Material Notes:
Description: Polyamide 66, reinforced with 13% of glass fiber, heat stabilized, with improved impact resistance, for injection molding.Available in: Europe, Latin America and North AmericaProduct Applications: In addition to primary polyamide properties, TECHNYL ® A 238 V13 offers a very good rigidity/impact resistance compromise, at high temperatures. This grade is used for under bonnet automotive parts, such as: various covers and fasteners. This product is available in natural.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 60.0 MPa
8700 psi
ISO 527 type 1 A
Elongation at Yield 8.0 %
8.0 %
ISO 527 type 1 A
Tensile Modulus 36.5 GPa
5290 ksi
ISO 527 Type 1A
Izod Impact, Notched (ISO) 10.0 kJ/m²
4.76 ft-lb/in²
ISO 180/1eA
Charpy Impact Unnotched 6.00 J/cm²
28.6 ft-lb/in²
ISO 179/1eU
Charpy Impact, Notched 0.800 J/cm²
3.81 ft-lb/in²
ISO 179/1eA
Processing Properties Metric English Comments
Moisture Content <= 0.20 %
<= 0.20 %