Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Gardner Impact | 0.451 J | 0.333 ft-lb | ASTM D5420 |
RheTech Products F37-01 40% Glass Fiber/Mineral Co-Reinforced Polypropylene, Chemically Coupled, Black Applications: ElectronicsBracketsBattery traysInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 0.451 J | 0.333 ft-lb | ASTM D5420 |
RheTech Products F40-01 40% Glass Fiber/Mineral Co-Reinforced Polypropylene, Chemically Coupled, Black Applications: Battery traysAir cleaner housingFunctional support decksInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 0.451 J | 0.333 ft-lb | ASTM D5420 |
RheTech Products F43-01 35% Glass Fiber/Mineral Co-Reinforced Polypropylene Copolymer, Chemically Coupled, Black Applications: Fan shroudsDip trayFunctional supportsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 0.451 J | 0.333 ft-lb | ASTM D5420 |
RheTech Products F56-01 40% Glass Fiber/Mineral Co-Reinforced Polypropylene, Chemically Coupled, Black Applications: Consumer goodsUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 0.451 J | 0.333 ft-lb | ASTM D5420 |
RheTech Products G20P100-00 20% Glass Fiber Reinforced Polypropylene, Natural Applications: Arm rest insertVacuum canisterStorage binConsolesBattery traysInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 0.451 J | 0.333 ft-lb | ASTM D5420 |
RheTech Products G20P100-599 20% Glass Fiber Reinforced Polypropylene, UV Stabilized, (Ford BJ4A) Medium Dark Parchment Applications: Arm rest insertVacuum canister insertStorage binConsolesBattery traysInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 0.451 J | 0.333 ft-lb | ASTM D5420 |
RheTech Products G30P100-01 30% Glass Fiber Reinforced Polypropylene, Black Applications: Fender apronsUnderhood componentsStructural componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 0.451 J | 0.333 ft-lb | ASTM D5420 |
RheTech Products GC20P100-00 15% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Natural Applications: Air Ducts - distributionBracketsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 0.451 J | 0.333 ft-lb | ASTM D5420 |
RheTech Products GC20P100-04 20% Glass Fiber Reinforced Polypropylene, Chemically Coupled, White Applications: Air Ducts - distributionBracketsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 0.451 J | 0.333 ft-lb | ASTM D5420 |
RheTech Products GC20P100-177UV 20% Glass Fiber Reinforced Polypropylene, Chemically Coupled, UV Stabilized, (Chrysler HS5) Gray Applications: Air Ducts - distributionBracketsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 0.451 J | 0.333 ft-lb | ASTM D5420 |
RheTech Products M30P100-01 30% Mica Reinforced Polypropylene, Black Applications: Fan shroudsHVAC ductworkClose-out panelsFiller panelsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 0.451 J | 0.333 ft-lb | ASTM D5420 |
RheTech Products RCT120-01 20% Talc Reinforced Polypropylene, Black, Recycled Content Applications: HVAC and I/P ComponentsUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 0.451 J | 0.333 ft-lb | ASTM D5420 |
RheTech Products G20P100-601 20% Glass Fiber Reinforced Polypropylene, UV Stabilized, (Ford ZUA5) Dark Graphite Applications: Arm rest insertVacuum canisterStorage binConsolesBattery traysInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 0.451 J | 0.333 ft-lb | ASTM D5420 |
RheTech Products G20P252-01 20% Glass Fiber Reinforced Polypropylene Copolymer, Black Applications: Interior trimArm rest insertConsolesDome light housingInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 0.451 J | 0.333 ft-lb | ASTM D5420 |
RheTech Products HP506-01 20% Talc Reinforced High Performance Polypropylene, Black Applications: Underhood componentsLamp housingsHVAC ductsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 0.451 J | 0.333 ft-lb | ASTM D5420 |
RheTech Products HP506-01A 21% Talc Reinforced High Performance Polypropylene, UV Stabilized, Black Applications: Automotive interior applicationsHVAC ductsTail lamp housingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 0.451 J | 0.333 ft-lb | ASTM D5420 |
RheTech Products M25P100-01 25% Mica Reinforced Polypropylene, Black Applications: Underhood applicationsInternal I/P ComponentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 0.451 - 271 J | 0.333 - 200 ft-lb | Average value: 13.4 J Grade Count:74 |
Overview of materials for Polypropylene with 20% Talc Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Talc Filler".Specific grades with primary filler content between 15% and 24% are .. |
|||
Gardner Impact | 0.451 J | 0.333 ft-lb | ASTM D3029 |
Plastics Group Polifil® GFPPCC-30 30% Glass Reinforced Polypropylene Polifil® GFPPCC series compounds are homopolymer polypropylenes reinforced with chemically coupled glass fibers. These compounds offer superior strength and stiffness, improved elevated temperature.. |
|||
Gardner Impact | 0.451 J | 0.333 ft-lb | ASTM D3029 |
Plastics Group Polifil® GFPPCC-40 40% Glass Reinforced Polypropylene Polifil® GFPPCC series compounds are homopolymer polypropylenes reinforced with chemically coupled glass fibers. These compounds offer superior strength and stiffness, improved elevated temperature.. |
|||
Gardner Impact | 0.451 J | 0.333 ft-lb | ASTM D3029 |
Plastics Group Polifil® M-20 20% Mica-Reinforced Polypropylene Polifil® M series compounds are homopolymer polypropylene resins reinforced with mica. They combine an improved range of high-stiffness values with low mold shrinkage. These compounds are used in l.. |
|||
Gardner Impact | 0.451 J | 0.333 ft-lb | ASTM D3029 |
Plastics Group Polifil® GFPP-30 30% Glass-Reinforced Polypropylene Polifil® GFPP series compounds are homopolymer polypropylene resins reinforced with glass fibers. They provide high impact with increased strength, stiffness, surface hardness, and higher continuou.. |
|||
Gardner Impact | 0.451 J | 0.333 ft-lb | ASTM D5420 |
RheTech Products M20P101-01 20% Mica Reinforced Polypropylene, Black Applications: Radiator air bafflesHVAC ductworkClose-out and filler panelsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 0.451 J | 0.333 ft-lb | ASTM D5420 |
RheTech Products F24-01 20% Glass Fiber/Mineral Co-Reinforced Polypropylene Copolymer, Chemically Coupled, Black Applications: Head lamp housingsBracketsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 0.451 J | 0.333 ft-lb | ASTM D5420 |
RheTech Products G20P100-406 20% Glass Fiber Reinforced Polypropylene, UV Stabilized, (Ford ZUEA) Midnight Black Applications: Arm rest insertVacuum canisterStorage binConsolesBattery traysInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 0.451 J | 0.333 ft-lb | ASTM D5420 |
RheTech Products GC20P100-00UV 20% Glass Fiber Reinforced Polypropylene, Chemically Coupled, UV Stabilized, Natural Injection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 0.451 J | 0.333 ft-lb | ASTM D5420 |
RheTech Products GC20P100-01 20% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Black Applications: Air Ducts - distributionBracketsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 0.451 J | 0.333 ft-lb | ASTM D5420 |
RheTech Products GC20P105-08FA 20% Glass Fiber Reinforced Polypropylene, Chemically Coupled, FDA Compliant, Black Applications: Water system housingFDA approved partsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 0.451 J | 0.333 ft-lb | ASTM D5420 |
RheTech Products HP506-01B 22% Talc Reinforced High Performance Polypropylene, UV Stabilized, Black Applications: Underhood componentsLamp housingsHVAC ductsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 0.451 - 2.26 J | 0.333 - 1.67 ft-lb | Average value: 1.13 J Grade Count:7 |
Overview of materials for Polypropylene with 30% Mica Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Mica Filler". Specific grades with primary filler content between 25% and 34% are.. |