Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Dry Time = 2 hour Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Dry Time 1 - 2 hour
1 - 2 hour
RheTech Products FT1002-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural
Applications: Step padsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products.
Dry Time 1 - 2 hour
1 - 2 hour
RheTech Products FT1002-00A Thermoplastic Polyolefin, Non-UV Stabilized, Natural
Applications: Step padsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products.
Dry Time 1 - 2 hour
1 - 2 hour
RheTech Products FT1055-685UV Thermoplastic Polyolefin, UV Stabilized, Graphite
Applications: Bumper coversInterior trimSplash shieldsInjection molding conditions reported in table.Information provided by RheTech Products.
Dry Time 1 - 2 hour
1 - 2 hour
RheTech Products FT2202-732UV Thermoplastic Polyolefin, UV Stabilized, YGYA Black
Applications: Box top railTail gate linerExterior trimInjection molding conditions reported in table.Information provided by RheTech Products.
Dry Time 1 - 2 hour
1 - 2 hour
RheTech Products FT2400-647UV Thermoplastic Polyolefin, UV Stabilized, 8798NM Grey
Applications: Bumper rub stripsHitch padsScuff padsInjection molding conditions reported in table.Information provided by RheTech Products.
Dry Time 1 - 2 hour
1 - 2 hour
RheTech Products FT4600-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural
Applications: Scuff platesInterior trimI/P componentsInjection molding conditions reported in table.Information provided by RheTech Products.
Dry Time 1 - 2 hour
1 - 2 hour
RheTech Products FT4802-690UV Thermoplastic Polyolefin, UV Stabilized, HS5 Medium Dark Neutral
Applications: Bodyside moldings and claddingsFacia and bumper coversExterior componentsInjection molding conditions reported in table.Information provided by RheTech Products.
Dry Time 1 - 2 hour
1 - 2 hour
RheTech Products FT4802-690UVA Thermoplastic Polyolefin, UV Stabilized, HS5 Medium Dark Neutral
Applications: Bodyside moldings and claddingsFacia and bumper coversExterior componentsInjection molding conditions reported in table.Information provided by RheTech Products.
Dry Time 1 - 2 hour
1 - 2 hour
RheTech Products FT4900-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural
Applications: Exterior componentsBodyside moldingsStep padsInjection molding conditions reported in table.Information provided by RheTech Products.
Dry Time 1 - 2 hour
1 - 2 hour
RheTech Products FT4900-74UV Thermoplastic Polyolefin, UV Stabilized, Exterior DX9 Black
Applications: Exterior componentsBodyside moldingsStep padsInjection molding conditions reported in table.Information provided by RheTech Products.
Dry Time 1 - 2 hour
1 - 2 hour
RheTech Products FT7013-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural
Applications: Scuff platesLift gate coversI/P componentsClose-out panelsInjection molding conditions reported in table.Information provided by RheTech Products.
Dry Time 1 - 2 hour
1 - 2 hour
RheTech Products FT7016-01UV Thermoplastic Polyolefin, UV Stabilized, Black
Applications: Bumper coversCladdingsInjection molding conditions reported in table.Information provided by RheTech Products.
Dry Time 1 - 2 hour
1 - 2 hour
RheTech Products G13P100-347UV 13% Glass Fiber Reinforced Polypropylene, UV Stabilized, 109D Medium Pewter
Applications: Dome lamp housingsFuel filler pocketInjection molding conditions reported in table.Information provided by RheTech Products.
Dry Time 1 - 2 hour
1 - 2 hour
RheTech Products G20P100-599 20% Glass Fiber Reinforced Polypropylene, UV Stabilized, (Ford BJ4A) Medium Dark Parchment
Applications: Arm rest insertVacuum canister insertStorage binConsolesBattery traysInjection molding conditions reported in table.Information provided by RheTech Products.
Dry Time 1 - 2 hour
1 - 2 hour
RheTech Products GC10P200-01 10% Glass Fiber Reinforced Polypropylene Copolymer, Non-UV Stabilized, Chemically Coupled, Black
Applications: HousingsStorage binsBracketsInjection molding conditions reported in table.Information provided by RheTech Products.
Dry Time 1 - 2 hour
1 - 2 hour
RheTech Products GC43P250-777 43% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Ivory
Applications: BracketsStructural supportsDurable GoodsInjection molding conditions reported in table.Information provided by RheTech Products.
Dry Time 1 - 2 hour
1 - 2 hour
RheTech Products HP514-01 14% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, Black
Applications: Glove box binInterior trimSteering column trimConsolesAir ducts - distributionInjection molding conditions reported in table.Information provided by RheTech Products.
Dry Time 1 - 2 hour
1 - 2 hour
RheTech Products HP514-393 14% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 110D Medium Dark Pewter
Applications: Glove box binInterior trimSteering column trimConsolesAir ducts - distributionInjection molding conditions reported in table.Information provided by RheTech Products.
Dry Time 1 - 2 hour
1 - 2 hour
RheTech Products HP517-00 23% Talc Reinforced High Performance Polypropylene Copolymer, Non-UV Stabilized, Natural
Applications: Interior trim moldingsSill platesTire coverInjection molding conditions reported in table.Information provided by RheTech Products.
Dry Time 1 - 2 hour
1 - 2 hour
RheTech Products HP519-01 26% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, Black
Applications: Interior trim moldingsSill platesAir ductsInjection molding conditions reported in table.Information provided by RheTech Products.
Dry Time 1 - 2 hour
1 - 2 hour
RheTech Products HP520-01 12% Talc Reinforced High Performance Polypropylene Copolymer, Non-UV Stabilized, Black
Applications: Interior trimCenter consolesGlove box binsInjection molding conditions reported in table.Information provided by RheTech Products.
Dry Time 1 - 2 hour
1 - 2 hour
RheTech Products HP521-229 15% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 195A Medium Neutral
Applications: Interior trimIP structural componentsScuff/kick platesInjection molding conditions reported in table.Information provided by RheTech Products.
Dry Time 1 - 2 hour
1 - 2 hour
RheTech Products T20P100-01UV 20% Talc Reinforced Polypropylene, UV Stabilized, General Purpose Black
Applications: Durable goodsElectronics housingsIP componentsClose out panelsInjection molding conditions reported in table.Information provided by RheTech Products.
Dry Time 1 - 2 hour
1 - 2 hour
RheTech Products T20P250-01UV 20% Talc Reinforced Polypropylene Copolymer, UV Stabilized, Black
Applications: Interior componentsI/P componentsInterior trimDurable goodsInjection molding conditions reported in table.Information provided by RheTech Products.
Dry Time 1 - 2 hour
1 - 2 hour
RheTech Products T30P200-01BG 30% Talc Reinforced Polypropylene Copolymer, Black, Blow Molding Grade
Applications: HVAC ductsSeat backsFlipper panelsInjection molding conditions reported in table.Information provided by RheTech Products.
Dry Time 1 - 2 hour
1 - 2 hour
in desiccant air dryer
Polykemi AB POLYelast TPE Z650A Thermoplastic Elastomer, SEBS-based, Co-injection Grade
Information provided by Polykemi AB
Dry Time 1 - 2 hour
1 - 2 hour
Tackfree, less if accelerated
Abatron TDS, AboThane 861019/8606-5 Acrylic/Polyurethane Enamel  (discontinued **)
Acrylic/polyurethane highest-grade glossy colored enamel for metal, plastics, concrete, wood, floors and structures indoor and outdoor. Rule 66 exempt. 2-component system for superior performance ..
Dry Time 1 - 2 hour
1 - 2 hour
BASF UltramidĀ® 1503-2F BK ND 3007 33% Glass Filled PA 66 (Dry)
Description: Ultramid 1503-2F BK ND3007 is a 33% glass reinforced, heat stabilized injection molding PA6/6 grade. It is designed to provide enhance hydroysis resistance for under-the-hood applicatio..
Dry Time 1 - 2 hour
1 - 2 hour
RheTech Products M20P101-01 20% Mica Reinforced Polypropylene, Black
Applications: Radiator air bafflesHVAC ductworkClose-out and filler panelsInjection molding conditions reported in table.Information provided by RheTech Products.
Dry Time 1 - 2 hour
1 - 2 hour
RheTech Products GC43P250-01 43% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Black
Applications: Consumer goodsFunctional supportsHead lamp bracketsDurable GoodsInjection molding conditions reported in table.Information provided by RheTech Products.