Processing Properties | Metric | English | Comments |
---|---|---|---|
Front Barrel Temperature | 210 - 238 °C | 410 - 460 °F | |
RheTech Products CC20P200-00 20% Calcium Carbonate Reinforced Polypropylene Copolymer, Natural Applications: Electrical housingsDurable goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 210 - 238 °C | 410 - 460 °F | |
RheTech Products F52-01 20% Mica Reinforced Polypropylene Copolymer, Black Applications: Functional support ductsHousingsUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 210 - 238 °C | 410 - 460 °F | |
RheTech Products FT4802-691UV Thermoplastic Polyolefin, UV Stabilized, RJ3 Dark Grey Green Applications: Bodyside moldings and claddingsFacia and bumper coversExterior componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 210 - 238 °C | 410 - 460 °F | |
RheTech Products HP531-00 22% Talc Reinforced High Performance Polypropylene Copolymer, Non-UV Stabilized, Natural Applications: IP structural componentsAir ducts - distributionA/B/C/ PillarsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 210 - 238 °C | 410 - 460 °F | |
RheTech Products M20P100-01 20% Mica Reinforced Polypropylene, Black Applications: Fan shroudsFiller panelsAir ductsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 210 - 238 °C | 410 - 460 °F | |
RheTech Products T12P600-430UVBG 12% Talc Reinforced Polypropylene Copolymer, UV Stabilized, Interior 848 Black, Blow Molding Grade Applications: Flipper panelsSeat backsLoad floorInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 210 - 238 °C | 410 - 460 °F | |
RheTech Products T20P100-01UV 20% Talc Reinforced Polypropylene, UV Stabilized, General Purpose Black Applications: Durable goodsElectronics housingsIP componentsClose out panelsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 210 - 221 °C | 410 - 430 °F | |
PlastiComp Complet® LGF40 - PP Homopolymer Polypropylene, 40% Long Glass Fiber Reinforced Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polypropylene with 40% long glass fiber reinforcementInformation provided by PlastiCom.. |
|||
Front Barrel Temperature | 210 - 227 °C | 410 - 440 °F | |
Polymer Resources ABS-G5 ABS, 5% Glass Reinforced Acrylonitrile Butadiene Styrene, 5% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information .. |
|||
Front Barrel Temperature | 210 - 227 °C | 410 - 440 °F | |
Polymer Resources ABS-G5-[color]-3 ABS, 5% Glass Reinforced, UV-stabilized Acrylonitrile Butadiene Styrene, 5% Glass Reinforced, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sampl.. |
|||
Front Barrel Temperature | 210 - 227 °C | 410 - 440 °F | |
Polymer Resources ABS-G15 ABS, 15% Glass Reinforced Acrylonitrile Butadiene Styrene, 15% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information.. |
|||
Front Barrel Temperature | 210 - 232 °C | 410 - 450 °F | |
Ineos Nova Zyntar® F7080UV Developmental Flame Retardant Polystyrene
(discontinued **) Features: General purpose non-Deca based resin (does not combine with Decabromodiphenyloxide)Good indoor UV light color stability(grey colors)UL94 V-0 @ 1.5 mm for all colors Good aesthetics for inj.. |
|||
Front Barrel Temperature | 210 - 230 °C | 410 - 446 °F | Injection Molding |
LG Chemical KEYFLEX BT GN7142F Ester Type TPE Description: Extrusion Molding, TPC-ET, Halogen Free Flame Retardant, Low ModulusApplication: Cable & Wire Jackets, Hose & Tubing, SheetInformation provided by LG Chemical |
|||
Front Barrel Temperature | 210 - 232 °C | 410 - 450 °F | |
Ineos Nova Zyntar® 7000 Flame Retardant Polystyrene Features:General purpose workhorse resinGood flow for injection moldingUL94 V-0 @ 1.5 mm for all colors UL94 5VA rating FOAMED @ 4.6 mm, 0.87-1.07 g/cc density, natural colorCustom colors availableA.. |
|||
Front Barrel Temperature | 210 - 230 °C | 410 - 446 °F | Injection Molding |
LG Chemical MP211 ABS, Low Gloss, Metal Plating Feature: Injection Molding, High Flow, Metal PlatingApplication: Decorative Parts (Home Appliance Door Handle Etc)CAS No. 9003-56-9 and 9003-54-7Information provided by LG Chemical |
|||
Front Barrel Temperature | 210 - 227 °C | 410 - 440 °F | |
MRC Polymers MAXTELâ„¢ 600 GF20 TPO, 20% Glass Fiber Filled For automotive exterior applications. Excellent process ability and dimensional stability.Internal and external lubricants can be addedCan be UV StabilizedInformation provided by MRC Polymers Inc. |
|||
Front Barrel Temperature | 210 - 227 °C | 410 - 440 °F | |
MRC Polymers MAXTELâ„¢ 600 GF30 TPO, 30% Glass Fiber Filled For automotive exterior applicationsExcellent process ability and dimensional stabilityCan be UV StabilizedInternal and external lubricants can be addedInformation provided by MRC Polymers Inc. |
|||
Front Barrel Temperature | 210 - 230 °C | 410 - 446 °F | |
LG Chemical LUPOL GP-3152F General Purpose Polypropylene, 15% Mineral Fillers, High Impact, Flame Retardant LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive: Bumper cover, instrument panel, glove box, air cleaner.. |
|||
Front Barrel Temperature | 210 - 230 °C | 410 - 446 °F | |
LG Chemical LUPOL LW-4407 Low Warpage Polypropylene, 40% Glass Fiber/Mineral Filler Reinforced, Heat Resistant LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive: Bumper cover, instrument panel, glove box, air cleaner.. |
|||
Front Barrel Temperature | 210 - 230 °C | 410 - 446 °F | |
LG Chemical LUPOL TE-5104K Thermoplastic Elastomer Alloy, 10% Polymer Alloy, High Modulus LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive exterior parts.Information Provided by LG Chem |
|||
Front Barrel Temperature | 210 - 230 °C | 410 - 446 °F | |
LG Chemical LUPOS GP-2200H General Purpose ABS, 20% Glass Fiber Reinforced, High Heat Resistance LUPOS resins are glass fiber reinforced styrene copolymers. LUPOS have improved strength, rigidity and dimensional stability. They offer excellent heat resistance, minimal mold shrinkage and have .. |
|||
Front Barrel Temperature | 210 - 230 °C | 410 - 446 °F | |
Samyang Triloy® 170 PC/PBT alloy Characteristics:Impact resistantChemical resistantDimensional stabilityProcessabilityFlame retardantApplications:Automotive bumperAutomotive outdoor handleAll information provided by Samyang |
|||
Front Barrel Temperature | 210 - 230 °C | 410 - 446 °F | |
Samyang Triloy® 210 PC/ABS alloy Characteristics:Impact resistantHeat resistantGood flowApplications:Camera partsExterior panelCluster fasciaWheel coverStructural applicationI/P. core panelHelmet shellGlove box doorCowl vent grillA.. |
|||
Front Barrel Temperature | 210 - 230 °C | 410 - 446 °F | |
Samyang Triloy® 210NH PC/ABS alloy, Flame Retardant Non-halogenCharacteristics:Impact resistantHeat resistantFlame retardantDimensional stabilityProcessabilityApplications:Cellular phoneMonitor housingCoffee makerHair dryerO/A partAll information pro.. |
|||
Front Barrel Temperature | 210 - 245 °C | 410 - 473 °F | Injection Molding |
Arkema Group KYNAR® 740 Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeabili.. |
|||
Front Barrel Temperature | 210 - 240 °C | 410 - 464 °F | Tube Extrusion |
Arkema Group KYNAR® 460 Polyvinylidene Fluoride Homopolymer - Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. Broad molecular weight distribution. High stability in harsh thermal, chemical and ultraviolet environments. High toughness a.. |
|||
Front Barrel Temperature | 210 - 224 °C | 410 - 435 °F | |
Ravago Manufacturing Americas Hylac® GP30G ABS, 30% Glass Fiber Reinforced Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Front Barrel Temperature | 210 - 220 °C | 410 - 428 °F | Injection Molding |
LG Chemical LI912 ASA Description: Good Weatherability, General PurposeApplication: Mail Box, Sprinkler, Sash Joiner, Toy, Satellite Antenna CoverCAS: 26299-47-8Information provided by LG Chemical |
|||
Front Barrel Temperature | 210 - 243 °C | 410 - 469 °F | |
Styrolution NAS® 30 Series High Performance Styrenic It has sparkling clarity and good scratch resistance. This easily processed copolymer blends well with K-Resin® to modify flexibility, surface hardness, and HDT. It meets USP XXIII Spec. of Class.. |
|||
Front Barrel Temperature | 210 - 238 °C | 410 - 460 °F | |
RheTech Products G20P252-00 20% Glass Fiber Reinforced Polypropylene Copolymer, Natural Applications: Interior trimArm rest insertConsolesDome light housingInjection molding conditions reported in table.Information provided by RheTech Products. |