Processing Properties | Metric | English | Comments |
---|---|---|---|
Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
RheTech Products FT1055-624 Thermoplastic Polyolefin, Non-UV Stabilized, General Purpose Light Grey Applications: Bumper coversInterior trimSplash shieldsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
RheTech Products FT4650-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural Applications: Scuff platesExterior grillesBodyside moldingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
RheTech Products FT4650-581UV Thermoplastic Polyolefin, UV Stabilized, HD2 Medium Quartz Metallic Applications: Scuff platesExterior grillesBodyside moldingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
RheTech Products FT4700-01A Thermoplastic Polyolefin, Non-UV Stabilized, Black Applications: CladdingsBodyside moldingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
RheTech Products FT4702-527UV Thermoplastic Polyolefin, UV Stabilized, XS9 Dark Neutral Metallic Applications: Exterior door moldingsRigid bumper coversBodyside claddings and fairingsAutomotive grillesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
RheTech Products FT7016-01 Thermoplastic Polyolefin, Non-UV Stabilized, Black Applications: Bumper coversCladdingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
RheTech Products G13P100-559UV 13% Glass Fiber Reinforced Polypropylene, UV Stabilized, (GM WPP 646H) Charcoal Metallic Applications: Interior trimAir ducts - distributionFuel filler pocketInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
RheTech Products G20P100-00 20% Glass Fiber Reinforced Polypropylene, Natural Applications: Arm rest insertVacuum canisterStorage binConsolesBattery traysInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
RheTech Products GC10P200-01 10% Glass Fiber Reinforced Polypropylene Copolymer, Non-UV Stabilized, Chemically Coupled, Black Applications: HousingsStorage binsBracketsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
RheTech Products GC20P100-00 15% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Natural Applications: Air Ducts - distributionBracketsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
RheTech Products GC35P200-01UV 35% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, UV Stabilized, General Purpose Black Applications: BracketsStructural componentsHeadlamp housingsWindow frameInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
RheTech Products HP514-438 14% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 167 Ebony Applications: Glove box binInterior trimSteering column trimConsolesAir ducts - distributionInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
RheTech Products HP519-01 26% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, Black Applications: Interior trim moldingsSill platesAir ductsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
RheTech Products HP521-01 15% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, Black Applications: Interior trimIP structural componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
RheTech Products HP531-00 22% Talc Reinforced High Performance Polypropylene Copolymer, Non-UV Stabilized, Natural Applications: IP structural componentsAir ducts - distributionA/B/C/ PillarsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
RheTech Products M30P100-01 30% Mica Reinforced Polypropylene, Black Applications: Fan shroudsHVAC ductworkClose-out panelsFiller panelsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
RheTech Products P100-00 Polypropylene, Natural Applications: Automotive componentsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
RheTech Products P107-00 Polypropylene Homopolymer, Natural Applications: Wire harnessesTrim componentsUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
RheTech Products P250-247 Polypropylene Copolymer, UV Stabilized, Black Applications: Center consolesInterior trimI/P componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
RheTech Products P252-674UV Polypropylene Copolymer, UV Stabilized, 447B Fawn Applications: Interior trimElectrical housingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
RheTech Products P254-01 Polypropylene Copolymer, Black Applications: Air ducts - distributionFuse panel coversSplash shieldsElectrical housingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
RheTech Products P258-01 Polypropylene Copolymer, UV Stabilized, Black Applications: Door/trunk scuffExterior grills and cowlsSteering column shroudsInterior trimInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
RheTech Products T10P100-01 10% Talc Reinforced Polypropylene, Black Applications: Consumer goodsAir ductsUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
RheTech Products T20P100-517UV 20% Talc Reinforced Polypropylene, UV Stabilized, Interior DX9 Black Applications: Center consolesIP componentsClose out panelsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
RheTech Products T20P200-01BG 20% Talc Reinforced Polypropylene Copolymer, General Purpose Black, Blow Molding Grade Applications: HVAC ductsSeat backsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
RheTech Products T40P250-00 40% Talc Reinforced Polypropylene Copolymer, Natural Applications: BracketsHousingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
RheTech Products G30P100-00 30% Glass Fiber Reinforced Polypropylene, Natural Applications: Fender apronsUnderhood componentsStructural componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
RheTech Products GC20P255-01 20% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Black Applications: BracketsUnderhood componentsElectrical housingsHeadlamp bracketsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
RheTech Products GC20P255-712UV 20% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, UV Stabilized, B231 Earth Grey Applications: Consumer goodsMiscellaneous bracketsExterior componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
RheTech Products HP507-01 38% Talc Reinforced High Performance Polypropylene, Non-UV Stabilized, Black Applications: IP structural componentsSpeaker housingsAutomotive interior componentsInjection molding conditions reported in table.Information provided by RheTech Products. |