flexibility and excellent sealing properties are needed.Elvaloy®..
Front Barrel Temperature 290 °C
554 °F
Extrusion lamination
DuPont Elvaloy® 3217 AC Ethylene and 17% Butyl Acrylate Copolymer
Elvaloy® 3217 AC contains antioxidant, slip and antiblock additives.Elvaloy® 3217 AC has been developed for film applications requiring a combination of softness, toughness and low friction. Typi..
Front Barrel Temperature 290 °C
554 °F
Extrusion lamination
DuPont Elvaloy® 3427 AC Ethylene and 27% Butyl Acrylate Copolymer
Elvaloy® 3427 AC can be used for coextrusion and compounding. It can also be used in extrusion coating. Elvaloy® 3427 AC is very soft and flexible, and has good adhesion to various polymers. It..
Front Barrel Temperature 290 °C
554 °F
Extrusion lamination
DuPont Elvaloy® 3717 AC Ethylene and 17% Butyl Acrylate Copolymer
Elvaloy® 3717 AC can be used for coextrusion, compounding and injection molding. In coextrusion, it can be used to improve sealing; in compounding, to improve low temperature and impact properties..
Front Barrel Temperature 290 °C
554 °F
Extrusion Coating
DuPont Nucrel® 30907 Ethylene Acid Copolymer Resin
Nucrel® 30907 is an ethylene acid copolymer resin available for use in conventional extrusion coating, coextrusion coating, and extrusion laminating equipment designed to process polyethylene resin..
Front Barrel Temperature 290 °C
554 °F
Extrusion lamination
DuPont Elvaloy® 2112 AC Ethylene and 12% Ethyl Acrylate Copolymer
Elvaloy® 2112 AC is intended for profile and tube extrusion. Its good chemical resistance, low temperature toughness and good flex life make it outstanding for tubing is various applications. The..
Front Barrel Temperature 290 °C
554 °F
Beijing Chemical Industry KAIFA® M109-G20N MPPO Resin
20% glass fiber reinforced, flame retardantInformation provided by Beijing Chemical Industry Research Institute (Group)
Front Barrel Temperature 290 - 330 °C
554 - 626 °F
Injection Molding
LG Chemical LUPOY GP2100 PC+GF10%, Heat Resistance
Description: Injection Molding, PC+GF10%, General Purpose, Heat ResistanceApplication: IT/OA, E&E Housing and Components, Automotive (Interior)CAS: 103598-77-2 and 65997-17-3Information provided by ..
Front Barrel Temperature 290 - 310 °C
554 - 590 °F
Injection Molding
LG Chemical LUPOY SC1004ML PC, High Impact
Description: Injection Molding, PC, General Purpose, High Impact, Good Coloring, Chemical ResistanceApplication: Mobile Phone HousingCAS: 103598-77-2 and 9046-16-6Information provided by LG Chemical..
Front Barrel Temperature 290 - 310 °C
554 - 590 °F
Injection Molding
LG Chemical LUCON CP6067 PC+CNT+CF
Description: Injection Molding, PC+CNT+CF, Electrostatic Dissipation, High Strength, High Flow & Good ProcessabilityApplication: Wafer Carrier Box, Conveyor belt bearing blockCAS No. 103598-77-2, 74..
Copyright © lookpolymers.com All Rights Reserved