| Category | Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 20% Talc Filler |
| Manufacturer | RheTech Products |
| Trade Name | |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | RheTech Products HP506-01B 22% Talc Reinforced High Performance Polypropylene, UV Stabilized, Black.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.07 g/cc | 1.07 g/cc | 23/23°C; ASTM D792 |
| Filler Content | 22 % | 22 % | ASTM D5630 |
| Linear Mold Shrinkage | 0.013 cm/cm | 0.013 in/in | ASTM D955 |
| Melt Flow | 9.0 g/10 min <br>@Load 2.16 kg,<br> Temperature 230 °C |
9.0 g/10 min <br>@Load 4.76 lb,<br> Temperature 446 °F |
ASTM D1238 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore D | 75 | 75 | ASTM D2240 |
| Tensile Strength at Break | 31.7 MPa | 4600 psi | 2 in/min; ASTM D638 |
| Flexural Modulus | 2.41 GPa | 350 ksi | Tangent; ASTM D790 |
| Izod Impact, Notched | 0.267 J/cm <br>@Temperature 23.0 °C |
0.500 ft-lb/in <br>@Temperature 73.4 °F |
ASTM D256 |
| Gardner Impact | 0.451 J | 0.333 ft-lb | ASTM D5420 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 0.46 MPa (66 psi) | 121 °C | 250 °F | ASTM D648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 67.2 °C | 153 °F | ASTM D648 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Rear Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
| Middle Barrel Temperature | 204 - 232 °C | 400 - 450 °F | |
| Front Barrel Temperature | 210 - 238 °C | 410 - 460 °F | |
| Nozzle Temperature | 216 - 227 °C | 420 - 440 °F | |
| Mold Temperature | 26.7 - 48.9 °C | 80.0 - 120 °F | |
| Drying Temperature | 65.6 - 82.2 °C | 150 - 180 °F | |
| Dry Time | 1 - 2 hour | 1 - 2 hour | |
| Moisture Content | <= 0.050 % | <= 0.050 % | Recommended |
| Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
| Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
| Back Pressure | 0.345 - 1.03 MPa | 50.0 - 150 psi |