Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Front Barrel Temperature = 554 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Front Barrel Temperature 290 - 330 °C
554 - 626 °F
PolyOne Edgetek® XP9242701 Polyphenylene Sulfide (PPS)
Injection Speed: 50 to 80% Holding Time: 3 to 9 sec Injection Time: 1 to 3 sec Cycle Time: 18 to 70 secInformation provided by PolyOne
Front Barrel Temperature 290 °C
554 °F
Extrusion lamination
DuPont Elvaloy® 1214 AC Ethylene and 14% Methyl Acrylate Copolymer  (discontinued **)
Elvaloy® 1214 AC is intended for film coextrusion and injection molding. It can be recommended in film applications where softness, flexibility and excellent sealing properties are needed.Elvaloy®..
Front Barrel Temperature 290 - 330 °C
554 - 626 °F
Injection Molding
LG Chemical LUPOY GN2101FC PC+GF10%, Halogen Free, Flame Retardant, Heat Resistance
Description: Injection Molding, PC+GF10%, Halogen Free Flame RetardanceApplication: IT/OA, Electric & Electronic Housing and ComponentsCAS: 103598-77-2 and 65997-17-3Information provided by LG Chemi..
Front Barrel Temperature 290 - 330 °C
554 - 626 °F
Injection Molding
LG Chemical LUPOY GP2102 PC+GF10%
Description: Injection Molding, PC+GF10%, General Purpose, Good Toughness, Chemical ResistanceApplication: Mobile Phone HousingCAS: 103598-77-2 and 65997-17-3Information provided by LG Chemical
Front Barrel Temperature 290 - 330 °C
554 - 626 °F
Injection Molding
LG Chemical LUPOY GP2200 PC+GF20%, Heat Resistance
Description: Injection Molding, PC+GF20%, General Purpose, Heat ResistanceApplication: IT/OA, E&E Housing and Components, Automotive (Interior)CAS: 103598-77-2 and 65997-17-3Information provided by ..
Front Barrel Temperature 290 - 330 °C
554 - 626 °F
Injection Molding
LG Chemical LUPOY GP2300 PC+GF30%, Heat Resistance
Description: Injection Molding, PC+GF30%, General Purpose, Heat ResistanceApplication: IT/OA, E&E Housing and Components, Automotive (Interior)CAS: 103598-77-2 and 65997-17-3Information provided by ..
Front Barrel Temperature 290 - 330 °C
554 - 626 °F
LG Chemical LUPOY GP-2400 General Purpose Modified PC, 40% Glass Fiber Reinforced, High Strength
Among the characteristics of LUPOY polycarbonate resins are excellent mechanical properties, high heat resistance, high impact strength, and dimensional stability.Applications:Automotive: Automotive..
Front Barrel Temperature 290 - 330 °C
554 - 626 °F
LG Chemical LUPOY GP-2401F General Purpose Modified PC, 40% Glass Fiber Reinforced, Flame Retardant
Among the characteristics of LUPOY polycarbonate resins are excellent mechanical properties, high heat resistance, high impact strength, and dimensional stability.Applications:Automotive: Automotive..
Front Barrel Temperature 290 - 310 °C
554 - 590 °F
Injection Molding
LG Chemical LUPOY SC1004A PC
Description: Injection Molding, PC, General Purpose, High Toughness, Chemical resistance, High Impact (at Low Temperature)Application: Mobile Phone HousingCAS: 103598-77-2 and 143106-82-5Information..
Front Barrel Temperature 290 - 300 °C
554 - 572 °F
Injection Molding
LG Chemical LUPOY SC1004AU PC, High Impact
Description: Injection Molding, PC, High Impact, High Flow, Good WeatherabilityApplication: Electric & Electronic HousingCAS: 103598-77-2 and 143106-82-5Information provided by LG Chemical
Front Barrel Temperature 290 - 310 °C
554 - 590 °F
Lavergne VYTEEN PCGF10BK PC 10% Glass Reinforced
Vyteen PCGF10BK is a 10% fiberglass reinforced general purpose Polycarbonate grade.Features: - Good processabilityTypical Applications: - Laptop computer docking - Laser printer gear - Toner car..
Front Barrel Temperature 290 - 310 °C
554 - 590 °F
Injection Molding
LG Chemical LUPOY GN1004FA PC, Halogen Free, Flame Retardant, Chemical Resistance
Description: Injection Molding, PC, Halogen Free Flame Retardant, Chemical Resistance, High Impact at Low TemperatureApplication: IT/OA Housing and ComponentsCAS: 103598-77-2 and 143106-82-5Informat..
Front Barrel Temperature 290 - 330 °C
554 - 626 °F
Injection Molding
LG Chemical LUPOY GN2101F PC+GF10%, Halogen Free, Flame Retardant, Heat Resistance
Description: Injection Molding, PC+GF10%, Halogen Free Flame Retardant, Heat ResistanceApplication: IT/OA, Electric & Electronic Housing and ComponentsCAS: 103598-77-2 and 65997-17-3Information prov..
Front Barrel Temperature 290 - 330 °C
554 - 626 °F
Injection Molding
LG Chemical LUPOY GN2201FM PC+GF20%, Halogen Free, Flame Retardant, Heat Resistance
Description: Injection Molding, PC+GF20%, Halogen Free Flame Retardant, Heat ResistanceApplication: IT/OA, Electric & Electronic Housing and ComponentsCAS: 103598-77-2 and 65997-17-3Information prov..
Front Barrel Temperature 290 °C
554 °F
Solvay Specialty Polymers Lavanta® 5115 WH 251 Polyester, High Performance (HPP), 15% Glass Fiber
Lavanta® 5115 WH 251 is a high-performance polyester (HPP) is a 15% glass reinforced, injection molding grade developed specifically for HB LED packaging applications that utilize surface mount t..
Front Barrel Temperature 290 °C
554 °F
Solvay Specialty Polymers Lavanta® 5115 WH224 Polyester, High Performance (HPP), 15% Glass Fiber
Lavanta® 5115 WH224 is a 15% glass fiber reinforced, high-performance polyester (HPP) injection molding grade developed specifically for HB LED packaging applications that utilize surface mount t..
Front Barrel Temperature 290 °C
554 °F
Extrusion lamination
DuPont Elvaloy® 1209 AC Ethylene and 9% Methyl Acrylate Copolymer
Elvaloy® 1209 AC is intended for film coextrusion and injection molding. It can be recommended in film applications where softness, flexibility and excellent sealing properties are needed.Elvaloy®..
Front Barrel Temperature 290 °C
554 °F
Extrusion lamination
DuPont Elvaloy® 1224 AC Ethylene and 24% Methyl Acrylate Copolymer
Elvaloy® 1224 AC is intended for extrusion, coextrusion, compounding and injection molding. Elvaloy® 1224 AC has good adhesion to various substrates (OPA, OPP, paperboard, etc.), gives excellent ..
Front Barrel Temperature 290 °C
554 °F
Extrusion lamination
DuPont Elvaloy® 1820 AC Ethylene and 20% Methyl Acrylate Copolymer
Elvaloy® 1820 AC is intended for film coextrusion, compounding and injection molding. Due to its high melt flow rate, it also can be used in extrusion coating/lamination. Elvaloy® 1820 AC has go..
Front Barrel Temperature 290 °C
554 °F
Extrusion lamination
DuPont Elvaloy® 1913 AC Ethylene and 13% Methyl Acrylate Copolymer
Elvaloy® 1913 AC is intended for film coextrusion and injection molding. It can be recommended in film applications where softness, flexibility and excellent sealing properties are needed.Elvaloy®..
Front Barrel Temperature 290 °C
554 °F
Extrusion lamination
DuPont Elvaloy® 2116 AC Ethylene and 16% Ethyl Acrylate Copolymer
Elvaloy® 2116 AC is intended for profile and tube extrusion. Its good chemical resistance, low temperature toughness and good flex life make it outstanding for specialty tubing. The material also..
Front Barrel Temperature 290 °C
554 °F
Extrusion lamination
DuPont Elvaloy® 3427 AC Ethylene and 27% Butyl Acrylate Copolymer
Elvaloy® 3427 AC can be used for coextrusion and compounding. It can also be used in extrusion coating. Elvaloy® 3427 AC is very soft and flexible, and has good adhesion to various polymers. It..
Front Barrel Temperature 290 °C
554 °F
Extrusion lamination
DuPont Elvaloy® 3717 AC Ethylene and 17% Butyl Acrylate Copolymer
Elvaloy® 3717 AC can be used for coextrusion, compounding and injection molding. In coextrusion, it can be used to improve sealing; in compounding, to improve low temperature and impact properties..
Front Barrel Temperature 290 °C
554 °F
Extrusion Coating
DuPont Nucrel® 30907 Ethylene Acid Copolymer Resin
Nucrel® 30907 is an ethylene acid copolymer resin available for use in conventional extrusion coating, coextrusion coating, and extrusion laminating equipment designed to process polyethylene resin..
Front Barrel Temperature 290 °C
554 °F
Extrusion lamination
DuPont Elvaloy® 1218 AC Ethylene and 18% Methyl Acrylate Copolymer
Elvaloy® 1218 AC is intended for coextrusion, compounding and injection molding. Elvaloy® 1218 AC has good adhesion to various substrates (OPA, OPP, paperboard, etc.), gives excellent sealing pro..
Front Barrel Temperature 290 °C
554 °F
Extrusion lamination
DuPont Elvaloy® 2112 AC Ethylene and 12% Ethyl Acrylate Copolymer
Elvaloy® 2112 AC is intended for profile and tube extrusion. Its good chemical resistance, low temperature toughness and good flex life make it outstanding for tubing is various applications. The..
Front Barrel Temperature 290 °C
554 °F
Extrusion lamination
DuPont Elvaloy® 2615 AC Ethylene and 15% Ethyl Acrylate Copolymer
Because of its high flexibility and high filler loading capacity, Elvaloy® 2615 AC is particularly suited for injection molded parts in the automotive and furniture industries. It also offers exce..
Front Barrel Temperature 290 °C
554 °F
Extrusion lamination
DuPont Elvaloy® 3107 AC Ethylene and 7% Butyl Acrylate Copolymer  (discontinued **)
Elvaloy® 3107 AC contains antioxidant, slip and antiblock additives.Elvaloy® 3107 AC is developed to give films with good sealing properties, impact strength at lower temperature, and low shrinkag..
Front Barrel Temperature 290 - 330 °C
554 - 626 °F
Injection Molding
LG Chemical LUPOY GP2100 PC+GF10%, Heat Resistance
Description: Injection Molding, PC+GF10%, General Purpose, Heat ResistanceApplication: IT/OA, E&E Housing and Components, Automotive (Interior)CAS: 103598-77-2 and 65997-17-3Information provided by ..
Front Barrel Temperature 290 - 310 °C
554 - 590 °F
Injection Molding
LG Chemical LUPOY SC1004ML PC, High Impact
Description: Injection Molding, PC, General Purpose, High Impact, Good Coloring, Chemical ResistanceApplication: Mobile Phone HousingCAS: 103598-77-2 and 9046-16-6Information provided by LG Chemical..