Processing Properties | Metric | English | Comments |
---|---|---|---|
Middle Barrel Temperature | 204 - 260 °C | 400 - 500 °F | |
Multibase Multi-Pro® 1004 R Polypropylene Features: Scratch Resistance, GoodHeat Resistance, HighStiffness, GoodForms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Middle Barrel Temperature | 204 - 232 °C | 400 - 450 °F | |
Multibase Multi-Pro® 1008 T Polypropylene Talc Filler, 10% by weight.Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Middle Barrel Temperature | 204 - 232 °C | 400 - 450 °F | |
Multibase Multi-Pro® 4009 T Polypropylene Talc Filled, 40% by weight.Forms:PelletsProcessing Methods:Injection MoldingUses: Lawn and Garden EquipmentTable ProductsFurnitureInformation provided by Multibase |
|||
Middle Barrel Temperature | 204 - 232 °C | 400 - 450 °F | |
Multibase Multi-Pro® 4015 THW Polypropylene Talc Filled, 40% by weight.Forms:PelletsProcessing Methods:Injection MoldingUses: Lawn and Garden EquipmentTable ProductsFurnitureInformation provided by Multibase |
|||
Middle Barrel Temperature | 204 - 232 °C | 400 - 450 °F | |
RheTech Products F22-01 20% Glass Fiber/Mineral Co-Reinforced Polypropylene, Black Applications: Support ductsHousingsBattery traysInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 204 - 232 °C | 400 - 450 °F | |
RheTech Products F52-01 20% Mica Reinforced Polypropylene Copolymer, Black Applications: Functional support ductsHousingsUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 204 - 232 °C | 400 - 450 °F | |
RheTech Products FT4650-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural Applications: Scuff platesExterior grillesBodyside moldingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 204 - 232 °C | 400 - 450 °F | |
RheTech Products FT4702-527UV Thermoplastic Polyolefin, UV Stabilized, XS9 Dark Neutral Metallic Applications: Exterior door moldingsRigid bumper coversBodyside claddings and fairingsAutomotive grillesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 204 - 232 °C | 400 - 450 °F | |
RheTech Products FT4702-698UV Thermoplastic Polyolefin, UV Stabilized, RXF Jet Black Applications: Bumper trimExterior componentsDoor claddingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 204 - 232 °C | 400 - 450 °F | |
RheTech Products FT5100-04 Thermoplastic Polyolefin, UV Stabilized, White Applications: IP structural componentBody side moldingInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 204 - 232 °C | 400 - 450 °F | |
RheTech Products G20P100-00 20% Glass Fiber Reinforced Polypropylene, Natural Applications: Arm rest insertVacuum canisterStorage binConsolesBattery traysInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 204 - 232 °C | 400 - 450 °F | |
RheTech Products HP800-706UV 20% Talc Reinforced High Performance Polypropylene Copolymer, Scratch Resistant, UV Stabilized, Impact Modified, SWB White Applications: Interior trim/Instrument panel componentsA/B pillarsGlove box doorsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 204 - 232 °C | 400 - 450 °F | |
RheTech Products T20P104-01 20% Talc Reinforced Polypropylene, Black Applications: Electronic housingsIP componentsHVAC ducts - air distributionClose out panelDurable goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 204 - 232 °C | 400 - 450 °F | |
RheTech Products T20P200-01BG 20% Talc Reinforced Polypropylene Copolymer, General Purpose Black, Blow Molding Grade Applications: HVAC ductsSeat backsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 204 - 216 °C | 400 - 420 °F | |
PlastiComp Complet® LCF30 - PP Homopolymer Polypropylene, 30% Long Carbon Fiber Reinforced Complet® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polypropylene with 30% carbon fiber reinforcementInformation provided by PlastiComp, Inc. |
|||
Middle Barrel Temperature | 204 - 216 °C | 400 - 420 °F | |
PlastiComp Complet® LGF60 - PP Homopolymer Polypropylene, 60% Long Glass Fiber Reinforced Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polypropylene with 60% long glass fiber reinforcementInformation provided by PlastiCom.. |
|||
Middle Barrel Temperature | 204 - 227 °C | 400 - 440 °F | |
Polymer Resources ABS-GP1-[color]-EP General Purpose ABS, Electroplating Grade General Purpose Acrylonitrile Butadiene Styrene, Electroplating GradeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sam.. |
|||
Middle Barrel Temperature | 204 - 221 °C | 400 - 430 °F | |
Ravago Manufacturing Americas Hylac® GP74G20 ABS, 20% Glass Fiber Reinforced Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Middle Barrel Temperature | 204 - 232 °C | 400 - 450 °F | |
RheTech Products M25P100-01 25% Mica Reinforced Polypropylene, Black Applications: Underhood applicationsInternal I/P ComponentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 204 - 232 °C | 400 - 450 °F | |
RheTech Products M25P251-01 25% Mica Reinforced Polypropylene Copolymer, Black Applications: Fan shroudsGlove box binFiller panelsClose-out panelsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 204 - 227 °C | 400 - 440 °F | |
Fiberfil® J-60/15/E Polypropylene Homopolymer, 15% Glass Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Middle Barrel Temperature | 204 - 227 °C | 400 - 440 °F | |
Fiberfil® J-60/20/FR Polypropylene Homopolymer, 20% Glass Reinforced, Flame Retardant Information provided by FIBERFIL Engineered Plastics |
|||
Middle Barrel Temperature | 204 - 227 °C | 400 - 440 °F | |
Fiberfil® PP-60/CC/20 Polypropylene Homopolymer, 20% Calcium Carbonate Information provided by FIBERFIL Engineered Plastics |
|||
Middle Barrel Temperature | 204 - 232 °C | 400 - 450 °F | |
Star Plastics ABS448T Molding Grade ABS Information provided by Star Plastics, Inc. |
|||
Middle Barrel Temperature | 204 °C | 400 °F | |
TPI Porene® ABS-AN450 Flame Retardant ABS Resin Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Middle Barrel Temperature | 204 - 227 °C | 400 - 440 °F | |
LTL Color Compounds ColorFast® GPA300X ABS Extrusion grade, high impact, high gloss ABSAll information provided by LTL Color Compounders, Inc. |
|||
Middle Barrel Temperature | 204 - 232 °C | 400 - 450 °F | |
RheTech Products GC20P105-08FA 20% Glass Fiber Reinforced Polypropylene, Chemically Coupled, FDA Compliant, Black Applications: Water system housingFDA approved partsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 204 - 232 °C | 400 - 450 °F | |
RheTech Products GC20P255-712UV 20% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, UV Stabilized, B231 Earth Grey Applications: Consumer goodsMiscellaneous bracketsExterior componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 204 - 232 °C | 400 - 450 °F | |
RheTech Products HP506-01B 22% Talc Reinforced High Performance Polypropylene, UV Stabilized, Black Applications: Underhood componentsLamp housingsHVAC ductsInjection molding conditions reported in table.Information provided by RheTech Products. |