Processing Properties | Metric | English | Comments |
---|---|---|---|
Dry Time | 1 - 2 hour | 1 - 2 hour | |
RheTech Products F56-01 40% Glass Fiber/Mineral Co-Reinforced Polypropylene, Chemically Coupled, Black Applications: Consumer goodsUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Dry Time | 1 - 2 hour | 1 - 2 hour | |
RheTech Products FRP102-00 Polypropylene, Flame Retardant, Natural Applications: Electrical component housingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Dry Time | 1 - 2 hour | 1 - 2 hour | |
RheTech Products FT1003-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural Applications: Step and hitch padsInterior component and trimA/B pillarsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Dry Time | 1 - 2 hour | 1 - 2 hour | |
RheTech Products FT1004-01 Thermoplastic Polyolefin, Non-UV Stabilized, Black Applications: Step padsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Dry Time | 1 - 2 hour | 1 - 2 hour | |
RheTech Products FT2202-732UV Thermoplastic Polyolefin, UV Stabilized, YGYA Black Applications: Box top railTail gate linerExterior trimInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Dry Time | 1 - 2 hour | 1 - 2 hour | |
RheTech Products FT2700-01 Thermoplastic Polyolefin, Non-UV Stabilized, Black Applications: Air deflectorsFuel filler shieldsUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Dry Time | 1 - 2 hour | 1 - 2 hour | |
RheTech Products FT3080-50 Thermoplastic Polyolefin, UV Stabilized, YGYA Black Applications: Step padsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Dry Time | 1 - 2 hour | 1 - 2 hour | |
RheTech Products FT4900-746UV Thermoplastic Polyolefin, UV Stabilized, CD7 Dark Slate Solid Applications: Exterior componentsBodyside moldingsStep padsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Dry Time | 1 - 2 hour | 1 - 2 hour | |
RheTech Products FT7016-50UV Thermoplastic Polyolefin, UV Stabilized, YGYA Black Applications: Bumper coversCladdingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Dry Time | 1 - 2 hour | 1 - 2 hour | |
RheTech Products G13P100-01UV 13% Glass Fiber Reinforced Polypropylene, UV Stabilized, Black Applications: Interior trimAir ducts - distributionFuel filler pocketInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Dry Time | 1 - 2 hour | 1 - 2 hour | |
RheTech Products G13P100-553UV 13% Glass Fiber Reinforced Polypropylene, UV Stabilized, (GM 501F) Dark Smoke Gray Applications: Interior trimAir ducts - distributionFuel filler pocketInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Dry Time | 1 - 2 hour | 1 - 2 hour | |
RheTech Products G20P100-01UV 20% Glass Fiber Reinforced Polypropylene, UV Stabilized, Black Applications: Rigid exterior componentsHousingsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Dry Time | 1 - 2 hour | 1 - 2 hour | |
RheTech Products GC15P200-00 15% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Black Applications: Electrical housingsUnderhood componentsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Dry Time | 1 - 2 hour | 1 - 2 hour | |
RheTech Products GC30P100-01 30% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Black Applications: Arm rest insertBattery trayBracketsAir cleaner housingInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Dry Time | 1 - 2 hour | 1 - 2 hour | |
RheTech Products HP519-01 26% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, Black Applications: Interior trim moldingsSill platesAir ductsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Dry Time | 1 - 2 hour | 1 - 2 hour | |
RheTech Products HP521-186 15% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 7701 Graphite Applications: Interior trimIP structural componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Dry Time | 1 - 2 hour | 1 - 2 hour | |
RheTech Products HP522-390 15% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, AYCA Medium Prairie Applications: ConsolesClose out panelInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Dry Time | 1 - 2 hour | 1 - 2 hour | |
RheTech Products HP531-680UV 22% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, Medium Scratch Resistant, BJAA Light Parchment Applications: I/P componentsInterior trimA/B/C/ PillarsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Dry Time | 1 - 2 hour | 1 - 2 hour | |
RheTech Products M12P100-01 12% Mica Reinforced Polypropylene, Black Applications: Fan shroudsAir ductsFiller panelsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Dry Time | 1 - 2 hour | 1 - 2 hour | |
RheTech Products M20P100-01 20% Mica Reinforced Polypropylene, Black Applications: Fan shroudsFiller panelsAir ductsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Dry Time | 1 - 2 hour | 1 - 2 hour | |
RheTech Products P256-762 Polypropylene Copolymer, Medium Grey Applications: Misc. ClipsElectrical housingInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Dry Time | 1 - 2 hour | 1 - 2 hour | |
RheTech Products T40P100-00A 40% Talc Reinforced Polypropylene, Natural Applications: Durable goodsHVAC componentsFunctional supportsElectrical housingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Dry Time | 1 - 2 hour | 1 - 2 hour | |
RheTech Products F35-01 35% Glass Fiber/Mineral Co-Reinforced Polypropylene Copolymer, Chemically Coupled, Black Applications: Interior trimUnderhood componentsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Dry Time | 1 - 2 hour | 1 - 2 hour | |
RheTech Products HP516-01 7% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, Black Applications: Interior trimCenter consolesHush panelsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Dry Time | 1 hour | 1 hour | Predrying Time |
Tisan TISETILEN® UNR Polyethylene TISETILEN has a wide area of application in construction, building auxiliary materials, lighting equipment, household appliance, toy industries, etc. General specifications include Low densityFlexib.. |
|||
Dry Time | 1 hour | 1 hour | Predrying Time |
Tisan TISOPLEN® 20% Talc Filled Heat Stabilized Homopolymer Polypropylene TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois.. |
|||
Dry Time | 1 - 2 hour | 1 - 2 hour | |
RheTech Products GC30P104-00 30% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Natural Applications: BracketsHead lamp housingsBattery trayInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Dry Time | 1 - 2 hour | 1 - 2 hour | |
RheTech Products HP501-00 High Performance Polypropylene Copolymer, Non-UV Stabilized, Natural Applications: Battery traysInterior TrimInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Dry Time | 1 - 2 hour | 1 - 2 hour | |
RheTech Products HP507-01 38% Talc Reinforced High Performance Polypropylene, Non-UV Stabilized, Black Applications: IP structural componentsSpeaker housingsAutomotive interior componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Dry Time | 1 - 2 hour | 1 - 2 hour | |
RheTech Products HP522-357 15% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, JA6A Black Applications: Center consolesAir vents louversInterior trimInjection molding conditions reported in table.Information provided by RheTech Products. |