Processing Properties | Metric | English | Comments |
---|---|---|---|
Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
RheTech Products E204-01 High Density Polyethylene, Black Applications: Electrical housingsUnderhood componentsConsumer GoodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
RheTech Products F38-01 35% Glass Fiber/Mineral Co-Reinforced Polypropylene, Chemically Coupled, Black Applications: Electrical housingsBracketsBattery traysInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
RheTech Products FT1001-177UV Thermoplastic Polyolefin, Non-UV Stabilized, HS5 Medium Dark Neutral Applications: Scuff platesBodyside moldingsStep and hitch padsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
RheTech Products FT1004-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural Applications: Step padsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
RheTech Products FT2400-647UV Thermoplastic Polyolefin, UV Stabilized, 8798NM Grey Applications: Bumper rub stripsHitch padsScuff padsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
RheTech Products FT7016-50UV Thermoplastic Polyolefin, UV Stabilized, YGYA Black Applications: Bumper coversCladdingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
RheTech Products G13P100-332UV 13% Glass Fiber Reinforced Polypropylene, UV Stabilized, (GM 9772) Light Neutral Applications: Interior trimAir ducts - distributionFuel filler pocketInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
RheTech Products G13P100-559UV 13% Glass Fiber Reinforced Polypropylene, UV Stabilized, (GM WPP 646H) Charcoal Metallic Applications: Interior trimAir ducts - distributionFuel filler pocketInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
RheTech Products G30P100-01 30% Glass Fiber Reinforced Polypropylene, Black Applications: Fender apronsUnderhood componentsStructural componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
RheTech Products GC20P100-00 15% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Natural Applications: Air Ducts - distributionBracketsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
RheTech Products GC30P100-01UV 30% Glass Fiber Reinforced Polypropylene, Chemically Coupled, UV Stabilized, Black Applications: Exterior automotive componentsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
RheTech Products HP513-00 High Performance Polypropylene Copolymer, Non-UV Stabilized, Natural Applications: Interior trimI/P componentsCenter consolesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
RheTech Products HP514-489 14% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 101E Lite Oak Applications: Glove box binInterior trimSteering column trimConsolesAir ducts - distributionInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
RheTech Products HP519-00 26% Talc Reinforced High Performance Polypropylene Copolymer, Non-UV Stabilized, Natural Applications: Interior trim moldingsSill platesAir ductsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
RheTech Products HP521-00 15% Talc Reinforced High Performance Polypropylene Copolymer, Non-UV Stabilized, Natural Applications: Interior trimIP structural componentsCenter consolesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
RheTech Products HP521-372 15% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 110D Medium Dark Pewter Applications: Interior trimIP structural componentsCenter consolesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
RheTech Products M25UVP250-01 25% Mica Reinforced Polypropylene Copolymer, UV Stabilized, Black Applications: BracketsCowl screensRigid exterior componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
RheTech Products P100-01 Polypropylene Homopolymer, Black Applications: Wire harnessesTrim componentsUnderhood applicationsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
RheTech Products P256-674UV Polypropylene Copolymer, UV Stabilized, 447B Fawn Applications: Interior trimElectrical housingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
RheTech Products P257-01 Polypropylene Copolymer, Black Applications: Splash shield and fender linersElectrical enclosuresUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
RheTech Products T12P600-430UVBG 12% Talc Reinforced Polypropylene Copolymer, UV Stabilized, Interior 848 Black, Blow Molding Grade Applications: Flipper panelsSeat backsLoad floorInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
RheTech Products T20P252-00 20% Talc Reinforced Polypropylene, Natural Applications: IP Structural componentsGlove box binWire troughInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
RheTech Products T40P106-01 40% Talc Reinforced Polypropylene, Black Applications: Underhood componentsHVAC ductworkFunctional supportsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
RheTech Products T40P108-01A 40% Talc Reinforced Polypropylene, Black Applications: Underhood componentsHVAC ductworkFunctional supportsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
RheTech Products T40P200-01 40% Talc Reinforced Polypropylene Copolymer, Black Applications: BracketsHousingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
RheTech Products HP505-01 23% Talc Reinforced High Performance Polypropylene Copolymer, Non-UV Stabilized, Black Applications: Glove box binConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
RheTech Products HP506-01A 21% Talc Reinforced High Performance Polypropylene, UV Stabilized, Black Applications: Automotive interior applicationsHVAC ductsTail lamp housingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
RheTech Products HP514-00UV 14% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, Natural Applications: Glove box binInterior trimSteering column trimConsolesAir ducts - distributionInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
RheTech Products CC30P100-00 30% Calcium Carbonate Reinforced Polypropylene, Natural Applications: Consumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Injection Pressure | 2.76 - 10.3 MPa | 400 - 1500 psi | |
RheTech Products GC15P200-01 15% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Black Applications: Electrical housingsUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products. |