Polymer Property : Izod Impact, Notched = 0.500 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 0.267 J/cm

@Temperature 23.0 °C
0.500 ft-lb/in

@Temperature 73.4 °F
ASTM D256
RheTech Products FRP102-01 Polypropylene, Flame Retardant, Black
Applications: Electrical component housingsInjection molding conditions reported in table.Information provided by RheTech Products.
Izod Impact, Notched 0.267 J/cm

@Temperature 23.0 °C
0.500 ft-lb/in

@Temperature 73.4 °F
ASTM D256
RheTech Products T20P100-01UV 20% Talc Reinforced Polypropylene, UV Stabilized, General Purpose Black
Applications: Durable goodsElectronics housingsIP componentsClose out panelsInjection molding conditions reported in table.Information provided by RheTech Products.
Izod Impact, Notched 0.267 J/cm
0.500 ft-lb/in
0.125 inch bar; ASTM D256
Network Polymers MS 150 IF Styrene Methyl Methacrylate Terpolymer
Description: Styrene Methyl Methacrylate TerpolymerInformation provided by Network Polymers Inc.
Izod Impact, Notched 0.267 J/cm
0.500 ft-lb/in
ASTM D256
Network Polymers NPP 30-1200 TF20
Description: 20% Talc Filled Homopolymer PolypropyleneInformation provided by Network Polymers Inc.
Izod Impact, Notched 0.267 J/cm
0.500 ft-lb/in
0.125 inch bar; ASTM D256
Network Polymers Softflex® 1104
Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc.
Izod Impact, Notched 0.267 J/cm
0.500 ft-lb/in
ASTM D256 Type A
Quadrant EPP Nylatron® GSM Nylon, Cast MoS2 Filled Type 6 (ASTM Product Data Sheet)
Izod Impact, Notched 0.267 J/cm

@Thickness 3.17 mm
0.500 ft-lb/in

@Thickness 0.125 in
ASTM D256
RTP Company RTP 1100  Polyethylene Terephthalate (PET) Base Resin  (discontinued **)
Base ResinComments:UnfilledUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided by RTP Company.Data for this pro..
Izod Impact, Notched 0.267 J/cm

@Thickness 3.17 mm
0.500 ft-lb/in

@Thickness 0.125 in
ASTM D256
RTP Company RTP 1182  Polyethylene Terephthalate (PET) Carbon Fiber 15%  (discontinued **)&l
Carbon Fiber 15%Comments:Carbon FiberUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided by RTP Company.Data fo..
Izod Impact, Notched 0.267 J/cm
0.500 ft-lb/in
ASTM D256 Type A
Quadrant EPP Semitron® 420 ESd V (ASTM Product Data Sheet)
Izod Impact, Notched 0.267 J/cm
0.500 ft-lb/in
ASTM D256
Ravago Manufacturing Americas Enviramid™ N2340MGHL BK Post Consumer Recycle Nylon 6, 25/15% Glass/Mineral Filled
Heat Stabilized, Lubricated, Black and made from EnViramid™ Post Consumer Recycled NylonInformation provided by Ravago.
Izod Impact, Notched 0.267 J/cm
0.500 ft-lb/in
ASTM D256
M. Holland Company PP400 Polypropylene Homopolymer
Features: Medium Flow, General PurposeUses: Closures, Food Containers, Household Goods, VialsApprovals: FDA 21 CFR 177.1520Processing Method: Injection MoldingInformation provided by M. Holland.
Izod Impact, Notched 0.267 J/cm
0.500 ft-lb/in
ASTM D256
Global TPP-110 10% Talc Filled Polypropylene
Information provided by Global Polymers Corporation.
Izod Impact, Notched 0.267 J/cm

@Thickness 3.17 mm
0.500 ft-lb/in

@Thickness 0.125 in
ASTM D256
Techmer ES HiFill® PP 0121 B Polypropylene
Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforInformation provided by TP Composites, Inc.
Izod Impact, Notched 0.267 J/cm
0.500 ft-lb/in
at 0°F; ASTM D256
A. Schulman PP 1116-01 Polypropylene Molding Grade Copolymer Polypropylene
DescriptionPolypropylene PP 1116-01 is a molding grade copolymer polypropylene with improved low temperature toughness and good room temperature toughness. Information provided by A. Schulman.
Izod Impact, Notched 0.267 J/cm
0.500 ft-lb/in
at 0°F; ASTM D256
A. Schulman PP 1817-01 Polypropylene Utility Grade Random Co-Polymer
DescriptionPolypropylene PP 1817-01 is a utility grade random co-polymer which can be used for general purpose injection molding, extrusion, or blow molding applications. It does not have a gel spe..
Izod Impact, Notched 0.267 J/cm
0.500 ft-lb/in
ASTM D256
Formosa Plastics Formolene® 4100P Injection Molding Polypropylene
Homopolymer with ESCR AdditivesApplications: Closures, small appliances, housewares and toys.Formolene 4100P is a low viscosity, highly isotactic polypropylene homopolymer designed for various injec..
Izod Impact, Notched 0.267 J/cm
0.500 ft-lb/in
ASTM D256
A. Schulman PP 1667-01 Polypropylene Natural Homopolymer Polypropylene
DescriptionPolypropylene PP 1667-01 is an easy flowing natural homopolymer polypropylene. It is for injection molding large parts with thin sections requiring good stiffness, heat resistance, and c..
Izod Impact, Notched 0.267 J/cm
0.500 ft-lb/in
ASTM D256
A. Schulman PP 3487-01 Polypropylene Homopolymer Polypropylene
DescriptionPolypropylene PP 3487-01 is a special homopolymer polypropylene formulated with a long term heat aging resistance. This material has excellent resistance to chemicals and solvents. High..
Izod Impact, Notched 0.267 J/cm

@Thickness 3.17 mm
0.500 ft-lb/in

@Thickness 0.125 in
ASTM D 256
RTP Company RTP 1300 TC-C-30 Polyphenylene Sulfide (PPS), Thermally Conductive - Electrically Conductive - Flame Retardant
Izod Impact, Notched 0.267 J/cm
0.500 ft-lb/in
Tra-Con Tra-Bond F211 General Purpose Fiber Optic Epoxy Adhesive
TRA-BOND F211 is a general purpose fiber optic epoxy adhesive recommended for bonding and small volume potting applications where superior wetting and physical properties are needed at both high and..
Izod Impact, Notched 0.267 J/cm

@Thickness 3.17 mm
0.500 ft-lb/in

@Thickness 0.125 in
D 256
RTP Company RTP 1300 AR 10 TFE 15 Polyphenylene Sulfide (PPS), Aramid Fiber Reinforced - PTFE Lubricated
Izod Impact, Notched 0.267 J/cm

@Thickness 3.20 mm
0.500 ft-lb/in

@Thickness 0.126 in
ASTM D 256
RTP Company RTP 200 TC-C-40 FR Nylon 6/6 (PA), Thermally Conductive - Electrically Conductive - Flame Retardant
Izod Impact, Notched 0.267 J/cm

@Thickness 3.17 mm
0.500 ft-lb/in

@Thickness 0.125 in
ASTM D 256
RTP Company RTP 200 TC-I-25 FR Nylon 6/6 (PA), Thermally Conductive - Electrically Insulative - Flame Retardant
Izod Impact, Notched 0.267 J/cm

@Temperature 22.8 °C
0.500 ft-lb/in

@Temperature 73.0 °F
ASTM D256
0203HS PPS, Unfilled
A very easy flowing, heat stabilized unfilled grade designed for melt blown processing. This grade demonstrates excellent chemical resistance and thermal stability. Intended for extrusion applicati..
Izod Impact, Notched 0.267 J/cm

@Thickness 3.17 mm
0.500 ft-lb/in

@Thickness 0.125 in
ASTM D256
RTP Company RTP 200D GB 30  Nylon 6/12 (PA 6/12) Glass Bead 30%  (discontinued **)
Glass Bead 30%Comments:Glass BeadUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided by RTP Company.Data for th..
Izod Impact, Notched 0.267 J/cm
0.500 ft-lb/in
ASTM D256
A. Schulman PP 3488-01 Polypropylene Homopolymer Polypropylene
DescriptionPolypropylene PP 3488-01 is a specially formulated homopolymer polypropylene designed for large appliance injection molding. This material has excellent chemical resistance in addition t..
Izod Impact, Notched 0.267 J/cm

@Temperature 23.0 °C
0.500 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Ineos H65C-00 Polypropylene Homopolymer
This is a high melt flow clarified and lightly lubricated homopolymer designed for high-speed injection molding. It exhibits excellent see-through clarity and meets the requirements of the U.S. Foo..
Izod Impact, Notched 0.267 J/cm - NB
0.500 ft-lb/in - NB
Average value: 2.14 J/cm Grade Count:169
Overview of materials for Polypropylene, Impact Modified; Molded/Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Impact Modified; Molded/Extruded". Each property range of values reported is minimum and ..
Izod Impact, Notched 0.267 J/cm

@Thickness 3.17 mm
0.500 ft-lb/in

@Thickness 0.125 in
D 256
RTP Company RTP 1199 X 115085 D Polyethylene Terephthalate Glycol Modified (PETG), Carbon Nanotube - ESD Protection
Izod Impact, Notched 0.267 J/cm
0.500 ft-lb/in
ASTM D256A
Braskem D130C Homopolymer Polypropylene
Description: High BulkApplications: Suggested Uses Include Fine Denier Staple Fiber, High Speed Fiber SpinningThis resin meets the requirements for olefin polymers as defined in 21 CFR, section 177...