Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.689 GPa | 100 ksi | Tangent; ASTM D790 |
RheTech Products FT2400-647UV Thermoplastic Polyolefin, UV Stabilized, 8798NM Grey Applications: Bumper rub stripsHitch padsScuff padsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 0.690 GPa | 100 ksi | ASTM D790 |
Nylene® 404 Nylon 6, 50% RH Injection molding grade. Nylene 404 is a heat stabilized version of 401 which is recommended for general purpose nylon molding applications in both thin and heavy sections. In addition to protection.. |
|||
Flexural Modulus | 0.689 GPa | 100 ksi | 1.3 mm/min; ASTM D790B |
Polimeros Mexicanos Rotolene® Diesel Tank Medium Density Polyethylene Hexene Copolymer Linear Medium Density Polyethylene. This resin is fully UV8 stabilized.High quality Polyethylene compound specially designed for automotive applications, water tanks, diesel tanks a.. |
|||
Flexural Modulus | 0.689 GPa | 100 ksi | Test Method I, Procedure B (chs speed 0.05 in/min); ASTM D790 |
Network Polymers NPP 25-1902 Description: Copolymer PolypropyleneInformation provided by Network Polymers Inc. |
|||
Flexural Modulus | 0.690 GPa | 100 ksi | ISO 178 |
Polimeri Europa Clearflex® RM 50 U Linear Medium Density Polyethylene Clearflex RM 50 U is a linear medium density polyethylene resin, with antioxidants and UV stabilizers, suitable for rotomolding applications.Items manufactured with Clearflex RM 50 U show good mecha.. |
|||
Flexural Modulus | 0.689 GPa | 100 ksi | 1.3mm per min; ASTM D790 |
Formosa Plastics Formolene® L63565U Rotational Molding LLDPE
(discontinued **) Hexene CopolymerApplications: Toys, medium tanks, material handling equipment and flat surface rotational molding applications.Formolene L63565U is fully heat and UV stabilized.Meets all requirement.. |
|||
Flexural Modulus | 0.690 GPa | 100 ksi | ASTM D790 |
Chevron Phillips Marlex® CL-200YJN (Natural) Rotational molding crosslinkable high density polyethylene
(disc Benefits: crosslinks during molding - has outstanding melt strength at 204°C, is formulated to provide maximum UV protection for long-term outdoor weathering, contains an internal mold release, exc.. |
|||
Flexural Modulus | 0.690 GPa | 100 ksi | ASTM D790 |
Chevron Phillips Marlex® CL-200YNR JN (Natural) Rotational molding crosslinkable high density polyethylene
(d Benefits: crosslinks during molding - has outstanding melt strength at 204°C, is formulated to provide maximum UV protection for long-term outdoor weathering, contains an internal mold release, exc.. |
|||
Flexural Modulus | 0.690 GPa | 100 ksi | 1.3 mm/min; ASTM D790 |
ICO Polymers ICORENEâ„¢ 190-1325 LMDPE Rotational Molding Resin Description: ICORENE 190-1325 is a linear medium density polyethylene copolymer developed for rotational molding. It has a good balance of properties such as toughness, easy flow and stiffness. Key.. |
|||
Flexural Modulus | 0.690 GPa | 100 ksi | 1.3 mm/min; ASTM D790 |
ICO Polymers ICORENEâ„¢ 195-1325 LMDPE Rotational Molding Resin Description: ICORENE 195-1325 is a linear medium density polyethylene copolymer developed for rotational molding. It has a good balance of properties such as toughness, easy flow and stiffness. Ke.. |
|||
Flexural Modulus | 0.690 GPa | 100 ksi | ASTM D747 |
Ineos B50-35H-176 HDPE B50-35H is a high density polyethylene copolymer developed for blow molding. It is recommended for use in applications which require a combination of high top load strength and good environmental s.. |
|||
Flexural Modulus | 0.690 GPa | 100 ksi | ASTM D790 |
Ineos K38-20-160 Polyethylene Copolymer K38-20-160 is a medium density polyethylene copolymer containing an organic yellow pigment system, designed specifically for the extrusion of natural gas pipe. It exhibits excellent long term stres.. |
|||
Flexural Modulus | 0.690 GPa | 100 ksi | ISO 178 |
Solvay TECHNYL® eXten D 458P PA6.10, DRY Description: Product in development - provisional datasheet. High viscosity unfilled plasticized PA6.10 for extrusion applications providing low end part warpage.Available in: Asia Pacific, Europe, .. |
|||
Flexural Modulus | 0.689 GPa | 100 ksi | ASTM D790 |
A. Schulman POLYTROPE™ TPP 510 Injection Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 510 is an injection molding grade olefinic thermoplastic elastomer. This product has excellent low temperature impact properties and flow characteristics suitable for moldi.. |
|||
Flexural Modulus | 0.689 GPa | 100 ksi | ASTM D790 |
A. Schulman POLYTROPE™ TPP 1010E-01 Olefinic Elastomer For Sheet Extrusion DescriptionPolytrope TPP 1010E-01 is an olefinic elastomer designed for sheet extrusion, profile extrusion and blow molding. TPP 1010E-01 is a natural product which can be colored and UV stabilized.. |
|||
Flexural Modulus | 0.689 GPa | 100 ksi | ASTM D790 |
A. Schulman POLYTROPE™ TPP 510 Injection Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 510 is an injection molding grade olefinic thermoplastic elastomer. This product has excellent low temperature impact properties and flow characteristics suitable for moldi.. |
|||
Flexural Modulus | 0.689 GPa | 100 ksi | at 1% secant; ASTM D790 |
A. Schulman SCHULINK® X XL350 Cross-Linkable, High Density Polyethylene DescriptionSchuLink XL 350 is a cross-linkable, high density polyethylene used from rotational molding. This resin offers high impact strength, good abrasion resistance, good stiffness, and excelle.. |
|||
Flexural Modulus | 0.689 GPa | 100 ksi | ASTM D790 |
A. Schulman POLYTROPE™ CB 1010U-330 Injection Molding Reactor Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope CB 1010U-330 is a color matched/color blended injection molding reactor grade olefinic thermoplastic elastomer (TPO). This product has excellent low temperature impact properti.. |
|||
Flexural Modulus | 0.689 GPa | 100 ksi | at 1% secant; ASTM D790 |
A. Schulman SCHULINK® X XL350 Cross-Linkable, High Density Polyethylene DescriptionSchuLink XL 350 is a cross-linkable, high density polyethylene used from rotational molding. This resin offers high impact strength, good abrasion resistance, good stiffness, and excelle.. |
|||
Flexural Modulus | 0.690 GPa | 100 ksi | tangent; ASTM D790 |
A. Schulman POLYPUR™ FPU 1377 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Flexural Modulus | 0.689 GPa | 100 ksi | ASTM D790 |
A. Schulman POLYTROPE™ TPP 1010E-01 Olefinic Elastomer For Sheet Extrusion DescriptionPolytrope TPP 1010E-01 is an olefinic elastomer designed for sheet extrusion, profile extrusion and blow molding. TPP 1010E-01 is a natural product which can be colored and UV stabilized.. |
|||
Flexural Modulus | 0.690 GPa | 100 ksi | 70°C, 1.3 mm/min, 50 mm span, method 1, tangent; ASTM D790 |
A. Schulman POLYFORT™ FTP 3130H-01/FTP 3130HU-Colors DescriptionPolyfort® FTP 3130H-01 (non-UV stabilized) and FTP 3130HU-Colors (UV-stabilized) are high flow injection molding polyolefin alloys which exhibit an exceptional stiffness-impact balance a.. |
|||
Flexural Modulus | 0.689 GPa | 100 ksi | ASTM D790 |
A. Schulman POLYTROPE™ TPP 1010-01 Injection Molding Reactor Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 1010-01 is an injection molding reactor grade olefinic thermoplastic elastomer (TPO). This product has excellent low temperature impact properties and flow characteristics .. |
|||
Flexural Modulus | 0.689 GPa | 100 ksi | ASTM D790 |
A. Schulman POLYTROPE™ TPP 1010E-01 Olefinic Elastomer For Sheet Extrusion DescriptionPolytrope TPP 1010E-01 is an olefinic elastomer designed for sheet extrusion, profile extrusion and blow molding. TPP 1010E-01 is a natural product which can be colored and UV stabilized.. |
|||
Flexural Modulus | 0.690 GPa | 100 ksi | 70°C, 1.3 mm/min, 50 mm span, method 1, tangent; ASTM D790 |
A. Schulman POLYFORT™ FTP 3130H-01/FTP 3130HU-Colors DescriptionPolyfort® FTP 3130H-01 (non-UV stabilized) and FTP 3130HU-Colors (UV-stabilized) are high flow injection molding polyolefin alloys which exhibit an exceptional stiffness-impact balance a.. |
|||
Flexural Modulus | 0.689 GPa | 100 ksi | ASTM D790 |
A. Schulman POLYTROPE™ TPP 1010HF-01 Injection Molding Reactor Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 1010HF-01 is an injection molding reactor grade olefinic thermoplastic elastomer (TPO). This product has excellent low temperature impact properties and flow characteristic.. |
|||
Flexural Modulus | 0.690 - 2.80 GPa | 100 - 406 ksi | Average value: 2.22 GPa Grade Count:10 |
Overview of materials for Nylon 6, Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Film Grade". Each property range of values reported is minimum and maximum values of appropriat.. |