Processing Properties | Metric | English | Comments |
---|---|---|---|
Drying Temperature | 65.6 - 82.2 °C | 150 - 180 °F | |
RheTech Products FRP255-01 Polypropylene Copolymer, Flame Retardant, Black Applications: Electrical component housingsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Drying Temperature | 65.6 - 82.2 °C | 150 - 180 °F | |
RheTech Products FT2600-00UV Thermoplastic Polyolefin, Non-UV Stabilized, Natural Applications: Interior trimSplash shieldScuff padsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Drying Temperature | 65.6 - 82.2 °C | 150 - 180 °F | |
RheTech Products FT2600-677UV Thermoplastic Polyolefin, UV Stabilized, 0848 Black Applications: Exterior trimStep pads and hitch padsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Drying Temperature | 65.6 °C | 150 °F | |
PolyOne Gravi-Tech™ GRV-UR-080-W Polyurethane, Unspecified (PUR, Unspecified) Information provided by PolyOne |
|||
Drying Temperature | 65.6 - 82.2 °C | 150 - 180 °F | |
RheTech Products FT5250-650UV Thermoplastic Polyolefin, UV Stabilized, Exterior 848 Black Applications: Cowl vent grillesExterior componentsBodyside moldingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Drying Temperature | 65.6 - 82.2 °C | 150 - 180 °F | |
RheTech Products G13P100-553UV 13% Glass Fiber Reinforced Polypropylene, UV Stabilized, (GM 501F) Dark Smoke Gray Applications: Interior trimAir ducts - distributionFuel filler pocketInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Drying Temperature | 65.6 - 82.2 °C | 150 - 180 °F | |
RheTech Products GC20P255-00 20% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Natural Applications: Underhood componentsElectrical housingsHeadlamp bracketsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Drying Temperature | 65.6 - 82.2 °C | 150 - 180 °F | |
RheTech Products GC30P200-01 30% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Black Applications: Window frameHead lamp housingInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Drying Temperature | 65.6 - 82.2 °C | 150 - 180 °F | |
RheTech Products GC30P200-01BG 30% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, General Purpose Black, Blow Molding Grade Applications: Load floorSeat backFunctional supportsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Drying Temperature | 65.6 - 82.2 °C | 150 - 180 °F | |
RheTech Products HP513-01 High Stiffness Polypropylene Copolymer, Medium Impact, UV Stabilized, Black Applications: Interior trimI/P componentsCenter consolesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Drying Temperature | 65.6 - 82.2 °C | 150 - 180 °F | |
RheTech Products HP514-182 14% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 7701 Graphite Applications: Glove box binInterior trimSteering column trimConsolesAir ducts - distributionInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Drying Temperature | 65.6 - 82.2 °C | 150 - 180 °F | |
RheTech Products HP521-188 15% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 9777 Medium Beige Applications: Interior trimIP structural componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Drying Temperature | 65.6 - 82.2 °C | 150 - 180 °F | |
RheTech Products HP532-01 20% Talc Reinforced High Performance Polypropylene, Non-UV Stabilized, Black Applications: Close out panelSpeaker grilleInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Drying Temperature | 65.6 - 82.2 °C | 150 - 180 °F | |
RheTech Products P249-01UV General Purpose Polypropylene Copolymer, UV Stabilized, Black Applications: LP bracketsSplash shieldsDoor/trunk scuffInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Drying Temperature | 65.6 - 82.2 °C | 150 - 180 °F | |
RheTech Products RCT120-01 20% Talc Reinforced Polypropylene, Black, Recycled Content Applications: HVAC and I/P ComponentsUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Drying Temperature | 65.6 - 82.2 °C | 150 - 180 °F | |
RheTech Products T10P102-00EG 10% Talc Reinforced Polypropylene, Extrusion Grade, Natural Injection molding conditions reported in table.Information provided by RheTech Products. |
|||
Drying Temperature | 65.6 - 82.2 °C | 150 - 180 °F | |
RheTech Products T20P252-01 20% Talc Reinforced Polypropylene Copolymer, Black Applications: IP Structural componentsGlove box binWire troughInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Drying Temperature | 65.6 - 82.2 °C | 150 - 180 °F | |
RheTech Products T28P100-01EG 28% Talc Reinforced Polypropylene, Black, Extrusion Grade Applications: Window trimConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Drying Temperature | 65.6 - 82.2 °C | 150 - 180 °F | |
RheTech Products T40P100-774UVA 40% Talc Reinforced Polypropylene, UV Stabilized, JA6A Black Applications: Wire troughBracketsConsolesFan shroudsFuse panel boxDoor cup pullsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Drying Temperature | 65.6 - 82.2 °C | 150 - 180 °F | |
RheTech Products HP520-00 12% Talc Reinforced High Performance Polypropylene Copolymer, Non-UV Stabilized, Natural Applications: Interior trimCenter consolesGlove box binsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Drying Temperature | 65.6 - 82.2 °C | 150 - 180 °F | |
RheTech Products HP521-288UV 15% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 167A Ebony Applications: Interior trimIP structural componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Drying Temperature | 65.6 - 82.2 °C | 150 - 180 °F | |
RheTech Products HP531-678UV 22% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, Medium Scratch Resistant, IT3A Medium Light Stone Applications: I/P componentsInterior trimA/B/C/ PillarsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Drying Temperature | 65.6 °C @Time 7200 sec |
150 °F @Time 2.00 hour |
|
Styrolution Zylar 650 MBS Zylar® 650 is an impact modified styrene acrylic copolymer that provides a balance of clarity and toughness, with outstanding strength and rigidity. Zylar 650 also has superior processing charact.. |
|||
Drying Temperature | 65.6 - 93.3 °C | 150 - 200 °F | Desiccant type |
CPT C-Flex® R70-050 Clear Biocompatible TPE C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current.. |
|||
Drying Temperature | 65.6 - 93.3 °C | 150 - 200 °F | Desiccant type |
CPT C-Flex® R70-190 Opaque Biocompatible TPE C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current.. |
|||
Drying Temperature | 65.6 - 82.2 °C | 150 - 180 °F | |
RheTech Products GC30P100-00 30% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Natural Applications: Arm rest insertBattery trayBracketsAir cleaner housingInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Drying Temperature | 65.6 - 82.2 °C | 150 - 180 °F | |
RheTech Products CC20P100-00 20% Calcium Carbonate Reinforced Polypropylene, Natural Applications: ElectronicsConsumer GoodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Drying Temperature | 65.6 - 82.2 °C | 150 - 180 °F | |
RheTech Products G20P252-00 20% Glass Fiber Reinforced Polypropylene Copolymer, Natural Applications: Interior trimArm rest insertConsolesDome light housingInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Drying Temperature | 65.6 - 82.2 °C | 150 - 180 °F | |
RheTech Products GC43P250-01 43% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Black Applications: Consumer goodsFunctional supportsHead lamp bracketsDurable GoodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Drying Temperature | 65.6 - 82.2 °C | 150 - 180 °F | |
RheTech Products HP522-357 15% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, JA6A Black Applications: Center consolesAir vents louversInterior trimInjection molding conditions reported in table.Information provided by RheTech Products. |