Overview of materials for High Density Polyethylene (HDPE), Crosslinkable

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Crosslinkable
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Overview of materials for High Density Polyethylene (HDPE), Crosslinkable.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Crosslinkable". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 0.872 - 1.47 g/cc
0.0315 - 0.0531 lb/in³
Average value: 0.959 g/cc Grade Count:27
Environmental Stress Crack Resistance >= 1000 hour

@Temperature 50.0 - 50.0 °C
>= 1000 hour

@Temperature 122 - 122 °F
Average value: 1000 hour Grade Count:3
Melt Flow 0.350 - 6.10 g/10 min
0.350 - 6.10 g/10 min
Average value: 1.50 g/10 min Grade Count:23
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 17.0 - 26.5 MPa
2470 - 3840 psi
Average value: 20.9 MPa Grade Count:19
Tensile Strength, Yield 18.0 - 26.0 MPa
2610 - 3770 psi
Average value: 20.1 MPa Grade Count:5
6.00 - 47.0 MPa

@Temperature -40.0 - 100 °C
870 - 6820 psi

@Temperature -40.0 - 212 °F
Average value: 26.5 MPa Grade Count:1
Elongation at Break 110 - 540 %
110 - 540 %
Average value: 356 % Grade Count:24
170 - 390 %

@Temperature 100 - 150 °C
170 - 390 %

@Temperature 212 - 302 °F
Average value: 280 % Grade Count:1
Elongation at Yield 7.00 - 16.0 %

@Temperature -40.0 - 100 °C
7.00 - 16.0 %

@Temperature -40.0 - 212 °F
Average value: 11.5 % Grade Count:1
Modulus of Elasticity 0.00600 - 1.30 GPa
0.870 - 189 ksi
Average value: 0.635 GPa Grade Count:11
0.130 - 3.30 GPa

@Temperature -40.0 - 100 °C
18.9 - 479 ksi

@Temperature -40.0 - 212 °F
Average value: 1.72 GPa Grade Count:1
Flexural Modulus 0.689 - 0.690 GPa
100 - 100 ksi
Average value: 0.690 GPa Grade Count:4
0.167 - 2.60 GPa

@Temperature -40.0 - 100 °C
24.2 - 377 ksi

@Temperature -40.0 - 212 °F
Average value: 1.38 GPa Grade Count:1
Charpy Impact, Notched 1.50 - 999.9 J/cm²

@Temperature -40.0 - 100 °C
7.14 - 4759 ft-lb/in²

@Temperature -40.0 - 212 °F
Average value: 1.50 J/cm² Grade Count:1
Thermal Properties Metric English Comments
CTE, linear 140 - 190 µm/m-°C
77.8 - 106 µin/in-°F
Average value: 163 µm/m-°C Grade Count:8
100 - 100 µm/m-°C

@Temperature -90.0 - -30.0 °C
55.6 - 55.6 µin/in-°F

@Temperature -130 - -22.0 °F
Average value: 100 µm/m-°C Grade Count:1
Specific Heat Capacity 1.80 - 2.03 J/g-°C
0.430 - 0.485 BTU/lb-°F
Average value: 1.91 J/g-°C Grade Count:9
Thermal Conductivity 0.450 - 0.490 W/m-K
3.12 - 3.40 BTU-in/hr-ft²-°F
Average value: 0.468 W/m-K Grade Count:10
Vicat Softening Point 50.0 - 129 °C
122 - 264 °F
Average value: 115 °C Grade Count:14
Brittleness Temperature -90.0 °C
-130 °F
Average value: -90.0 °C Grade Count:3
Electrical Properties Metric English Comments
Electrical Resistivity 4.10e+15 ohm-cm
4.10e+15 ohm-cm
Average value: 4.10e+15 ohm-cm Grade Count:3
1.40e+15 - 2.70e+15 ohm-cm

@Temperature 90.0 - 90.0 °C
1.40e+15 - 2.70e+15 ohm-cm

@Temperature 194 - 194 °F
Average value: 2.27e+15 ohm-cm Grade Count:3
Dielectric Constant 2.30 - 2.40
2.30 - 2.40
Average value: 2.33 Grade Count:3
Dielectric Strength 32.0 - 35.0 kV/mm
813 - 889 kV/in
Average value: 33.7 kV/mm Grade Count:3
Dissipation Factor 0.000500 - 0.000600
0.000500 - 0.000600
Average value: 0.000567 Grade Count:3
Processing Properties Metric English Comments
Processing Temperature 246 - 326 °C
475 - 619 °F
Average value: 286 °C Grade Count:3
Die Temperature 182 - 220 °C
360 - 428 °F
Average value: 204 °C Grade Count:10
Melt Temperature 140 - 200 °C
284 - 392 °F
Average value: 173 °C Grade Count:22
Head Temperature 200 - 210 °C
392 - 410 °F
Average value: 204 °C Grade Count:9
Screw Cooling Temperature 70.0 - 90.0 °C
158 - 194 °F
Average value: 80.0 °C Grade Count:7
Die Cooling Temperature 180 - 230 °C
356 - 446 °F
Average value: 209 °C Grade Count:12