Processing Properties | Metric | English | Comments |
---|---|---|---|
Back Pressure | 0.345 - 1.03 MPa | 50.0 - 150 psi | |
Multibase Nylex™ 2185 R15 Polyamide + PP Glass fiber reinforcement, 15% Filler by Weight. Features: Crack Resistance, GoodDimensional Stability, GoodImpact Resistance, GoodMoisture ResistantProcessability, GoodForms:PelletsProcessing Metho.. |
|||
Back Pressure | 0.345 - 1.03 MPa | 50.0 - 150 psi | |
RheTech Products F43-01A 35% Glass Fiber/Mineral Co-Reinforced Polypropylene Copolymer, Chemically Coupled, Black Applications: Electrical component supportsFunctional supportsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Back Pressure | 0.345 - 1.03 MPa | 50.0 - 150 psi | |
RheTech Products FT4802-690UV Thermoplastic Polyolefin, UV Stabilized, HS5 Medium Dark Neutral Applications: Bodyside moldings and claddingsFacia and bumper coversExterior componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Back Pressure | 0.345 - 1.03 MPa | 50.0 - 150 psi | |
RheTech Products FT5100-04 Thermoplastic Polyolefin, UV Stabilized, White Applications: IP structural componentBody side moldingInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Back Pressure | 0.345 - 1.03 MPa | 50.0 - 150 psi | |
RheTech Products G13P100-332UV 13% Glass Fiber Reinforced Polypropylene, UV Stabilized, (GM 9772) Light Neutral Applications: Interior trimAir ducts - distributionFuel filler pocketInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Back Pressure | 0.345 - 1.03 MPa | 50.0 - 150 psi | |
RheTech Products HP514-438 14% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 167 Ebony Applications: Glove box binInterior trimSteering column trimConsolesAir ducts - distributionInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Back Pressure | 0.345 - 1.03 MPa | 50.0 - 150 psi | |
RheTech Products T15P100-00 12% Talc Reinforced Polypropylene, Natural Applications: Component housingConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Back Pressure | 0.345 - 1.03 MPa | 50.0 - 150 psi | |
RheTech Products T20P104-01 20% Talc Reinforced Polypropylene, Black Applications: Electronic housingsIP componentsHVAC ducts - air distributionClose out panelDurable goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Back Pressure | 0.345 - 1.03 MPa | 50.0 - 150 psi | |
RheTech Products T20P252-01 20% Talc Reinforced Polypropylene Copolymer, Black Applications: IP Structural componentsGlove box binWire troughInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Back Pressure | 0.345 - 1.38 MPa | 50.0 - 200 psi | |
PTS Tristar® PC-10R-(18) 18 MFI Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Back Pressure | 0.345 - 1.03 MPa | 50.0 - 150 psi | |
RheTech Products F32-01 32% Glass Fiber/Mineral Co-Reinforced Polypropylene, Chemically Coupled, Black Applications: Head lamp housingBracketsUnderhood componentsElectrical housingsFunctional supportsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Back Pressure | 0.345 - 1.21 MPa | 50.0 - 175 psi | keep minimum |
MRC Polymers MAXNITE™ 500 GF15 PET, 15% Glass Fiber Filled
(discontinued **) Information provided by MRC Polymers Inc. |
|||
Back Pressure | 0.345 - 0.689 MPa | 50.0 - 99.9 psi | |
LNP Thermocomp® LF-1006 MG Polyetheretherketone, Glass milled Glass Fiber
(discontinued **) Features: Low WarpageForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still a.. |
|||
Back Pressure | 0.345 MPa | 50.0 psi | |
Ineos Nova Zyntar® F7120 Developmental Flame Retardant Polystyrene
(discontinued **) Features: High flow for thin wall partsGood balance of physical propertiesUL94 V-0 @ 1.5 mm for black color Good aesthetics for injection molding Applications:Large television cabinetsConsumer elect.. |
|||
Back Pressure | 0.345 - 0.689 MPa | 50.0 - 100 psi | Typically 50 psi |
NOVA Chemicals DYLARK® 238 Impact Grade Engineering Resin Features:High heat resistance Good chemical resistance High impact strength Excellent flow characteristicsApplications:Automotive interior trim applications Automotive consoles Structural HousingsIn.. |
|||
Back Pressure | 0.345 - 0.689 MPa | 50.0 - 99.9 psi | |
LNP Lubricomp® EL-4030 Polyetherimide, PTFE Additive
(discontinued **) Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac.. |
|||
Back Pressure | 0.345 - 0.689 MPa | 50.0 - 99.9 psi | |
Solvay Specialty Polymers Udel® GF-110 Polysulfone (PSU)
(Unverified Data**) Udel GF-110, resin is a 10% glass fiber reinforced polysulfone (PSU). Glass fiber substantially increases the rigidity, tensile strength, creep resistance, dimensional stability and chemical resista.. |
|||
Back Pressure | 0.345 - 1.21 MPa | 50.0 - 175 psi | |
MRC Polymers NAXELLâ„¢ PC110-919 General Purpose Polycarbonate, Medium High MFR Polycarbonate for colorable productsMFR can be modified between 10 to 40 g/10minCan be UV stabilizedInternal and external lubricant can be addedCan be clear to color matchedNot for products that req.. |
|||
Back Pressure | 0.345 MPa | 50.0 psi | |
Multibase Multi-Flex® A 1540 Natural TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodSoftUV Resistance, Go.. |
|||
Back Pressure | 0.345 MPa | 50.0 psi | |
Multibase Multi-Flex® A 9402 MR TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodUV Resistance, Good .. |
|||
Back Pressure | 0.345 MPa | 50.0 psi | |
Wellman Wellamid® GS25-66 22L-N, 25% Glass Sphere Filled Nylon 66, Lubricated Typical Applications: Potentiometer liners, electrical coil forms, automotive window lift and power door lock switch bodies, gears, thick wall section moldings, emission control valves.Data provided.. |
|||
Back Pressure | 0.345 MPa | 50.0 psi | |
Wellman Wellamid® XT1482-N Impact Modified Nylon 66, Lubricated & Heat Stabilized Typical Applications: Automotive fasteners, living hinge, head lamp adjustment devices, ink pen components, wire separators, hardware components, window installation clips, safety equipment.Data pro.. |
|||
Back Pressure | 0.345 - 0.689 MPa | 50.0 - 100 psi | |
Elastocon TPE Technologies Elastocon® 8058N Thermoplastic Elastomer Elastocon® 8058N is a colorable thermoplastic elastomer formulated for applications that require rubber-like properties and a good surface finish. Elastocon® 8058N is FDA compliant and well suited.. |
|||
Back Pressure | 0.345 - 1.03 MPa | 50.0 - 150 psi | |
CTC SunPro® SP 200 P4058 Polypropylene Copolymer SunPro® SP 200 P 4058 is a general purpose, medium flow, polypropylene copolymer. It has applications in automotive wheel housings and general purpose automotive. Automotive Certifications: Chrysl.. |
|||
Back Pressure | 0.345 - 0.689 MPa | 50.0 - 100 psi | Processing |
ExxonMobil Santoprene® 111-35 Thermoplastic Elastomer A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range .. |
|||
Back Pressure | 0.345 - 0.689 MPa | 50.0 - 100 psi | |
ExxonMobil Santoprene® 8211-65 Thermoplastic Elastomer A soft, colorable, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in dif.. |
|||
Back Pressure | 0.345 - 1.72 MPa | 50.0 - 250 psi | |
Clariant Renol PCSP0006 Polycarbonate, Laser Markable Data provided by Clariant Masterbatches |
|||
Back Pressure | 0.345 - 0.689 MPa | 50.0 - 99.9 psi | |
Elastocon TPE Technologies Elastocon® STK56PA Thermoplastic Elastomer Elastocon® STK56PA thermoplastic elastomer has been developed for applications that require soft rubber-like properties and a good surface finish. Elastocon® STK56PA is well suited for consumer go.. |
|||
Back Pressure | 0.345 - 0.689 MPa | 50.0 - 100 psi | Processing |
ExxonMobil Santoprene® 171-55 Thermoplastic Elastomer
(discontinued **) A soft, black, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated use, as well as those.. |
|||
Back Pressure | 0.345 - 1.03 MPa | 50.0 - 150 psi | |
RheTech Products CC20P100-01 20% Calcium Carbonate Reinforced Polypropylene, Black Applications: ElectronicsConsumer GoodsInjection molding conditions reported in table.Information provided by RheTech Products. |