Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Rear Barrel Temperature = 390 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Rear Barrel Temperature 199 - 260 °C
390 - 500 °F
Multibase Multi-Pro® 2005 RCI Polypropylene
Glass Fiber Reinforced, 20% by weight.Features:Heat Resistance, HighScratch ResistantStiffness, GoodForms:PelletsProcessing Methods:Injection MoldingUses:Automotive ApplicationsInformation provided ..
Rear Barrel Temperature 199 - 260 °C
390 - 500 °F
Multibase Multi-Pro® 3012 RC Polypropylene
Glass Fiber Reinforced, 30% by weight.Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase
Rear Barrel Temperature 199 - 227 °C
390 - 440 °F
RheTech Products CC20P200-00 20% Calcium Carbonate Reinforced Polypropylene Copolymer, Natural
Applications: Electrical housingsDurable goodsInjection molding conditions reported in table.Information provided by RheTech Products.
Rear Barrel Temperature 199 - 227 °C
390 - 440 °F
RheTech Products FT4650-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural
Applications: Scuff platesExterior grillesBodyside moldingsInjection molding conditions reported in table.Information provided by RheTech Products.
Rear Barrel Temperature 199 - 227 °C
390 - 440 °F
RheTech Products FT4650-01UV Thermoplastic Polyolefin, Non-UV Stabilized, Black
Applications: Scuff platesExterior grillesBodyside moldingsInjection molding conditions reported in table.Information provided by RheTech Products.
Rear Barrel Temperature 199 - 227 °C
390 - 440 °F
RheTech Products FT4702-527UV Thermoplastic Polyolefin, UV Stabilized, XS9 Dark Neutral Metallic
Applications: Exterior door moldingsRigid bumper coversBodyside claddings and fairingsAutomotive grillesInjection molding conditions reported in table.Information provided by RheTech Products.
Rear Barrel Temperature 199 - 227 °C
390 - 440 °F
RheTech Products FT4702-715UV Thermoplastic Polyolefin, UV Stabilized, ZSP Deep Grey
Applications: Exterior componentsGrillesBumper trimDoor componentsInjection molding conditions reported in table.Information provided by RheTech Products.
Rear Barrel Temperature 199 - 227 °C
390 - 440 °F
RheTech Products FT4802-691UV Thermoplastic Polyolefin, UV Stabilized, RJ3 Dark Grey Green
Applications: Bodyside moldings and claddingsFacia and bumper coversExterior componentsInjection molding conditions reported in table.Information provided by RheTech Products.
Rear Barrel Temperature 199 - 227 °C
390 - 440 °F
RheTech Products FT7011-01 Thermoplastic Polyolefin, Non-UV Stabilized, Black
Applications: Claddings and faciasExterior componentsInjection molding conditions reported in table.Information provided by RheTech Products.
Rear Barrel Temperature 199 - 227 °C
390 - 440 °F
RheTech Products GC20P100-177UV 20% Glass Fiber Reinforced Polypropylene, Chemically Coupled, UV Stabilized, (Chrysler HS5) Gray
Applications: Air Ducts - distributionBracketsInjection molding conditions reported in table.Information provided by RheTech Products.
Rear Barrel Temperature 199 - 227 °C
390 - 440 °F
RheTech Products HP517-00 23% Talc Reinforced High Performance Polypropylene Copolymer, Non-UV Stabilized, Natural
Applications: Interior trim moldingsSill platesTire coverInjection molding conditions reported in table.Information provided by RheTech Products.
Rear Barrel Temperature 199 - 227 °C
390 - 440 °F
RheTech Products HP531-00 22% Talc Reinforced High Performance Polypropylene Copolymer, Non-UV Stabilized, Natural
Applications: IP structural componentsAir ducts - distributionA/B/C/ PillarsInjection molding conditions reported in table.Information provided by RheTech Products.
Rear Barrel Temperature 199 - 227 °C
390 - 440 °F
RheTech Products HP532-01 20% Talc Reinforced High Performance Polypropylene, Non-UV Stabilized, Black
Applications: Close out panelSpeaker grilleInjection molding conditions reported in table.Information provided by RheTech Products.
Rear Barrel Temperature 199 - 227 °C
390 - 440 °F
RheTech Products T12P600-430UVBG 12% Talc Reinforced Polypropylene Copolymer, UV Stabilized, Interior 848 Black, Blow Molding Grade
Applications: Flipper panelsSeat backsLoad floorInjection molding conditions reported in table.Information provided by RheTech Products.
Rear Barrel Temperature 199 - 227 °C
390 - 440 °F
RheTech Products T20P104-01 20% Talc Reinforced Polypropylene, Black
Applications: Electronic housingsIP componentsHVAC ducts - air distributionClose out panelDurable goodsInjection molding conditions reported in table.Information provided by RheTech Products.
Rear Barrel Temperature 199 - 227 °C
390 - 440 °F
RheTech Products T20P252-01 20% Talc Reinforced Polypropylene Copolymer, Black
Applications: IP Structural componentsGlove box binWire troughInjection molding conditions reported in table.Information provided by RheTech Products.
Rear Barrel Temperature 199 - 210 °C
390 - 410 °F
PlastiComp Complet® LCF40 - PP Homopolymer Polypropylene, 40% Long Carbon Fiber Reinforced
Complet® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polypropylene with 40% carbon fiber reinforcementInformation provided by PlastiComp, Inc.
Rear Barrel Temperature 199 - 210 °C
390 - 410 °F
PlastiComp Complet® LCF50 - PP Homopolymer Polypropylene, 50% Long Carbon Fiber Reinforced
Complet® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polypropylene with 50% carbon fiber reinforcementInformation provided by PlastiComp, Inc.
Rear Barrel Temperature 199 - 210 °C
390 - 410 °F
PlastiComp Complet® LGF40 - PP Homopolymer Polypropylene, 40% Long Glass Fiber Reinforced
Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polypropylene with 40% long glass fiber reinforcementInformation provided by PlastiCom..
Rear Barrel Temperature 199 - 227 °C
390 - 440 °F
RheTech Products M25P251-01 25% Mica Reinforced Polypropylene Copolymer, Black
Applications: Fan shroudsGlove box binFiller panelsClose-out panelsInjection molding conditions reported in table.Information provided by RheTech Products.
Rear Barrel Temperature 199 - 210 °C
390 - 410 °F
Fiberfil® J-60/20/E Polypropylene Homopolymer, 20% Glass Reinforced, Chemically coupled
Information provided by FIBERFIL Engineered Plastics
Rear Barrel Temperature 199 - 210 °C
390 - 410 °F
Fiberfil® J-60/30 Polypropylene Homopolymer, 30% Glass Reinforced
Information provided by FIBERFIL Engineered Plastics
Rear Barrel Temperature 199 - 210 °C
390 - 410 °F
Fiberfil® J-60/30/FR Polypropylene Homopolymer, 30% Glass Fiber Reinforced, Flame Retardant
Information provided by FIBERFIL Engineered Plastics
Rear Barrel Temperature 199 - 210 °C
390 - 410 °F
Fiberfil® M-1492 BK223 Polypropylene Homopolymer, Glass Reinforced, mica Filled, Chemically coupled
Information provided by FIBERFIL Engineered Plastics
Rear Barrel Temperature 199 - 210 °C
390 - 410 °F
Fiberfil® J-62/30/E8 Polypropylene Copolymer, 30% Glass Fiber Reinforced, Chemically coupled
Information provided by FIBERFIL Engineered Plastics
Rear Barrel Temperature 199 - 216 °C
390 - 420 °F
Teknor Apex Telcar® TL-8431 Thermoplastic Elastomer
Notes: RoHS Compliant Uses: Appliance Wire Insulation; Appliance Wire Jacketing; Cable Jacketing; Connectors; Flexible Cord Jacketing; Electrical/Electronic Applications; Industrial Cable Jacketing;..
Rear Barrel Temperature 199 - 227 °C
390 - 440 °F
RheTech Products M20P101-01 20% Mica Reinforced Polypropylene, Black
Applications: Radiator air bafflesHVAC ductworkClose-out and filler panelsInjection molding conditions reported in table.Information provided by RheTech Products.
Rear Barrel Temperature 199 - 210 °C
390 - 410 °F
Fiberfil® J-68/30/E/UV Polypropylene Copolymer, 30% Glass Fiber Reinforced, Chemically coupled, UV Stabilized
Information provided by FIBERFIL Engineered Plastics
Rear Barrel Temperature 199 - 227 °C
390 - 440 °F
RheTech Products GC20P600-01UV 20% Glass Fiber Reinforced Polypropylene, Chemically Coupled, UV Stabilized, Black
Applications: Sun roof trimFan shroudInjection molding conditions reported in table.Information provided by RheTech Products.
Rear Barrel Temperature 199 - 227 °C
390 - 440 °F
RheTech Products HP506-01B 22% Talc Reinforced High Performance Polypropylene, UV Stabilized, Black
Applications: Underhood componentsLamp housingsHVAC ductsInjection molding conditions reported in table.Information provided by RheTech Products.
Copyright © lookpolymers.com All Rights Reserved