Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.450 - 3.80 W/m-K | 3.12 - 26.4 BTU-in/hr-ft²-°F | Average value: 1.16 W/m-K Grade Count:5 |
Overview of materials for Polyphthalamide (PPA), Carbon Fiber This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Carbon Fiber". Each property range of values reported is minimum and maximum values of .. |
|||
Thermal Conductivity | 0.450 W/m-K | 3.12 BTU-in/hr-ft²-°F | |
Premix Premi-Glas® 1286 Glass Reinforced SMC Description: Premi-Glas® 1286 is a glass reinforced thermoset sheet molding compound designed for automotive under the hood applications. Key features and benefits: Designed for compression molding.. |
|||
Thermal Conductivity | 0.450 W/m-K | 3.12 BTU-in/hr-ft²-°F | ASTM E1461 |
Park Electrochemical Nelco® N7000-2 HT/N7000-3 Toughened Polyimide Laminate and Prepreg The Nelco N7000-2 HT laminate and N7000-3 prepreg are a series of toughened polyimide materials for use in high-reliability multilayers. This combined resin system provides excellent thermal perform.. |
|||
Thermal Conductivity | 0.450 W/m-K | 3.12 BTU-in/hr-ft²-°F | DIN 52612 |
Lehmann & Voss LUVOCOM® 1105-7185 PEEK, with carbon fiber, PTFE, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; low thermal coefficient of expansion.Dynamic stressed parts at high m.. |
|||
Thermal Conductivity | 0.450 W/m-K | 3.12 BTU-in/hr-ft²-°F | DIN 52612 |
Lehmann & Voss LUVOCOM® 1105-8350 PEEK, with carbon fiber, PTFE, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; low thermal coefficient of expansion.Dynamic stressed parts at high m.. |
|||
Thermal Conductivity | 0.450 W/m-K | 3.12 BTU-in/hr-ft²-°F | DIN 52612 |
Lehmann & Voss LUVOCOM® 1105-8422 PEEK, with carbon fiber, PTFE, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; low thermal coefficient of expansion.Dynamic stressed parts at high m.. |
|||
Thermal Conductivity | 0.450 W/m-K | 3.12 BTU-in/hr-ft²-°F | DIN 52612 |
Lehmann & Voss LUVOCOM® 20-7343 Polyphthalamide, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Low influence from moisture an.. |
|||
Thermal Conductivity | 0.450 W/m-K | 3.12 BTU-in/hr-ft²-°F | DIN 52612 |
Lehmann & Voss LUVOCOM® 50/CF/15/TF/15/SI/2/BK-HB Polycarbonate, with carbon fiber, PTFE, lubricant modified Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High-strength and high-stiff parts; low coefficient of expansi.. |
|||
Thermal Conductivity | 0.450 W/m-K | 3.12 BTU-in/hr-ft²-°F | DIN 52612 |
Lehmann & Voss LUVOCOM® 50-1396 Polycarbonate, with carbon fiber, glass fiber and PTFE, electrically conducting Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High-strength and high-stiff parts; low coefficient of expansi.. |
|||
Thermal Conductivity | 0.450 W/m-K | 3.12 BTU-in/hr-ft²-°F | DIN 52612 |
Lehmann & Voss LUVOCOM® 50-7446 Polycarbonate, with carbon fiber, PTFE, lubricant modified Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High-strength and high-stiff parts; low coefficient of expansi.. |
|||
Thermal Conductivity | 0.450 W/m-K | 3.12 BTU-in/hr-ft²-°F | DIN 52612 |
Lehmann & Voss LUVOCOM® 6-7595 Polyamide 12, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Especially suitable at dynamic.. |
|||
Thermal Conductivity | 0.450 W/m-K | 3.12 BTU-in/hr-ft²-°F | DIN 52612 |
Lehmann & Voss LUVOCOM® 80-7050 Polyacetal-copolymer, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts; low thermal coefficient of expansion.Electrically conductive, suitable for.. |
|||
Thermal Conductivity | 0.450 W/m-K | 3.12 BTU-in/hr-ft²-°F | DIN 52612 |
Lehmann & Voss LUVOCOM® 1105/CF/10/GR/10/TF/10-2 PEEK, with carbon fiber, PTFE, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; low thermal coefficient of expansion.Dynamic stressed parts at high m.. |
|||
Thermal Conductivity | 0.450 - 0.470 W/m-K | 3.12 - 3.26 BTU-in/hr-ft²-°F | ASTM C177 |
Solvay Specialty Polymers Polidan® PNT 0553/23 Polyethylene, Crosslinked (XLPE) POLIDAN® PNT 0553/23 is a silane crosslinkable PE compound which is used together with a catalyst masterbatch to accelerate the crosslinking reaction.Features: Crosslinkable; Good Flexibility; Lo.. |
|||
Thermal Conductivity | 0.450 - 0.470 W/m-K | 3.12 - 3.26 BTU-in/hr-ft²-°F | ASTM C177 |
Solvay Specialty Polymers Polidan® PNT 0555/06 Polyethylene, Crosslinked (XLPE) POLIDAN® PNT 0555/06 is a silane crosslinkable PE compound which is used together with a catalyst masterbatch to accelerate the crosslinking reaction. It is used for flexible crosslinkable pipes... |
|||
Thermal Conductivity | 0.450 - 0.470 W/m-K | 3.12 - 3.26 BTU-in/hr-ft²-°F | ASTM C177 |
Solvay Specialty Polymers Polidan® PNT 0856/35 Polyethylene, Crosslinked (XLPE) POLIDAN® PNT 0856/35 is a silane crosslinkable PE compound which is used together with a catalyst masterbatch to accelerate the crosslinking reaction.Features: Crosslinkable; Good Flexibility; Lo.. |
|||
Thermal Conductivity | 0.450 - 0.470 W/m-K | 3.12 - 3.26 BTU-in/hr-ft²-°F | ASTM C177 |
Solvay Specialty Polymers Polidan® T/A-HF Polyethylene, Crosslinked (XLPE) POLIDAN® T/A-HF is a silane crosslinkable PE compound which is used together with a catalyst masterbatch to accelerate the crosslinking reaction. It is used for flexible crosslinkable pipes.Featu.. |
|||
Thermal Conductivity | 0.450 - 0.470 W/m-K | 3.12 - 3.26 BTU-in/hr-ft²-°F | ASTM C177 |
Solvay Specialty Polymers Polidan® T/A-LX Polyethylene, Crosslinked (XLPE) POLIDAN® T/A-LX is a silane crosslinkable PE compound which is used together with a catalyst masterbatch to accelerate the crosslinking reaction. It is used for flexible crosslinkable pipes.Featu.. |
|||
Thermal Conductivity | 0.450 W/m-K @Temperature 100 °C |
3.12 BTU-in/hr-ft²-°F @Temperature 212 °F |
ASTM E1461 |
Plenco 3509 Phenolic, Granular, Injection Molded PLENCO 03509 is a mineral and flock filled phenolic molding compound offering excellent electrical properties, dimensional stability, and improved heat resistance. UL recognized under component file.. |
|||
Thermal Conductivity | 0.450 W/m-K | 3.12 BTU-in/hr-ft²-°F | ASTM E1461 |
Vyncolit BXE7670 Glass Filled Phenolic Molding Compound Novolac resin based, mainly glass fiber filled. Due to its unique composition, excellent balance between mechanical, thermal and dimensional stability.Information provided by Sumitomo Bak North Ame.. |
|||
Thermal Conductivity | 0.450 W/m-K | 3.12 BTU-in/hr-ft²-°F | |
Daelim H&L Plavis-G15 DF 15% Graphite Filled Aromatic Polyimide Bearing Direct Formed. Plavis-G-15: Graphite 15 wt% filled, Self lubricating grade for wear and friction applications.General Plavis information for all grades:PLAVIS polyimide has nitrogen bonded to 3 ca.. |
|||
Thermal Conductivity | 0.450 W/m-K @Temperature 100 °C |
3.12 BTU-in/hr-ft²-°F @Temperature 212 °F |
ASTM E1225 |
Arlon 25FR Low-Cost Ceramic Hydrocarbon High Frequency, Low Loss Thermoset Laminate and Prepreg for Double-sided, Multilayer and Mixed Dielectric Printed Circuit BoardsLow loss ceramic-filled thermoset resinTight dielectric tolerance cont.. |
|||
Thermal Conductivity | 0.450 W/m-K @Temperature 100 °C |
3.12 BTU-in/hr-ft²-°F @Temperature 212 °F |
ASTM E1225 |
Arlon 25N Low-Cost Ceramic Hydrocarbon High Frequency, Low Loss Thermoset Laminate and Prepreg for Double-sided, Multilayer and Mixed Dielectric Printed Circuit BoardsLow loss ceramic-filled thermoset resinTight dielectric tolerance cont.. |
|||
Thermal Conductivity | 0.450 W/m-K | 3.12 BTU-in/hr-ft²-°F | ASTM E1461 |
Arlon EP2 Enhanced Polyimide Laminate and Prepreg High reliability and high temperature materialEP2 Enhanced Polyimide is the next generation of polyimide and prepreg products, engineered for improved properties and processing and for applications .. |
|||
Thermal Conductivity | >= 0.450 W/m-K | >= 3.12 BTU-in/hr-ft²-°F | Compound Property |
Arlon Thermabond®-II 99760N008 0.008" (0.203 mm) Unsupported/Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Unsupported/Uncured RubberAppearance: White/gray gumAppearance: White/grey gumThis data Represents typical values for the production material. The data should not be used.. |
|||
Thermal Conductivity | >= 0.450 W/m-K | >= 3.12 BTU-in/hr-ft²-°F | Compound Property |
Arlon Thermabond®-II 99760N015 0.015" (0.381 mm) Unsupported/Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Unsupported/Uncured RubberAppearance: White/grey gumThis data Represents typical values for the production material. The data should not be used to write, or in place of,.. |
|||
Thermal Conductivity | 0.450 W/m-K @Temperature 100 °C |
3.12 BTU-in/hr-ft²-°F @Temperature 212 °F |
ASTM E1225 |
Arlon AD350A PTFE/Woven Fiberglass/Ceramic Filled Composite Tighter Dielectric Tolerance Low Z-Axis Thermal ExpansionCeramic Filled PTFEHigh Thermal ConductivityLarge Panel SizeBenefits:Higher Consistency of PerformanceSuperior PTH AdhesionHeat Dissipation a.. |
|||
Thermal Conductivity | 0.450 W/m-K @Temperature 1400 °C |
3.12 BTU-in/hr-ft²-°F @Temperature 2550 °F |
|
Sinotek Materials Graphite Felt Heat Insulation Material Information provided by Sinotek |
|||
Thermal Conductivity | 0.450 - 0.490 W/m-K | 3.12 - 3.40 BTU-in/hr-ft²-°F | Average value: 0.468 W/m-K Grade Count:10 |
Overview of materials for High Density Polyethylene (HDPE), Crosslinkable This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Crosslinkable". Each property range of values reported is minimum and .. |