Mechanical Properties Metric English Comments
Tensile Strength, Yield 0.0827 - 47.0 MPa
12.0 - 6820 psi
Average value: 4.49 MPa Grade Count:499
Overview of materials for Thermoplastic Elastomer, Melt-Processible Rubber
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Elastomer, Melt-Processible Rubber". Each property range of values reported is minimum and..
Tensile Strength, Yield 6.00 - 47.0 MPa

@Temperature -40.0 - 100 °C
870 - 6820 psi

@Temperature -40.0 - 212 °F
Average value: 26.5 MPa Grade Count:1
Overview of materials for High Density Polyethylene (HDPE), Crosslinkable
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Crosslinkable". Each property range of values reported is minimum and ..