Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 9.0 - 16 g/10 min @Load 1.20 kg, Temperature 300 °C |
9.0 - 16 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
Polymer Resources PC-FR2A-D Polycarbonate, Flame Retardant, Medium Flow Polycarbonate, Flame Retardant, Medium FlowFeatures: • High Impact Resistance • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-i.. |
|||
Melt Flow | 9.0 g/10 min @Load 1.20 kg, Temperature 300 °C |
9.0 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® ML7667 PC Copolymer (Asia Pacific) Lexan* ML7667 specialty polycarbonate (PC) resin is a 9% GF reinforced, UV stabilized, flame retarded injection molding grade. This medium flow specialty PC resin combines UL94 V0 @ 1.5mm, 5VB @ 3.. |
|||
Melt Flow | 9.0 g/10 min @Load 1.20 kg, Temperature 300 °C |
9.0 g/10 min @Load 2.65 lb, Temperature 572 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Lexan® FXD164R PC (Europe-Africa-Middle East) Transparent/translucent medium viscosity PC for light diffusion special effects, FDA compliant and mold release containing. The color package may affect performance.This data was supplied by SABIC-I.. |
|||
Melt Flow | 9.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
9.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
LG Chemical LUCEL HI515W POM+Rubber, High Impact Feature: Injection Molding, POM+Rubber, High ImpactApplication: Gears, Automobile ClipCAS No. 66455-31-0 and 155123-66-3Information provided by LG Chemical |
|||
Melt Flow | 9.0 g/10 min @Load 1.20 kg, Temperature 300 °C |
9.0 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
Kotec Carbotex K-50UV Polycarbonate, General Purpose, UV Stability Grade Features: UV stability, Medium viscosity, TransparentApplications: OA equipment, Communications, Precision parts, Machineries, Lighting fixtures, Safety products, E & E parts, Household applications.. |
|||
Melt Flow | 9.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
9.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Lucobit Lucolit® 1321 Polyolefin TPO Granules, Blue Lucolit is a colored, highly stabilized, bitumen-free TPO raw material based on polyolefins. Lucolit products display excellent tear resistance, flexibility, and weathering resistance. Lucolit exhi.. |
|||
Melt Flow | 9.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
9.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Lucobit Lucolit® 1322 Polyolefin TPO Granules, Red Lucolit is a colored, highly stabilized, bitumen-free TPO raw material based on polyolefins. Lucolit products display excellent tear resistance, flexibility, and weathering resistance. Lucolit exhi.. |
|||
Melt Flow | 9.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
9.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Lucobit Lucolit® 1323 Polyolefin TPO Granules, Green Lucolit is a colored, highly stabilized, bitumen-free TPO raw material based on polyolefins. Lucolit products display excellent tear resistance, flexibility, and weathering resistance. Lucolit exhi.. |
|||
Melt Flow | 9.0 g/10 min | 9.0 g/10 min | (Condition L) ASTM D-1238 |
Multibase Multi-Flex® TPE A 5009 Multi-Flex TPE contains Kraton™ G.Data provided by Multibase. |
|||
Melt Flow | 9.0 g/10 min | 9.0 g/10 min | 230/2.16 (typical); ASTM D1238 |
Fiberfil® J-60/20/E8/M Polypropylene Homopolymer, 20% Glass Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Melt Flow | 9.0 g/10 min @Load 5.00 kg, Temperature 200 °C |
9.0 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
LG Chemical 40 AF Flame Retardant HIPS High impact, Safety standards: listed with UL CSA, and classified according to IEC 707, Meet requirements for flammability, mechanical and electrical properties, Applications include televisions, VT.. |
|||
Melt Flow | 9.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
9.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
LyondellBasell Hifaxâ„¢ CA45 Thermoplastic Olefin Resin Key Features: medium melt flow, medium modulus thermoplastic elastomeric olefin resin, excellent balance of properties, excellent processability, good colorability, excellent surface appearanceAppli.. |
|||
Melt Flow | 9.0 g/10 min @Load 6.60 kg, Temperature 337 °C |
9.0 g/10 min @Load 14.6 lb, Temperature 639 °F |
ASTM D1238 |
SABIC Innovative Plastics ULTEM HU1000 PEI Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI).. |
|||
Melt Flow | 9.0 g/10 min @Load 5.00 kg, Temperature 300 °C |
9.0 g/10 min @Load 11.0 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics NORYL GFN2 PPE+PS PPE+PS blend. 20% Glass reinforced. UL746C F1. NSF 61 listing in several colors (restrictions apply). FDA compliance (restrictions apply). Low water absorption. Hydrolytic stability. Dimensional sta.. |
|||
Melt Flow | 9.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
9.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
A. Schulman POLYBATCH™ White 8350 AP Concentrate Based In LDPE DescriptionPOLYBATCH® 8350 AP is an advanced performance white color concentrate containing 50% TiO2 based in LDPE. This product has been specifically engineered to provide improved resistance to .. |
|||
Melt Flow | 9.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
9.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Polyram RamOfin PPH302G4 Polypropylene, 20% Glass Fiber 20% glass fiber reinforced polypropylene for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Melt Flow | 9.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
9.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Polyram RamTal PM1509 Acetal, Low Friction Polyacetal copolymer for decreased friction and improved wear resistance for injection molding applications.Information provided by Polyram Ram On Ind. |
|||
Melt Flow | 9.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
9.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Polyram RamTal PM8427 Acetal, Impact modified Impact modified polyacetal for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Melt Flow | 9.0 g/10 min @Load 1.20 kg, Temperature 300 °C |
9.0 g/10 min @Load 2.65 lb, Temperature 572 °F |
ISO 1133 |
Polyram RamTough PZ307G4 Polycarbonate, 20% Glass Fiber, UV Stabilized 20% glass fiber reinforced polycarbonate, UV stabilized, for injection molding applications.Information provided by Polyram. |
|||
Melt Flow | 9.0 g/10 min @Temperature 230 °C |
9.0 g/10 min @Temperature 446 °F |
ASTM D1238 |
Total PPH 3571 Polypropylene, Film Extrusion Grade Homopolymer film gradeLow Residuals - Fina 3571 utilizes the new Fina proprietary process technology to provide extremely low residuals for improved color stability and clarity.Slip/Antiblock - Fina.. |
|||
Melt Flow | 9.0 g/10 min | 9.0 g/10 min | |
Zylog Hipolyene® 1532 HC EX Thermoplastic Polyolefin & PP Compound Information provided by Zylog Plastalloys Pvt. Ltd. |
|||
Melt Flow | 9.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
9.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
GB/T 3682 |
Chengdu Polyster KP-200-50 Silicone Masterbatch KP-200 series silicone masterbatches are white pellets or white powder which made from ultra-high molecular weight polysiloxane, used by plastics as processing aids and impart expected silicone bene.. |
|||
Melt Flow | 9.0 - 10 g/10 min @Load 2.16 kg, Temperature 230 °C |
9.0 - 10 g/10 min @Load 4.76 lb, Temperature 446 °F |
|
Breplast Bretene PP Polypropylene Composite Recovered polypropylene compositeInformation provided by Breplast S.p.A. |
|||
Melt Flow | 9.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
9.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Azoty Tarnow™ TARNOFORM 300 LS POM Injection molding grade based on Tarnoform 300 modified with soluble light stabilizers improving weathering stability.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Melt Flow | 9.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
9.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Barlog Plastics KEBAFORM C 901 FA POM Copolymer unreinforced, reduced formaldehyde emission POMInformation provided by BARLOG plastics GmbH. |
|||
Melt Flow | 9.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
9.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Barlog Plastics KEBAFORM C 903 LF POM Copolymer unreinforced, improved wear and friction POMInformation provided by BARLOG plastics GmbH. |
|||
Melt Flow | 9.0 g/10 min | 9.0 g/10 min | |
Custom Resins Duratel™ MF9 Acetal Copolymer
(discontinued **) Description: Duratel™ MF9 is a 9 melt flow, general purpose acetal copolymer. Information provided by Custom Resins. |
|||
Melt Flow | 9.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
9.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Azoty Tarnow™ TARNOFORM 300 GB2 POM 10% glass beads filled grade with increased stiffness and hardness with lowered shrinkageInformation provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Melt Flow | 9.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
9.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Polyram RamOfin PPC350M6 Polypropylene, 30% Mineral Filled 30% Mineral filled, heat stabilized polypropylene for injection molding applications.Information provided by Polyram. |