Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.450 W/m-K | 3.12 BTU-in/hr-ft²-°F | |
Quantum Composites LYTEX® 4181 55% Carbon Fiber Reinforced Epoxy SMC LYTEX 4181 is an epoxy ESC molding compound designed for structural applications requiring excellent mechanical properties, retention of properties at elevated temperatures, good chemical resistance.. |
|||
Thermal Conductivity | 0.450 W/m-K | 3.12 BTU-in/hr-ft²-°F | |
Quantum Composites LYTEX® 4182 50-55% Carbon Fiber Reinforced Epoxy SMC LYTEX 4182 is an epoxy ESC molding compound designed for structural applications requiring excellent mechanical properties, retention of properties at elevated temperatures, good chemical resistance.. |
|||
Thermal Conductivity | 0.450 - 3.80 W/m-K | 3.12 - 26.4 BTU-in/hr-ft²-°F | Average value: 1.16 W/m-K Grade Count:5 |
Overview of materials for Polyphthalamide (PPA), Carbon Fiber This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Carbon Fiber". Each property range of values reported is minimum and maximum values of .. |
|||
Thermal Conductivity | 0.450 W/m-K | 3.12 BTU-in/hr-ft²-°F | D24/23; IPC-TM-650, 2.6.2.1 |
Rogers Corporation RO3730 Antenna Grade Laminate RO3730™ Laminates have the excellent thermo-mechanical properties and electrical characteristics that antenna designers need. The laminates have a dielectric constant of 3.0 and a loss tangent of.. |
|||
Thermal Conductivity | 0.450 W/m-K | 3.12 BTU-in/hr-ft²-°F | |
Premix Premi-Glas® 1286 Glass Reinforced SMC Description: Premi-Glas® 1286 is a glass reinforced thermoset sheet molding compound designed for automotive under the hood applications. Key features and benefits: Designed for compression molding.. |
|||
Thermal Conductivity | 0.450 W/m-K | 3.12 BTU-in/hr-ft²-°F | ASTM E1461 |
Park Electrochemical Nelco® N7000-2 HT/N7000-3 Toughened Polyimide Laminate and Prepreg The Nelco N7000-2 HT laminate and N7000-3 prepreg are a series of toughened polyimide materials for use in high-reliability multilayers. This combined resin system provides excellent thermal perform.. |
|||
Thermal Conductivity | 0.450 W/m-K | 3.12 BTU-in/hr-ft²-°F | DIN 52612 |
Lehmann & Voss LUVOCOM® 1105-7185 PEEK, with carbon fiber, PTFE, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; low thermal coefficient of expansion.Dynamic stressed parts at high m.. |
|||
Thermal Conductivity | 0.450 W/m-K | 3.12 BTU-in/hr-ft²-°F | DIN 52612 |
Lehmann & Voss LUVOCOM® 1105-8350 PEEK, with carbon fiber, PTFE, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; low thermal coefficient of expansion.Dynamic stressed parts at high m.. |
|||
Thermal Conductivity | 0.450 W/m-K | 3.12 BTU-in/hr-ft²-°F | DIN 52612 |
Lehmann & Voss LUVOCOM® 1105-8422 PEEK, with carbon fiber, PTFE, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; low thermal coefficient of expansion.Dynamic stressed parts at high m.. |
|||
Thermal Conductivity | 0.450 W/m-K | 3.12 BTU-in/hr-ft²-°F | DIN 52612 |
Lehmann & Voss LUVOCOM® 20-7343 Polyphthalamide, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Low influence from moisture an.. |
|||
Thermal Conductivity | 0.450 W/m-K | 3.12 BTU-in/hr-ft²-°F | DIN 52612 |
Lehmann & Voss LUVOCOM® 50/CF/15/TF/15/SI/2/BK Polycarbonate, with carbon fiber, PTFE, lubricant modified Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High-strength and high-stiff parts; low coefficient of expansi.. |
|||
Thermal Conductivity | 0.450 W/m-K | 3.12 BTU-in/hr-ft²-°F | DIN 52612 |
Lehmann & Voss LUVOCOM® 50/CF/15/TF/15/SI/2/BK-HB Polycarbonate, with carbon fiber, PTFE, lubricant modified Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High-strength and high-stiff parts; low coefficient of expansi.. |
|||
Thermal Conductivity | 0.450 W/m-K | 3.12 BTU-in/hr-ft²-°F | DIN 52612 |
Lehmann & Voss LUVOCOM® 50-7446 Polycarbonate, with carbon fiber, PTFE, lubricant modified Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High-strength and high-stiff parts; low coefficient of expansi.. |
|||
Thermal Conductivity | 0.450 W/m-K | 3.12 BTU-in/hr-ft²-°F | DIN 52612 |
Lehmann & Voss LUVOCOM® 80-7050 Polyacetal-copolymer, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts; low thermal coefficient of expansion.Electrically conductive, suitable for.. |
|||
Thermal Conductivity | 0.450 W/m-K | 3.12 BTU-in/hr-ft²-°F | DIN 52612 |
Lehmann & Voss LUVOCOM® 1105/CF/10/GR/10/TF/10-2 PEEK, with carbon fiber, PTFE, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; low thermal coefficient of expansion.Dynamic stressed parts at high m.. |
|||
Thermal Conductivity | 0.450 - 0.470 W/m-K | 3.12 - 3.26 BTU-in/hr-ft²-°F | ASTM C177 |
Solvay Specialty Polymers Polidan® PNT 0553/23 Polyethylene, Crosslinked (XLPE) POLIDAN® PNT 0553/23 is a silane crosslinkable PE compound which is used together with a catalyst masterbatch to accelerate the crosslinking reaction.Features: Crosslinkable; Good Flexibility; Lo.. |
|||
Thermal Conductivity | 0.450 - 0.470 W/m-K | 3.12 - 3.26 BTU-in/hr-ft²-°F | ASTM C177 |
Solvay Specialty Polymers Polidan® PNT 0555/06 Polyethylene, Crosslinked (XLPE) POLIDAN® PNT 0555/06 is a silane crosslinkable PE compound which is used together with a catalyst masterbatch to accelerate the crosslinking reaction. It is used for flexible crosslinkable pipes... |
|||
Thermal Conductivity | 0.450 - 0.470 W/m-K | 3.12 - 3.26 BTU-in/hr-ft²-°F | ASTM C177 |
Solvay Specialty Polymers Polidan® PNT 0856/35 Polyethylene, Crosslinked (XLPE) POLIDAN® PNT 0856/35 is a silane crosslinkable PE compound which is used together with a catalyst masterbatch to accelerate the crosslinking reaction.Features: Crosslinkable; Good Flexibility; Lo.. |
|||
Thermal Conductivity | 0.450 - 0.470 W/m-K | 3.12 - 3.26 BTU-in/hr-ft²-°F | ASTM C177 |
Solvay Specialty Polymers Polidan® T/A-HF Polyethylene, Crosslinked (XLPE) POLIDAN® T/A-HF is a silane crosslinkable PE compound which is used together with a catalyst masterbatch to accelerate the crosslinking reaction. It is used for flexible crosslinkable pipes.Featu.. |
|||
Thermal Conductivity | 0.450 - 0.470 W/m-K | 3.12 - 3.26 BTU-in/hr-ft²-°F | ASTM C177 |
Solvay Specialty Polymers Polidan® T/A-LX Polyethylene, Crosslinked (XLPE) POLIDAN® T/A-LX is a silane crosslinkable PE compound which is used together with a catalyst masterbatch to accelerate the crosslinking reaction. It is used for flexible crosslinkable pipes.Featu.. |
|||
Thermal Conductivity | 0.450 W/m-K @Temperature 100 °C |
3.12 BTU-in/hr-ft²-°F @Temperature 212 °F |
ASTM E1461 |
Plenco 3509 Phenolic, Granular, Injection Molded PLENCO 03509 is a mineral and flock filled phenolic molding compound offering excellent electrical properties, dimensional stability, and improved heat resistance. UL recognized under component file.. |
|||
Thermal Conductivity | 0.450 W/m-K @Temperature 100 °C |
3.12 BTU-in/hr-ft²-°F @Temperature 212 °F |
ASTM E1225 |
Arlon 25FR Low-Cost Ceramic Hydrocarbon High Frequency, Low Loss Thermoset Laminate and Prepreg for Double-sided, Multilayer and Mixed Dielectric Printed Circuit BoardsLow loss ceramic-filled thermoset resinTight dielectric tolerance cont.. |
|||
Thermal Conductivity | 0.450 W/m-K @Temperature 100 °C |
3.12 BTU-in/hr-ft²-°F @Temperature 212 °F |
ASTM E1225 |
Arlon 25N Low-Cost Ceramic Hydrocarbon High Frequency, Low Loss Thermoset Laminate and Prepreg for Double-sided, Multilayer and Mixed Dielectric Printed Circuit BoardsLow loss ceramic-filled thermoset resinTight dielectric tolerance cont.. |
|||
Thermal Conductivity | 0.450 W/m-K | 3.12 BTU-in/hr-ft²-°F | ASTM E1461 |
Arlon EP2 Enhanced Polyimide Laminate and Prepreg High reliability and high temperature materialEP2 Enhanced Polyimide is the next generation of polyimide and prepreg products, engineered for improved properties and processing and for applications .. |
|||
Thermal Conductivity | >= 0.450 W/m-K | >= 3.12 BTU-in/hr-ft²-°F | Compound Property |
Arlon Thermabond®-II 99760N008 0.008" (0.203 mm) Unsupported/Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Unsupported/Uncured RubberAppearance: White/gray gumAppearance: White/grey gumThis data Represents typical values for the production material. The data should not be used.. |
|||
Thermal Conductivity | 0.450 W/m-K | 3.12 BTU-in/hr-ft²-°F | Mfr. internal test |
Ascend Performance Materials VYDYNE® R220 Nylon, Mineral Reinforced Typical property data. VYDYNE is a registered trademark of Solutia Inc. |
|||
Thermal Conductivity | 0.450 W/m-K @Temperature 100 °C |
3.12 BTU-in/hr-ft²-°F @Temperature 212 °F |
ASTM E1225 |
Arlon AD350A PTFE/Woven Fiberglass/Ceramic Filled Composite Tighter Dielectric Tolerance Low Z-Axis Thermal ExpansionCeramic Filled PTFEHigh Thermal ConductivityLarge Panel SizeBenefits:Higher Consistency of PerformanceSuperior PTH AdhesionHeat Dissipation a.. |
|||
Thermal Conductivity | 0.450 W/m-K @Temperature 1400 °C |
3.12 BTU-in/hr-ft²-°F @Temperature 2550 °F |
|
Sinotek Materials Graphite Felt Heat Insulation Material Information provided by Sinotek |
|||
Thermal Conductivity | 0.450 - 0.490 W/m-K | 3.12 - 3.40 BTU-in/hr-ft²-°F | Average value: 0.468 W/m-K Grade Count:10 |
Overview of materials for High Density Polyethylene (HDPE), Crosslinkable This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Crosslinkable". Each property range of values reported is minimum and .. |