Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Specific Gravity = 1.07 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Specific Gravity 1.07 g/cc
1.07 g/cc
NuSil R-2631 Silicone, Electrically Conductive
General Purpose: Electrically ConductiveComments: Low Duromter, ToughCure System: PlatinumInformation provided by NuSil
Specific Gravity 1.07 g/cc
1.07 g/cc
23/23°C; ASTM D792
RheTech Products RCC220-01 20% Calcium Carbonate Reinforced Polypropylene Copolymer, Black, Recycled Content
Applications: I/P hush panelsSplash shieldsUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products.
Specific Gravity 1.07 g/cc
1.07 g/cc
ASTM D792
Noble Polymers Regis™ 285107 Thermoplastic Olefin (TPO)
Regis is a TPO (thermoplastic olefin) produced by Noble Polymers based on olefin/elastomer compounding. We have created Regis for use in bumpers and bumper fascias, air dams, exterior panels, materi..
Specific Gravity 1.07 g/cc
1.07 g/cc
Resinlab® CYNERGY CA6101 Adhesive
Description: The CYNERGY 6100 SERIES products are used to bond metal to itself or other substrates. It is available in five standard viscosities.Application: The CYNERGY SERIES of the cyanoacrylates..
Specific Gravity 1.07 g/cc
1.07 g/cc
ASTM D792
RTP Company RTP 281F  Nylon 12 (PA 12) Carbon Fiber 10%  (discontinued **)
Carbon Fiber 10%Comments:Carbon FiberUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided by RTP Company.Data fo..
Specific Gravity 1.07 g/cc
1.07 g/cc
ASTM D792
LG Chemical LI921NS ASA
Description: High Weatherability, AntistaticApplication: Sanitary ApplicationsCAS: 26299-47-8Information provided by LG Chemical
Specific Gravity 1.07 g/cc
1.07 g/cc
ASTM D792
LG Chemical LI951 Heat Resistant ASA
Description: High Heat ASAApplication: Automotive Part (Radiator Grill, Side Mirror)CAS: 26299-47-8Information provided by LG Chemical
Specific Gravity 1.07 g/cc
1.07 g/cc
ASTM D792
LG Chemical LUCON 6080EX ABS+CF
Description: Injection Molding, ABS+CF, Electrostatic Dissipation, Wide Processing RangeApplication: Carrying Cart Pipe Coating, BLU carrying TrayCAS No. 9003-56-9, 9003-54-7 and 7782-42-6Informatio..
Specific Gravity 1.07 g/cc
1.07 g/cc
Momentive Performance Materials TUFELâ„¢ II 94205 Low Volatile Extrusion Heat Cured Rubber
Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta..
Specific Gravity 1.07 g/cc
1.07 g/cc
Shin-Etsu Silicones KF-7312k Fluid
Information Provided by Shin-Etsu Silicones of America, Inc.
Specific Gravity 1.07 g/cc
1.07 g/cc
ASTM D792
Samsung Cheil Industries Starex® WX-9300UV ASA, Unreinforced Heat Resistant
Information provided by Samsung Cheil Industries.
Specific Gravity 1.07 g/cc
1.07 g/cc
ASTM D792
SABIC Innovative Plastics NORYL PX1712 PPE+HIPS (Asia Pacific)
PPE/HIPS unfilled high heat for auto interior
Specific Gravity 1.07 g/cc
1.07 g/cc
ASTM D792
A. Schulman POLYTROPE™ TPP 524 Injection Molding Grade Olefinic Thermoplastic Elastomer
DescriptionPolytrope TPP 524 is an injection molding grade olefinic thermoplastic elastomer. This mineral filled product is recommended for applications requiring high stiffness and low thermal exp..
Specific Gravity 1.07 g/cc
1.07 g/cc
ASTM D792
A. Schulman POLYBATCH™ Orange 1096 Concentrate Based In Polyethylene
DescriptionPOLYBATCH® 1096 is an orange color concentrate based in polyethylene. This concentrate was designed to provide color in polyolefin film and molding applications. POLYBATCH® 1096 is he..
Specific Gravity 1.07 g/cc
1.07 g/cc
ASTM D792
Chase Plastics CP Pryme® ASA300 BK General Purpose (Utility) ASA Molding Resin
Information provided by Chase Plastics.
Specific Gravity 1.07 g/cc
1.07 g/cc
ISO 1183/1
A. Schulman POLYFORT™ FPP 1876 22% Mineral Filled Copolymer, UV Inhibited Polypropylene
DescriptionPolyfort® FPP 1876 is a 22% mineral filled copolymer UV Inhibited Polypropylene. It is high flow. Information provided by A. Schulman.
Specific Gravity 1.07 g/cc
1.07 g/cc
ASTM D792
Lubrizol Estane® MVT 75AT3 Thermoplastic Polyurethane, Moisture Vapor Transmission
Type: Estane® MVT 75AT3 is a 75A aromatic polyether-based thermoplastic polyurethane (TPU).Features: High moisture vapor transmission with low water swell. Excellent low temperature properties and..
Specific Gravity 1.07 g/cc
1.07 g/cc
ASTM D792
A. Schulman SCHULAMID® E-17222 High Impact Nylon 66
Information provided by A. Schulman.
Specific Gravity 1.07 g/cc
1.07 g/cc
ASTM D792
A. Schulman POLYFLAM™ E-17338 22% CACO3 Filled Copolymer Polypropylene
DescriptionPolyfort® E 17338 is a 22% filled copolymer polypropylene product. Information provided by A. Schulman.
Specific Gravity 1.07 g/cc
1.07 g/cc
Trelleborg R520 Natural Rubber Polyisoprene
All information provided by Trelleborg
Specific Gravity 1.07 g/cc
1.07 g/cc
ASTM D792
Diamond Polymers NYLON 6615 HS Natural
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Specific Gravity 1.07 g/cc
1.07 g/cc
ASTM D792
Diamond Polymers SAN 268 Styrene Acrylonitrile, Transparent Engineering Thermoplastic
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Specific Gravity 1.07 g/cc
1.07 g/cc
Esstech X-943-7466 Triethyleneglycol Dimethacrylate, C14H22O6
Triethylene glycol dimethacrylate is a difunctional monomer that has been the foundation of many long-standing dental formulations. It has ideal water absorptivity and stability properties. Listed ..
Specific Gravity 1.07 g/cc
1.07 g/cc
ASTM D792
Clariant Renol PA233HT Nylon 6, Improved Processability, Easily Colorable, Highly Toughened
Data provided by Clariant Masterbatches
Specific Gravity 1.07 g/cc
1.07 g/cc
ASTM D792
Bhansali Engineering Abstron IMC25 ABS-PC Alloy
Medium FlowInformation provided by Bhansali
Specific Gravity 1.07 g/cc
1.07 g/cc
resin
BCC Products BC 8660E Urethane Elastomer
BC8660E is a multi-purpose elastomer that can perform many functions. Special product characteristics are: excellent use for molds for casting of concrete and plaster, resists moisture absorption, d..
Specific Gravity 1.07 g/cc

@Temperature 25.0 °C
1.07 g/cc

@Temperature 77.0 °F
Dow Corning 3037 INTERMEDIATE
Reactive silicone intermediate for coil coatings, appliance finishes and other finishes where improved heat or weathering resistance is needed. Typically reacted with saturated polyesters or oil-fre..
Specific Gravity 1.07 g/cc
1.07 g/cc
ASTM D 792
RTP Company EMI 2862-60A Value-added Thermoplastic Polyolefin Elastomer, Stainless Steel Fiber - Electrically Conductive - EMI/RFI/ESD Protection
Data for this product has not been recently verified, please contact RTP Company for more information before specifying this grade.
Specific Gravity 1.07 g/cc
1.07 g/cc
ASTM D792
Bhansali Engineering Santron IMS1000 Sparkle SAN Resin
High Transparent SANInformation provided by Bhansali
Copyright © lookpolymers.com All Rights Reserved