Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 2.03 - 3.30 GPa | 294 - 479 ksi | Average value: 2.64 GPa Grade Count:50 |
Overview of materials for PVC, High Impact This property data is a summary of similar materials in the MatWeb database for the category "PVC, High Impact". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
Modulus of Elasticity | 1.40 - 3.30 GPa | 203 - 479 ksi | Average value: 2.46 GPa Grade Count:26 |
Overview of materials for Polypropylene with 40% Calcium Carbonate (CaCO3) Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Calcium Carbonate (CaCO3) Filler". Specific grades with primary filler content be.. |
|||
Modulus of Elasticity | 0.100 - 3.30 GPa | 14.5 - 479 ksi | Average value: 1.75 GPa Grade Count:25 |
Overview of materials for Nylon 6, Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Film Grade". Each property range of values reported is minimum and maximum values of appropriat.. |
|||
Modulus of Elasticity | 0.0000689 - 3.30 GPa | 0.0100 - 479 ksi | Average value: 2.45 GPa Grade Count:19 |
Overview of materials for Acetal Homopolymer, PTFE-Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, PTFE-Filled". Each property range of values reported is minimum and maximum values o.. |
|||
Modulus of Elasticity | 1.80 - 3.30 GPa | 261 - 479 ksi | Average value: 2.96 GPa Grade Count:19 |
Overview of materials for Acrylic, Extruded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Extruded". Each property range of values reported is minimum and maximum values of appropriate .. |
|||
Modulus of Elasticity | 2.80 - 3.30 GPa | 406 - 479 ksi | Average value: 3.17 GPa Grade Count:4 |
Overview of materials for Acrylic, Cast This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Cast". Each property range of values reported is minimum and maximum values of appropriate MatW.. |
|||
Modulus of Elasticity | 0.130 - 3.30 GPa @Temperature -40.0 - 100 °C |
18.9 - 479 ksi @Temperature -40.0 - 212 °F |
Average value: 1.72 GPa Grade Count:1 |
Overview of materials for High Density Polyethylene (HDPE), Crosslinkable This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Crosslinkable". Each property range of values reported is minimum and .. |
|||
Modulus of Elasticity | 0.145 - 3.30 GPa @Temperature -40.0 - 150 °C |
21.0 - 479 ksi @Temperature -40.0 - 302 °F |
Average value: 0.997 GPa Grade Count:8 |
Overview of materials for Nylon 6, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Impact Grade". Each property range of values reported is minimum and maximum values of appropri.. |