Polymer Property : Die Cooling Temperature = 356 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Die Cooling Temperature 180 - 200 °C
356 - 392 °F
Solvay Specialty Polymers Cogegum® AFR/920-UV Polyolefin
Flame Retardant; Good UV Resistance; Halogen Free; Low Smoke Emission; Low Toxicity; Self ExtinguishingUses: Cable Jacketing; Low Voltage Insulation; Wire & Cable ApplicationsExtrusion equipment: st..
Die Cooling Temperature 180 - 210 °C
356 - 410 °F
Solvay Specialty Polymers Cogegum® GFR/350 Polyolefin
Cogegum® XLPO-HFFR - Crosslinkable Halogen Free Fire Retardant compound. Silane grafted compound moisture curable by addition of a catalyst masterbatch (Sioplas® method). It consists of a pol..
Die Cooling Temperature 180 - 220 °C
356 - 428 °F
Solvay Specialty Polymers Polidan® EC/110 Polyethylene, Crosslinked (XLPE)
Polidan® XLPE-PEX -Cross-linkable Polyethylene. Low density polyethylene based compound crosslinkable by moisture; it consists of a silane pregrafted base compound (Sioplas® method) to be use..
Die Cooling Temperature 180 - 230 °C
356 - 446 °F
Solvay Specialty Polymers Polidan® EC/51 Polyethylene, Crosslinked (XLPE)
Flexible low density polyethylene based compound crosslinkable by moisture; it consists of a silane pregrafted base compound (Sioplas® method) to be used with a catalyst masterbatch.Standards com..
Die Cooling Temperature 180 - 220 °C
356 - 428 °F
Solvay Specialty Polymers Polidiemme® G/420 Thermoset Elastomer (TSE)
Polidiemme® XLPO -Cross-linkable Polyolefin. Elastomer based compound crosslinkable by ambient moisture, consisting of a silane pregrafted base compound to be used with a catalyst masterbatch (Si..
Die Cooling Temperature 180 - 200 °C
356 - 392 °F
Solvay Specialty Polymers Cogegum® AFR/960 Polyolefin
Cogegum® HFFR -Halogen Free Fire Retardant compound. Polyolefin based thermoplastic compound containing a fire retardant system that contributes to give the cable self-extinguish properties withou..
Die Cooling Temperature 180 - 230 °C
356 - 446 °F
Average value: 209 °C Grade Count:12
Overview of materials for High Density Polyethylene (HDPE), Crosslinkable