Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DuPont Elvaloy® 1224 AC Ethylene and 24% Methyl Acrylate Copolymer

Category Polymer , Film , Thermoplastic , Ethylene Methyl Acrylate , Ethylene-Methyl Acrylate Copolymer, Molding Grade
Manufacturer DuPont Packaging and Industrial Polymers
Trade Name Elvaloy®
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF DuPont Elvaloy® 1224 AC Ethylene and 24% Methyl Acrylate Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Elvaloy® 1224 AC is intended for extrusion, coextrusion, compounding and injection molding. Elvaloy® 1224 AC has good adhesion to various substrates (OPA, OPP, paperboard, etc.), gives excellent sealing properties and has high filler acceptance.Elvaloy® 1224 AC is easily processed on standard equipment used for low-density polyethylene.Information provided by DuPont.
Physical Properties Metric English Comments
Density 0.944 g/cc
0.0341 lb/in³
ASTM D792 - ISO 1183
Melt Flow 2.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
2.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238 - ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore A 78
78
ASTM D2240 - ISO 868
Hardness, Shore D 27
27
ASTM D2240 - ISO 868
Tensile Strength at Break 12.0 MPa
1740 psi
500 mm/min; ASTM D638 - ISO 527-2
Elongation at Break 846 %
846 %
500 mm/min; ASTM D638 - ISO 527-2
Tensile Modulus 0.0180 GPa
2.61 ksi
1 mm/min; ASTM D638 - ISO 527-2
Thermal Properties Metric English Comments
Melting Point 91.0 °C
196 °F
By DSC; ASTM D3418 - ISO 3146
Vicat Softening Point 48.0 °C
118 °F
A<sub>50</sub> (10N); ASTM D1525 - ISO 306
Processing Properties Metric English Comments
Rear Barrel Temperature 150 °C
302 °F
Extrusion lamination and extrusion coating
150 °C
302 °F
Cast film
150 °C
302 °F
Blown film
Middle Barrel Temperature 160 °C
320 °F
Blown film
210 °C
410 °F
Cast film
220 °C
428 °F
Extrusion lamination
Front Barrel Temperature 170 °C
338 °F
Blown film
250 °C
482 °F
Cast film
290 °C
554 °F
Extrusion lamination
Adapter Temperature 180 °C
356 °F
Blown film
250 °C
482 °F
Cast Film
290 °C
554 °F
Extrusion lamination
Die Temperature 180 °C
356 °F
Blown film
250 °C
482 °F
Cast film
290 °C
554 °F
Extrusion lamination
Descriptive Properties Value Comments
MA-Content 24 wt.%
DuPont Method